# US 2008/0072798 A1 · Improved Asphaltic Concrete Compositions That Contain Anhydrite As Anti-Stripping Asphalt Agents

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0072798 A1
- Document ID: US20080072798A1
- Status: Published application
- Kind: A1
- Application number: 11/815,069
- Filed: 2005-07-01
- Published: 2008-03-27
- Earliest claimed: 2005-01-31
- Assignees: Gcc Technology and Processes S.A.
- Inventors: Armando Garcia Luna; Jamie Valenzuela Grado
- Web page: https://patentgrep.com/patent/US20080072798A1

## CPC

- C04B 40/0039: {Premixtures of ingredients}
- C04B 26/26: Bituminous materials, e.g. tar, pitch {(C08L95/00 takes precedence)}
- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- E01C 7/26: mixed with other materials, e.g. cement, rubber, leather, fibre {(fibrous material reinforcements for bituminous paving E01C11/165)}
- C04B 2111/00215: {Mortar or concrete mixtures defined by their oxide composition}
- C04B 2111/0075: {for road construction}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- E01C: CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE; MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR (forming roads or like surfaces by compacting or grading snow or ice E01H)

## Abstract

The present invention describes improved asphaltic concrete compositions resistant to the stripping, as well as their methods of obtaining. Also compositions that contain anhydrite are described that result to be useful like anti-stripping agents of asphaltic concretes. The described anti-stripping compositions allow to improve the properties of union of the asphaltic concrete compositions after their application, increasing with it the useful lifetime of coverings elaborated with these materials.

## Claims

### Claim at position 1

1-32. (canceled)

### Claim 33

An asphaltic concrete composition resistant to stripping that comprise an asphalt cementitious, a stony aggregate and an anti-stripping composition, wherein the anti-stripping composition is constituted by a mixture that comprise:
a) Portland cement in a percentage in weight with respect to the total weight of anti-stripping composition from 25 to 40%, and
b) Anhydrite in a percentage in weight with respect to the total weight of anti-stripping composition from 60 to 75%.

### Claim 34 (depends on 33)

The asphaltic concrete of claim 33, wherein the Portland cement is selected of the group that comprise type-1, type-2, type-3, type-4 and type-5.

### Claim 35 (depends on 34)

The asphaltic concrete of claim 34, wherein the Portland cement is provided in form of clinker.

### Claim 36 (depends on 33)

The asphaltic concrete of claim 33, wherein the anti-stripping composition comprise:
a) Sulphates in a percentage in weight with respect to the total weight of the anti-stripping composition of 38%,
b) CaO in a percentage in weight with respect to the total weight of the anti-stripping composition of 60%, and
c) Alumina in a percentage in weight with respect to the total weight of the anti-stripping composition of 2%.

### Claim 37 (depends on 36)

The asphaltic concrete of claim 36, wherein the anti-stripping composition comprise:
Percentage in weight with respect to the
total weight of the anti-stripping
Component
composition (%)
SiO2
9-10
Al2O3
0-2
Fe2O3
0-1.3
CaO
50-60
MgO
0-0.2
K2O
0-0.3
Na2O
0-0.2
SO3
34-38
Free lime
0-0.3
PPI
0-1.0

### Claim 38 (depends on 33)

The asphaltic concrete of claim 33, wherein the anti-stripping composition has a mesh fineness of 325 in a 80% as minimum.

### Claim 39 (depends on 38)

The asphaltic concrete of claim 38, wherein the anti-stripping composition has a mesh fineness of 325 in a 99%.

### Claim 40 (depends on 33)

The asphaltic concrete of claim 33, wherein the anti-stripping composition has a minimum compressive strength of 180 Kg/cm2 at 7 days and 250 Kg/cm2 at 28 days.

### Claim 41 (depends on 33)

The asphaltic concrete of claim 33, wherein the Portland cement is in a percentage in weight with respect to the total weight of anti-stripping composition of 40%, and the anhydrite in a percentage in weight with respect to the total weight of anti-stripping composition of 60%.

### Claim 42 (depends on 33)

The asphaltic concrete of claim 33, wherein the Index of retained strength is of 93% as minimum.

### Claim 43 (depends on 42)

The asphaltic concrete of claim 42, wherein the anti-stripping composition is in a percentage in weight with respect to the total weight of the asphaltic concrete from 0.5 to 3.0%.

### Claim 44 (depends on 43)

The asphaltic concrete of claim 43, wherein the anti-stripping composition is in a percentage in weight with respect to the total weight of the asphaltic concrete from 1.0 to 2.0%.

### Claim 45

A method to improve the anti-stripping properties of asphaltic concrete compositions, wherein the method comprise to add to the asphaltic concrete composition an anti-stripping composition constituted by a mixture that comprise:
a) Portland cement in a percentage in weight with respect to the total weight of anti-stripping composition from 25 to 40%,
b) Anhydrite in a percentage in weight with respect to the total weight of anti-stripping composition from 60 to 75%.

### Claim 46 (depends on 45)

The method of claim 45, wherein the Portland cement is selected from a group that comprise type-1, type-2, type-3, type-4 and type-5.

### Claim 47 (depends on 46)

The method of claim 46, wherein the Portland cement is provided in clinker form.

### Claim 48 (depends on 45)

The method of claim 45, wherein the anti-stripping composition comprise:
a) Sulphates in a percentage in weight with respect to the total weight of the anti-stripping composition of 38%,
b) CaO in a percentage in weight with respect to the total weight of the anti-stripping composition of 60%, and
c) Alumina in a percentage in weight with respect to the total weight of the anti-stripping composition of 2%.

### Claim 49 (depends on 48)

The method of claim 48, wherein the anti-stripping composition comprise:
Percentage in weight with respect to the
total weight of the anti-stripping
Component
composition (%)
SiO2
9-10
Al2O3
0-2
Fe2O3
0-1.3
CaO
50-60
MgO
0-0.2
K2O
0-0.3
Na2O
0-0.2
SO3
34-38
Free lime
0-0.3
PPI
0-1.0

### Claim 50 (depends on 45)

The method of claim 45, wherein the anti-stripping composition has a mesh fineness of 325 in a 80% as minimum.

### Claim 51 (depends on 50)

The method of claim 50, wherein the anti-stripping composition has a mesh fineness of 325 in a 99%.

### Claim 52 (depends on 45)

The method of claim 45, wherein the anti-stripping composition has a minimum compressive strength of 180 Kg/cm2 at 7 days and 250 Kg/cm2 at 28 days.

### Claim 53 (depends on 45)

The method of claim 45, wherein the Portland cement is in a percentage in weight with respect to the total weight of the anti-stripping composition of 40%, and the anhydrite in a percentage in weight with respect to the total weight of anti-stripping composition of 60%.

### Claim 54 (depends on 45)

The method of claim 45, wherein the anti-stripping composition is added to the asphaltic concrete in a percentage in weight with respect to the total weight of the asphaltic concrete from 0.5 to 3.0%.

### Claim 55 (depends on 54)

The method of claim 54, wherein the anti-stripping composition is added to the asphaltic concrete in a percentage in weight with respect to the total weight of the asphaltic concrete from 1.0 to 2.0%.

### Claim 56 (depends on 45)

The method of claim 45, wherein the anti-stripping composition is added to the asphaltic concrete in powder form.

### Claim 57 (depends on 45)

The method of claim 45, wherein the anti-stripping composition is added to the asphaltic concrete in slurry form.

### Claim 58

The use of a cementitious composition that comprise:
a) Portland cement in a percentage in weight with respect to the total weight of the cementitious from 25 to 40%, and
b) Anhydrite in a percentage in weight with respect to the total weight of the cementitious from 60 to 75%,
as anti-stripping agent of asphaltic concrete.

### Claim 59 (depends on 58)

The use of claim 58, wherein the Portland cement is selected of the group that comprise type-1, type-2, type-3, type-4 and type-5.

### Claim 60 (depends on 59)

The use of claim 59, wherein the Portland cement is provided in clinker form.

### Claim 61 (depends on 58)

The use of claim 58, wherein the cementitious composition comprise:
a) Sulphates in a percentage in weight with respect to the total weight of the cementitious composition of 38%,
b) CaO in a percentage in weight with respect to the total weight of the cementitious composition of 60%, and
c) Alumina in a percentage in weight with respect to the total weight of the cementitious composition of 2%.

### Claim 62 (depends on 61)

The use of claim 61, wherein the cementitious composition comprise:
Percentage in weight with respect to the
total weight of the anti-stripping
Component
composition (%)
SiO2
9-10
Al2O3
0-2
Fe2O3
0-1.3
CaO
50-60
MgO
0-0.2
K2O
0-0.3
Na2O
0-0.2
SO3
34-38
Free lime
0-0.3
PPI
0-1.0

### Claim 63 (depends on 58)

The use of claim 58, wherein the cementitious composition has a mesh fineness of 325 in a 80% like minimum.

### Claim 64 (depends on 63)

The use of claim 63, wherein the cementitious composition has a mesh fineness of 325 in a 99%.

### Claim 65 (depends on 58)

The use of claim 58, wherein the cementitious composition has a minimum compressive strength of 180 Kg/cm2 at 7 days and 250 Kg/cm2 at 28 days.

### Claim 66 (depends on 58)

The use of claim 58, wherein the Portland cement is in a percentage in weight with respect to the total weight of the cementitious of 40%, and the anhydrite in a percentage in weight with respect to the total weight of the cementitious of 60%.