# US 2008/0075968 A1 · Metallurgical powder composition and method of production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0075968 A1
- Document ID: US20080075968A1
- Status: Published application
- Kind: A1
- Application number: 11/902,042
- Filed: 2007-09-18
- Published: 2008-03-27
- Earliest claimed: 2006-09-22
- Assignees: Höganäs AB
- Inventors: Ola Bergman; Paul Nurthen
- Web page: https://patentgrep.com/patent/US20080075968A1

## CPC

- C22C 38/22: with molybdenum or tungsten
- B22F 1/16: Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10)
- B22F 9/082: {atomising using a fluid (using centrifugal force B22F9/10)}
- C22C 33/0207: {Using a mixture of pre-alloyed powders or a master alloy}
- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- Y10T 428/12181: Composite powder [e.g., coated, etc.]
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relates to a wear resistant iron-based powder, suitable for the production of pressed and sintered components, comprising 10-20% by weight of Cr, 0.5-5% by weight of Mo and 1-2% by weight of C. The powder is characterised in that it includes pre-alloyed water atomised iron-based powder particles and chromium carbide particles diffusion bonded onto said pre-alloyed powder particles. The invention also relates to a method of producing this powder.

## Claims

### Claim 1

An iron-based powder comprising:
10-20% by weight of Cr;
0.5-5% by weight of Mo; and
1-2% by weight of C;
characterised in that the powder includes pre-alloyed water atomised iron-based powder particles and chromium carbide particles diffusion bonded onto said pre-alloyed powder particles.

### Claim 2 (depends on 1)

An iron-based powder according to claim 1, wherein the chromium carbide particles have an average size in the range of 8-45 μm.

### Claim 3 (depends on 1)

An iron-based powder according to claim 1, wherein the chromium carbide particles have an average size in the range of 10-30 μm.

### Claim 4 (depends on 1)

An iron-based powder according to claim 1, wherein said powder includes 5-30% by volume of chromium carbide.

### Claim 5 (depends on 1)

An iron-based powder according to claim 1, consisting of 10-15 wt % of Cr, 1-1.5 wt % of Mo, 0.5-1.5 wt % of V, 0.5-1.5 wt % of Si, 1-2 wt % of C, and the balance Fe.

### Claim 6

A method of producing an iron-based powder comprising:
mixing particles of a pre-alloyed water atomised iron-based powder with particles of chromium carbide; and
annealing the mixture, whereby the particles of chromium carbide are diffusion bonded onto the particles of the pre-alloyed powder.

### Claim 7 (depends on 6)

A method according to claim 6, wherein the chromium carbide particles have an average size in the range of 8-45 μm.

### Claim 8 (depends on 6)

A method according to claim 6, wherein the chromium carbide particles have an average size in the range of 10-30 μm.

### Claim 9 (depends on 6)

A method according to claim 6, wherein the pre-alloyed powder comprises 2-10% by weight of Cr, 0.5-5% by weight of Mo and 0.1-1% by weight of C.

### Claim 10 (depends on 6)

A method according to claim 6, wherein the pre-alloyed powder consists of 3-7% by weight of Cr, 1-2% by weight of Mo, 0.2-0.5% by weight of C, and balance Fe.

### Claim 11 (depends on 2)

An iron-based powder according to claim 2, consisting of 10-15 wt % of Cr, 1-1.5 wt % of Mo, 0.5-1.5 wt % of V, 0.5-1.5 wt % of Si, 1-2 wt % of C, and the balance Fe.

### Claim 12 (depends on 3)

An iron-based powder according to claim 3, consisting of 10-15 wt % of Cr, 1-1.5 wt % of Mo, 0.5-1.5 wt % of V, 0.5-1.5 wt % of Si, 1-2 wt % of C, and the balance Fe.

### Claim 13 (depends on 4)

An iron-based powder according to claim 4, consisting of 10-15 wt % of Cr, 1-1.5 wt % of Mo, 0.5-1.5 wt % of V, 0.5-1.5 wt % of Si, 1-2 wt % of C, and the balance Fe.

### Claim 14 (depends on 7)

A method according to claim 7, wherein the pre-alloyed powder comprises 2-10% by weight of Cr, 0.5-5% by weight of Mo and 0.1-1% by weight of C.

### Claim 15 (depends on 8)

A method according to claim 8, wherein the pre-alloyed powder comprises 2-10% by weight of Cr, 0.5-5% by weight of Mo and 0.1-1% by weight of C.

### Claim 16 (depends on 7)

A method according to claim 7, wherein the pre-alloyed powder consists of 3-7% by weight of Cr, 1-2% by weight of Mo, 0.2-0.5% by weight of C, and balance Fe.

### Claim 17 (depends on 8)

A method according to claim 8, wherein the pre-alloyed powder consists of 3-7% by weight of Cr, 1-2% by weight of Mo, 0.2-0.5% by weight of C, and balance Fe.