# US 2008/0076231 A1 · Method for fabricating capacitor of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0076231 A1
- Document ID: US20080076231A1
- Status: Published application
- Kind: A1
- Application number: 11/952,767
- Filed: 2007-12-07
- Published: 2008-03-27
- Earliest claimed: 2003-04-04
- Assignees: Hynix Semiconductor Inc.
- Inventors: Dong-Woo SHIN; Hyung-Bok Choi; Jong-Min Lee; Jin-Woong Kim
- Web page: https://patentgrep.com/patent/US20080076231A1

## CPC

- H10D 1/712: {being rough surfaces, e.g. using hemispherical grains}
- H10D 1/042: {using deposition processes to form electrode extensions}
- H10D 1/716: {having vertical extensions}
- H10P 32/302: {Doping polycrystalline silicon or amorphous silicon layers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention relates to a method for fabricating a capacitor of a semiconductor device. The method includes the steps of: forming a first amorphous silicon layer doped with an impurity in a predetermined first doping concentration suppressing dopants from locally agglomerating; forming an impurity undoped second amorphous silicon layer on the first amorphous silicon layer in an in-situ condition; forming a storage node by patterning the first amorphous silicon layer and the second amorphous silicon layer; forming silicon grains on a surface of the storage node; and doping the impurity to the storage node and the silicon grains until reaching a second predetermined concentration for providing conductivity required by the storage node.

## Claims

### Claim at position 1

1-4. (canceled)

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein the step of doping the impurity onto the storage node and the silicon grains proceeds by performing another doping method of a furnace annealing in an atmosphere of a gas containing phosphorus.

### Claim 6 (depends on 5)

The method as recited in claim 5, wherein the furnace annealing is performed at a temperature in a range from about 600° C. to about 750° C. and a pressure ranging from about 5 torr to about 10 torr for about 1 hour to about 2 hours by flowing PH3 gas with a quantity ranging from about 100 sccm to about 200 sccm.

### Claim 7 (depends on 1)

The method as recited in claim 1, wherein the step of doping the impurity onto the storage node and the silicon grains further includes the steps of:
performing a chamber plasma doping in an atmosphere of a gas containing phosphorus; and
diffusing the doped impurity through a furnace annealing.

### Claim 8 (depends on 7)

The method as recited in claim 7, wherein the chamber plasma doping is performed at a temperature ranging from about 700° C. to about 800° C. and a pressure ranging from about 1.5 torr to about 2.5 torr for about 1 minute and about 5 minutes by supplying a plasma power in a range from about 300 W to about 500 W and PH3 gas flowed with a quantity ranging from about 100 sccm to about 500 sccm.

### Claim 9 (depends on 7)

The method as recited in claim 7, wherein the furnace annealing is performed at a temperature ranging from about 600° C. to about 750° C. and a pressure ranging from about 5 torr to about 10 torr in an atmosphere of nitrogen for about 1 hour to about 2 hours.

### Claim at position 7

10-11. (canceled)

### Claim 12

A method for fabricating a capacitor of a semiconductor device, comprising the steps of:
forming an insulation layer having contact holes on an upper surface of a substrate;
forming a plurality of plugs connected to the substrate by being filled into the contact holes;
forming an isolation layer having holes exposing the plurality of the plugs on the insulation layer;
forming a first amorphous silicon layer doped with an impurity in a predetermined first doping concentration suppressing dopants from locally agglomerating;
forming an impurity undoped second amorphous silicon layer on the first amorphous silicon layer in an in-situ condition;
forming a storage node by patterning the first amorphous silicon layer and the second amorphous silicon layer;
forming silicon grains on a surface of the storage node; and
doping the impurity to the storage node and the silicon grains until reaching a second predetermined concentration for providing conductivity required by the storage node.

### Claim 13 (depends on 12)

The method as recited in claim 12, after the step of doping the impurity onto the storage node and the silicon grains, further comprising the steps of:
removing selectively the isolation layer;
doping additionally the impurity to compensate a doping profile of the storage node; and
forming sequentially a dielectric layer and a plate on the storage node.

### Claim 14 (depends on 12)

The method as recited in claim 12, after the step of doping the impurity onto the storage node and the silicon grains, further comprising the step of forming sequentially a dielectric layer and a plate on the storage node and the isolation layer.

### Claim 15 (depends on 13)

The method as recited in claim 13, wherein the step of doping additionally the impurity to compensate the doping profile of the storage node proceeds by performing one doping method of a chamber plasma doping in an atmosphere of a gas containing phosphorus.

### Claim 16 (depends on 15)

The method as recited in claim 15, wherein the chamber plasma doping is performed at a temperature ranging from about 700° C. to about 800° C. and a pressure ranging from about 1.5 torr to about 2.5 torr for about 2 minutes to about 5 minutes by supplying a plasma power ranging from about 300 W to about 500 w and PH3 gas with a flow quantity ranging from about 300 sccm to about 500 sccm.

### Claim 17 (depends on 13)

The method as recited in claim 13, wherein the step of doping additionally the impurity to compensate the doping profile of the storage node proceeds by performing another doping method of a furnace annealing in an atmosphere of a gas containing phosphorus.

### Claim 18 (depends on 17)

The method as recited in claim 17, wherein the furnace annealing is performed at a temperature ranging from about 600° C. to about 750° C. and a pressure ranging from about 5 torr to about 10 torr for about 1 hour to about 2 hours by flowing PH3 gas with a quantity in a range from about 100 sccm to about 200 sccm.

### Claim 19 (depends on 12)

The method as recited in claim 12, wherein the first doping concentration ranges from about 1×1019/cm3 to about 2×1020/cm3 and the second doping concentration ranges from about 24×1020/cm3 to about 1×1022/cm3.

### Claim 20 (depends on 12)

The method as recited in claim 12, wherein the step of doping the impurity on the storage node and the silicon grains proceeds by performing one method of a chamber plasma doping in an atmosphere of a gas containing phosphorus.

### Claim 21 (depends on 20)

The method as recited in claim 20, wherein the chamber plasma doping is performed at a temperature ranging from about 700° C. to about 800° C. and a pressure ranging from about 1.5 torr to about 2.5 torr for about 2 minutes to about 5 minutes by supplying a plasma power in a range from about 300 W to about 500 W and PH3 gas with a flow quantity ranging from about 300 sccm to about 500 sccm.

### Claim 22 (depends on 12)

The method as recited in claim 12, wherein the step of doping the impurity on the storage node and the silicon grains proceeds by performing another method of a furnace annealing in an atmosphere of a gas containing phosphorus.

### Claim 23 (depends on 22)

The method as recited in claim 22, wherein the furnace annealing is performed at a temperature ranging from about 600° C. to about 750° C. and a pressure ranging from about 5 torr to about 10 torr for about 1 hour to about 2 hours by flowing PH3 gas with a quantity in a range from about 100 sccm to about 200 sccm.

### Claim 24 (depends on 12)

The method as recited in claim 12, wherein the step of doping the impurity onto the storage node and the silicon grains includes the steps of:
performing a chamber plasma doping in an atmosphere of a gas containing phosphorus; and
diffusing the doped impurity through a furnace annealing.

### Claim 25 (depends on 24)

The method as recited in claim 24, wherein the chamber plasma doping is performed at a temperature ranging from about 700° C. to about 800° C. and a pressure ranging from about 1.5 torr to about 2.5 torr for about 1 minute to about 5 minutes by supplying a plasma power in a range from about 300 W to about 500 W and PH3 gas with a flow quantity ranging from about 300 sccm to about 500 sccm.

### Claim 26 (depends on 24)

The method as recited in claim 24, wherein the furnace annealing is performed at a temperature ranging from about 600° C. to about 750° C. and a pressure ranging from about 5 torr to about 10 torr in an atmosphere of nitrogen for about 1 hour to about 2 hours.

### Claim 27 (depends on 12)

The method as recited in claim 12, wherein the step of forming the silicon grains on the surface of the storage node further includes the step of cleaning the surface of the storage node on which the silicon grains are formed.

### Claim 28 (depends on 27)

The method as recited in claim 27, wherein the step of cleaning the surface of the storage node proceeds by using a wet chemical such as HF or BOE.