# US 2008/0073654 A1 · Display device and fabrication method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0073654 A1
- Document ID: US20080073654A1
- Status: Published application
- Kind: A1
- Application number: 11/898,997
- Filed: 2007-09-18
- Published: 2008-03-27
- Earliest claimed: 2006-09-27
- Assignees: Hitachi Displays, Ltd.
- Inventors: Hidekazu Miyake; Toshihiko Itoga; Eiji OUE; Takeshi Noda
- Web page: https://patentgrep.com/patent/US20080073654A1

## CPC

- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6731: {Top-gate only TFTs}
- H10D 30/6732: {Bottom-gate only TFTs}
- H10D 30/6745: {Polycrystalline or microcrystalline silicon}
- H10D 86/0229: {characterised by control of the annealing or irradiation parameters}
- H10D 86/421: {having a particular composition, shape or crystalline structure of the active layer}
- H10D 86/425: {having different crystal properties in different TFTs or within an individual TFT}
- H10D 86/427: {having different thicknesses of the semiconductor bodies in different TFTs}
- H10D 86/431: {having different compositions, shapes, layouts or thicknesses of gate insulators in different TFTs}
- H10D 86/471: {having different architectures, e.g. having both top-gate and bottom-gate TFTs}
- H10D 86/60: wherein the TFTs are in active matrices
- H10D 30/673: {characterised by the shapes, relative sizes or dispositions of the gate electrodes}
- H10D 62/117: {Shapes of semiconductor bodies}
- H10D 62/40: Crystalline structures
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3808: {using laser beams}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Improvement in characteristics of a SELAX-TFT and throughput of ELA crystallization is achieved. When a thin film transistor using pseudo single crystal semiconductor and a thin film transistor using particulate polysilicon semiconductor are formed on a single substrate, the film thickness of an amorphous semiconductor film before crystallization in the pseudo single crystal semiconductor portion is greater than that in the polysilicon semiconductor portion.

## Claims

### Claim 1

A method for fabricating a display device in which a thin film transistor using a pseudo single crystal semiconductor and a thin film transistor using a particulate polycrystalline semiconductor are formed on a single substrate, wherein a film thickness of an amorphous semiconductor film before crystallization in a pseudo single crystal semiconductor portion is greater than that in a polycrystalline semiconductor portion.

### Claim 2 (depends on 1)

The method for fabricating a display device according to claim 1,
wherein the pseudo single crystal semiconductor portion and the polycrystalline semiconductor portion are formed in the same layer.

### Claim 3 (depends on 1)

The method for fabricating a display device according to claim 1,
wherein the pseudo single crystal semiconductor portion and the polycrystalline semiconductor portion are formed in different layers.

### Claim 4 (depends on 1)

The method for fabricating a display device according to claim 1,
wherein the layer thickness of the amorphous semiconductor film before crystallization in the pseudo single crystal semiconductor portion is 50 to 400 nm, and the layer thickness of the amorphous semiconductor film before crystallization in the polycrystalline semiconductor portion is 30 to 70 nm.

### Claim 5

A display device having a thin film transistor using a pseudo single crystal semiconductor and a thin film transistor using a particulate polycrystalline semiconductor on a single substrate, wherein an average film thickness of a semiconductor layer in the thin film transistor using the pseudo single crystal semiconductor is greater than an average film thickness of a semiconductor layer in the thin film transistor using the polycrystalline semiconductor.

### Claim 6 (depends on 5)

The display device according to claim 5,
wherein the pseudo single crystal semiconductor portion and the polycrystalline semiconductor portion are formed in the same layer.

### Claim 7 (depends on 5)

The display device according to claim 5,
wherein the pseudo single crystal semiconductor portion and the polycrystalline semiconductor portion are formed in different layers.

### Claim 8 (depends on 7)

The display device according to claim 7,
wherein the gate electrode of one of the thin film transistor using the pseudo single crystal semiconductor and the thin film transistor using the particulate polycrystalline semiconductor is formed of a semiconductor film formed in the same layer as the semiconductor layer of the other thin film transistor.

### Claim 9 (depends on 5)

The display device according to claim 5,
wherein the average film thickness of the pseudo single crystal semiconductor is 50 to 400 nm, and the average film thickness of the polycrystalline semiconductor is 30 to 70 nm.