# US 2008/0076224 A1 · Methods of forming flash memory devices including blocking oxide films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0076224 A1
- Document ID: US20080076224A1
- Status: Published application
- Kind: A1
- Application number: 11/756,427
- Filed: 2007-05-31
- Published: 2008-03-27
- Earliest claimed: 2006-09-27
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Min-kyung Ryu; Han-mei Choi; Seung-hwan Lee; Sun-jung Kim; Se-hoon Oh
- Web page: https://patentgrep.com/patent/US20080076224A1

## CPC

- H10D 64/685: {being perpendicular to the channel plane}
- H10D 30/69: IGFETs having charge trapping gate insulators, e.g. MNOS transistors
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10D 64/037: {comprising charge-trapping insulators}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 64/01316: {the conductor comprising a layer of elemental metal contacting the insulator, e.g. Ta, W, Mo or Al}
- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of forming a flash memory device can include forming a tunneling oxide film on a semiconductor substrate, forming a charge storing layer on the tunneling oxide film, forming a first blocking oxide film on the charge storing layer at a first temperature, forming a second blocking oxide film on the first blocking oxide film at a second temperature higher than the first temperature, and forming a gate electrode on the second blocking oxide film.

## Claims

### Claim 1

A method of manufacturing a flash memory device comprising:
forming a tunneling oxide film on a semiconductor substrate;
forming a charge storing layer on the tunneling oxide film;
forming a first blocking oxide film on the charge storing layer at a first temperature;
forming a second blocking oxide film on the first blocking oxide film at a second temperature higher than the first temperature; and
forming a gate electrode on the second blocking oxide film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first temperature is about room temperature to about 600° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second temperature is about 250 to about 950° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first blocking oxide film is formed to a thickness of about 5 to about 50% of a combined thickness of the first blocking oxide film and the second blocking oxide film.

### Claim 5 (depends on 1)

The method of claim 1, wherein a combined thickness of the first blocking oxide film and the second blocking oxide film is about 150 to about 250 Angstroms.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first blocking oxide film and the second blocking oxide film each comprise a metal and oxygen.

### Claim 7 (depends on 6)

The method of claim 6 wherein the first blocking oxide film and the second blocking oxide film each comprise Al2O3, SiO2, HfO2, ZrO2, LaO, LaAlO, LaHfO and/or HfAlO.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first blocking oxide film and the second blocking oxide film are each formed by physical vapor deposition (PVD), atomic layer deposition (ALD) or chemical vapor deposition (CVD).

### Claim 9 (depends on 1)

The method of claim 1, wherein the tunneling oxide film comprises a film including silicon and oxygen.

### Claim 10 (depends on 1)

The method of claim 1, wherein the charge storing layer comprises a silicon nitride film, a metal oxide film, a metal nitride film or a combination thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein the gate electrode comprises a material of TaN, TiN, W, WN, HfN and/or tungsten silicide.

### Claim 12

A method of forming a flash memory device comprising:
forming a first blocking oxide film directly on a charge storing layer at a first temperature using a first deposition step so that the first blocking oxide film has a dielectric constant greater than SiOxNy formed to an equal thickness; and
forming a second blocking oxide film on the first blocking oxide film at a second temperature higher than the first temperature so that a combined impurity content of the first and second blocking oxide films is less than a layer formed at the first temperature to a combined thickness of the first and second blocking oxide films.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first temperature is about 25 to about 600° C.

### Claim 14 (depends on 12)

The method of claim 12, wherein the second temperature is about 250 to about 950° C.

### Claim 15 (depends on 12)

The method of claim 12, wherein the first blocking oxide film is formed to a thickness of about 5 to about 50% of the combined thickness of the first and second blocking oxide films.

### Claim 16 (depends on 12)

The method of claim 12, wherein the combined thickness of the first and second blocking oxide films is about 150 to about 250 Angstromns.

### Claim 17 (depends on 12)

The method of claim 12, wherein the first blocking oxide film and the second blocking oxide film each comprise a metal and oxygen.

### Claim 18 (depends on 17)

The method of claim 17 wherein the first blocking oxide film and the second blocking oxide film each comprise Al2O3, SiO2, HfO2, ZrO2, LaO, LaAlO, LaHfO and/or HfAlO.

### Claim 19 (depends on 12)

The method of claim 12, wherein the first blocking oxide film and the second blocking oxide film are each formed by physical vapor deposition (PVD), atomic layer deposition (ALD) or chemical vapor deposition (CVD).

### Claim 20

A method of forming a flash memory device comprising:
forming a first blocking oxide film directly on a charge storing layer at a first temperature of about 250° C. to a first thickness comprising from about 5% to about less than 50% of a total thickness of a combined blocking oxide film; and
forming a second blocking oxide film directly on the first blocking oxide film at a second temperature of about 600° C. to provide the combined blocking oxide film.