# US 2008/0072797 A1 · Fiber reinforced cement composition and products and manufacturing process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0072797 A1
- Document ID: US20080072797A1
- Status: Published application
- Kind: A1
- Application number: 11/598,815
- Filed: 2006-11-14
- Published: 2008-03-27
- Earliest claimed: 2006-09-27
- Assignees: Nichiha Corporation
- Inventors: Kazuo Utagaki; Tadashi Sugita; Satoshi Takayama
- Web page: https://patentgrep.com/patent/US20080072797A1

## CPC

- C04B 28/04: Portland cements
- C04B 28/18: containing mixtures of the silica-lime type
- C04B 2111/29: {Frost-thaw resistance}
- C04B 2111/30: Nailable or sawable materials
- C04B 2111/34: Non-shrinking or non-cracking materials
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- Y10S 106/01: Fly ash
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The problems to be solved by the invention are to provide a fiber reinforced cement composition for obtaining a fiber reinforced cement product which is excellent in bending strength, dimensional stability and installation property such as handling property, flexibility performance and nail performance, as well as a process for manufacturing the product. Namely, the fiber reinforced cement composition comprises the following raw materials: a hydraulic inorganic material, a siliceous material and a woody reinforcement, wherein the siliceous material is a mixture of an average particle size of not less than 15 μm and not more than 50 μm which is burned ash of coal and/or rhyolite and an average particle size of not less than 1 μm and not more than 15 μm which is burned ash of coal and/or rhyolite. The effects of the present invention, it is possible to obtain a fiber reinforced cement product having good bending strength, dimensional stability and installation property such as handling property, flexibility performance and nail performance.

## Claims

### Claim 1

A fiber reinforced cement composition comprising the following raw materials: a hydraulic inorganic material, a siliceous material and a woody reinforcement, wherein the siliceous material is a mixture of an average particle size of not less than 15 μm and not more than 50 μm which is burned ash of coal and/or rhyolite and an average particle size of not less than 1 μm and not more than 15 μm which is burned ash of coal and/or rhyolite.

### Claim 2 (depends on 1)

The fiber reinforced cement composition according to claim 1, wherein burned ash of coal is fly ash and rhyolite is pearlstone.

### Claim 3 (depends on 1)

The fiber reinforced cement composition according to claim 1, wherein the hydraulic inorganic material is a portland cement.

### Claim 4 (depends on 1)

The fiber reinforced cement composition according to claim 1, wherein the woody reinforcement is a mixture of NUKP and/or NBKP and used paper in a ratio of the NUKP and/or NBKP to used paper in a range of from 1:1 to 4:1.

### Claim 5 (depends on 1)

The fiber reinforced cement composition according to claim 1, additionally comprising mica and a water-soluble resin.

### Claim 6

A fiber reinforced cement composition comprising the following raw materials: not less than 25% by mass and not more than 45% by mass of the hydraulic inorganic material, not less than 5% by mass and not more than 12% by mass of the woody reinforcement, not less than 50% by mass and not more than 65% by mass of the siliceous material, wherein a finely dividing siliceous material which is an average particle size of not less than 1 μm and not more than 15 μm is not less than 25% by mass and not more than 75% by mass of the whole siliceous material consisting of the siliceous material which is an average particle size of not less than 15 μm and not more than 50 μm and the finely dividing siliceous material which is an average particle size of not less than 1 μm and not more than 15 μm, and the siliceous material is burned ash of coal and/or rhyolite.

### Claim 7 (depends on 6)

The fiber reinforced cement composition according to claim 6, wherein the hydraulic inorganic material is a portland cement, the woody reinforcement is a mixture of NUKP and/or NBKP and used paper in a ratio of the NUKP and/or NBKP to used paper in a range of from 1:1 to 4:1, the siliceous material which is an average particle size of not less than 15 μm and not more than 50 μm is fly ash and/or pearlstone, the finely dividing siliceous material which is an average particle size of not less than 1 μm and not more than 15 μm is fly ash and/or pearlstone.

### Claim 8 (depends on 7)

The fiber reinforced cement composition according to claim 7, additionally comprising mica in an amount of not less than 1% by mass and not more than 7% by mass and a water-soluble resin in an amount of not less than 0.25% by mass and not more than 1.5% by mass based on the composition.

### Claim 9 (depends on 6)

The fiber reinforced cement product manufactured from the fiber reinforced cement composition according to claim 6.

### Claim 10 (depends on 7)

The fiber reinforced cement product manufactured from the fiber reinforced cement composition according to claim 7.

### Claim 11 (depends on 8)

The fiber reinforced cement product manufactured from the fiber reinforced cement composition according to claim 8.

### Claim 12

A process for manufacturing the fiber reinforced cement product comprising the steps of: dispersing in water a raw material composition comprising as main raw materials not less than 25% by mass and not more than 45% by mass of hydraulic inorganic material, not less than 50% by mass and not more than 65% by mass of the siliceous material, not less than 5% by mass and not more than 12% by mass of the woody reinforcement, wherein a finely dividing siliceous material which is an average particle size of not less than lum and not more than 15 μm is not less than 25% by mass and not more than 75% by mass of the whole siliceous material consisting of the siliceous material which is an average particle size of not less than 15 μm and not more than 50 μm and the finely dividing siliceous material which is an average particle size of not less than 1 μm and not more than 15 μm, and the siliceous material is burned ash of coal and/or rhyolite to give a slurry of the raw materials; forming a green mat from the slurry; and pressing the green mat by press molding and thereafter curing the mat in an autoclave.

### Claim 13 (depends on 12)

The process for manufacturing the fiber reinforced cement product according to claim 12, wherein the hydraulic inorganic material is a portland cement, the woody reinforcement is a mixture of NUKP and/or NBKP and used paper in a ratio of the NUKP and/or NBKP to used paper in a range of from 1:1 to 4:1, the siliceous material which is an average particle size of not less than 15 μm and not more than 50 μm is fly ash and/or pearlstone, the finely dividing siliceous material which is an average particle size of not less than 1 μm and not more than 15 μm is fly ash and/or pearlstone.

### Claim 14 (depends on 13)

The process for manufacturing the fiber reinforced cement product according to claim 13, additionally comprising mica in an amount of not less than 1% by mass and not more than 7% by mass and a water-soluble resin in an amount of not less than 0.25% by mass and not more than 1.5% by mass based on the composition.