# US 2008/0075972 A1 · Copper electrolytic solution containing quaternary amine compound polymer with specific skeleton and organo-sulfur compound as additives, and electrolytic copper foil manufactured using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0075972 A1
- Document ID: US20080075972A1
- Status: Published application
- Kind: A1
- Application number: 11/974,462
- Filed: 2007-10-12
- Published: 2008-03-27
- Earliest claimed: 2002-12-25
- Assignees: Nikko Materials Co., Ltd.
- Inventors: Masashi Kumagai; Mikio Hanafusa
- Web page: https://patentgrep.com/patent/US20080075972A1

## CPC

- C25D 3/38: of copper
- Y10T 428/12993: Surface feature [e.g., rough, mirror]
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

There is obtained a low-profile electrolytic copper foil with a small surface roughness on the side of the rough surface (the opposite side from the lustrous surface) in the manufacture of an electrolytic copper foil using a cathode drum, and more particularly an electrolytic copper foil which allows fine patterning, and is superior in terms of elongation and tensile strength at ordinary temperatures and high temperatures. The present invention provides a copper electrolytic solution, containing as additives an organo-sulfur compound and a quaternary amine compound polymer obtained by homopolymerizing a compound in which nitrogen of an acrylic type compound having a dialkylamino group is quaternized, or copolymerizing the compound with another compound having an unsaturated bond, and an electrolytic copper foil manufactured using this electrolytic solution.

## Claims

### Claim 1

A method of manufacturing an electrolytic copper foil comprising the step of electrodepositing a copper foil on a cathode from a copper electrolytic solution containing, as additives, an organo-sulfur compound and a quaternary amine compound polymer obtained by homopolymerizing a compound in which nitrogen of an acrylic compound having a dialkylamino group is quaternized or copolymerizing the compound with another compound having an unsaturated bond.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said compound obtained by quaternizing nitrogen of an acrylic compound having a dialkylamino group is expressed by the following general formula (1), (2) or (3),
wherein in general formulae (1) through (3), R1 indicates hydrogen or an alkyl group with 1 to 5 carbon atoms, R2 indicates an alkyl group with 1 to 5 carbon atoms, R3 indicates an alkyl group with 1 to 5 carbon atoms, a benzyl group or an allyl group, X1− indicates Cl−, Br− or CH3SO4−, and n indicates an integer of 1 to 5.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said organo-sulfur compound is a compound expressed by the following general formula (4) or (5),
X—R1—(S)n—R2—Y (4)
R4—S—R3—SO3Z (5)
wherein in general formulae (4) and (5), R1, R2 and R3 each indicate an alkylene group with 1 to 8 carbon atoms, R4 indicates a group selected from the group consisting of hydrogen,
X is selected from the group consisting of hydrogen, a sulfonic acid group, a phosphonic acid group, and an alkali metal salt group or ammonium salt group of sulfonic acid or phosphonic acid, Y is selected from the group consisting of a sulfonic acid group, a phosphonic acid group, and an alkali metal salt group of sulfonic acid or phosphonic acid, Z indicates hydrogen or an alkali metal, and n is 2 or 3.

### Claim 4 (depends on 1)

A copper electrolytic foil formed by the method according to claim 1.

### Claim 5 (depends on 4)

A copper-clad laminate comprising the copper electrolytic foil according to claim 4.

### Claim 6 (depends on 4)

The copper electrolytic foil according to claim 4, wherein the foil has a surface roughness Rz of not more than 1.4 μm, a high-temperature elongation of not less than 10% and a high-temperature tensile strength of 20 kgf/mm2.