# US 2008/0075949 A1 · Coated Component Consisting of Quartz Glass, and Method for Producing Said Component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0075949 A1
- Document ID: US20080075949A1
- Status: Published application
- Kind: A1
- Application number: 11/661,160
- Filed: 2005-08-23
- Published: 2008-03-27
- Earliest claimed: 2004-08-23
- Assignees: Heraeus Quarzglas GmH & Co. KG
- Inventors: Ulrich Kirst; Wolfgang Stang; Juergen Weber; Waltraud Werdecker; Martin Trommer; Joerg Becker
- Web page: https://patentgrep.com/patent/US20080075949A1

## CPC

- C03C 17/25: by deposition from the liquid phase
- C03B 19/066: {for the production of quartz or fused silica articles (other processes specially adapted for the production of quartz or fused silica articles C03B20/00)}
- C03C 17/02: with glass (C03C17/34, C03C17/44 take precedence)
- C03C 2217/213: SiO2
- Y10T 428/26: Web or sheet containing structurally defined element or component, the element or component having a specified physical dimension
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to methods for producing a coated component consisting of quartz glass, according to which the component surface is at least partially provided with a SiO2 glass composition that differs from the quartz glass of the base body. The aim of the invention is to provide a novel way of coating a quartz glass component with a SiO2 glass composition that can be produced in a cost-effective, reproducible manner, with any thickness, and can fulfil various functions according to the concrete embodiment thereof. To this end, an amorphous slip containing SiO2 particles is produced and applied to the surface of the base body, forming a slip layer which is dried and then vitrified, forming a SiO2 glass composition. The quartz glass components coated in this way can be advantageously used especially in the production of semiconductors.

## Claims

### Claim 1

A method for producing a coated component of quartz glass, said method comprising: covering a surface of a base body of quartz glass at least in part with an SiO2 glass mass which differs in its optical, physical or chemical properties from quartz glass of the base body, wherein a slip containing amorphous SiO2 particles is produced and applied to the surface of the base body so as to form a slip layer, and the slip layer is dried and subsequently vitrified so as to form an SiO2 glass mass, wherein the SiO2 particles have particle sizes in a range of not more than 100 μm, and wherein a majority by volume of the SiO2 particles have particle sizes in a range from 1 μm to 50 μm, and wherein the SiO2 particles are produced by wet milling SiO2 start grains.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a dried slip layer is vitrified by heating said dried slip layer to a temperature ranging from 1000° C. to 1600° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a dried slip layer is vitrified in a hydrogen atmosphere.

### Claim 4 (depends on 1)

The method according to claim 1, wherein a dried slip layer is vitrified using a burner flame.

### Claim 5 (depends on 1)

The method according to claim 1, wherein a dried slip layer is vitrified using a laser.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the SiO2 glass mass is formed as a thickening in portions of the base body.

### Claim 7 (depends on 1)

The method according to claim 1, wherein dopants chosen from the group consisting of yttrium, aluminum, nitrogen, carbon and any compounds thereof are added to the slip.

### Claim 8

A method for producing a quartz glass component, said method comprising: preparing a slip from SiO2 particles and a liquid, forming a porous green body therefrom by mold casting and drying, and densifying said porous green body completely or in part by sintering, wherein the SiO2 particles are amorphous, are prepared by wet-milling SiO2 start grains in the liquid, and have particle sizes in a range of not more than 500 μm during mold casting, wherein a majority by volume of the SiO2 particles have particle sizes in a range of between 1 μm and 50 μm, and wherein the green body is densified by heating in a hydrogen-containing atmosphere.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the amorphous SiO2 particles have particle sizes in a range of not more than 50 μm during slip casting.

### Claim 10 (depends on 8)

The method according to claim 8, wherein a hydrogen content in the hydrogen-containing atmosphere during sintering is at least 70 vol. %.

### Claim 11

A quartz glass component comprising: a base body of quartz glass having a surface covered at least in part with an SiO2 glass mass which differs in its optical, physical or chemical properties from quartz glass of the base body, wherein the glass mass is prepared from a dried vitrified slip mass containing amorphous SiO2 particles, wherein the SiO2 glass mass is opaque or at least partly opaque and comprises a material with characteristics of a species with respect to the base body.

### Claim 12 (depends on 11)

The quartz glass component according to claim 11, wherein the SiO2 glass mass is formed with a surface free from cracks and without any tools at an average surface roughness Ra of at least 0.5 μm.

### Claim 13 (depends on 12)

The quartz glass component according to claim 12, wherein the surface of the SiO2 glass mass has an average surface roughness Ra of at least 1.0 μm.

### Claim 14 (depends on 11)

The quartz glass component according to claim 11, wherein the SiO2 glass mass has a thickened portion of the base body.

### Claim 15 (depends on 11)

The quartz glass component according to claim 11, wherein the SiO2 glass mass contains dopants chosen from the group consisting of yttrium, aluminum, nitrogen, carbon and any compounds thereof.

### Claim 16 (depends on 1)

The method according to claim 1, wherein a dried slip layer is vitrified by heating said dried slip layer to a temperature ranging from 1100° C. to 1400° C.