# US 2008/0057448 A1 · Photothermographic material and image forming method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0057448 A1
- Document ID: US20080057448A1
- Status: Published application
- Kind: A1
- Application number: 11/896,145
- Filed: 2007-08-30
- Published: 2008-03-06
- Earliest claimed: 2006-09-04
- Assignees: FUJIFILM Corporation
- Inventors: Hideo Fushimi
- Web page: https://patentgrep.com/patent/US20080057448A1

## CPC

- G03C 1/49863: {Inert additives, e.g. surfactants, binders}
- G03C 1/49818: {Silver halides}
- G03C 1/04: with macromolecular additives; with layer-forming substances
- G03C 1/385: {containing fluorine}
- G03C 1/49827: {Reducing agents}
- G03C 1/49881: {characterised by the process or the apparatus}
- G03C 2001/03594: {Size of the grains}
- G03C 2200/52: Rapid processing
- G03C 2200/60: Temperature
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

The present invention provides a photothermographic material having, on at least one side of a support, an image forming layer including at least a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent for silver ions, and a binder, and at least one non-photosensitive layer, wherein: 1) a mean grain size of the photosensitive silver halide is from 10 nm to 40 nm in terms of equivalent circular diameter, and a number of coated grains thereof is from 550 grains/μm2 to 10000 grains/μm2; and 2) the photothermographic material includes a fluorocarbon compound represented by the following formula (FC-1), (FC-2), or (FC-3). A photothermographic material and an image forming method which exhibit improved coated surface state and high quality are provided. (Rf)p—Y-(L-Z)q: Formula (FC-1) Rf-L-Z′-L-Rf: Formula (FC-2) Z-L-Rf′-L-Z: Formula (FC-3)

## Claims

### Claim 1

A photothermographic material comprising, on at least one side of a support, an image forming layer comprising at least a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent for silver ions, and a binder, and at least one non-photosensitive layer, wherein:
1) a mean grain size of the photosensitive silver halide is from 10 nm to 40 nm in terms of equivalent circular diameter, and a number of coated grains thereof is from 550 grains/μm2 to 10000 grains/μm2; and
2) the photothermographic material comprises a fluorocarbon compound represented by the following formula (FC-1), (FC-2), or (FC-3):
(Rf)p—Y-(L-Z)q Formula (FC-1):
Rf-L-Z′-L-Rf Formula (FC-2):
Z-L-Rf′-L-Z Formula (FC-3):
wherein Rf represents a fluoroalkyl group or fluoroalkenyl group having 3 to 17 fluorine atoms; Rf′ represents a fluoroalkylene group or fluoroalkenylene group having 3 to 17 fluorine atoms; L represents a bond or a divalent linking group; Y represents a bond or a saturated linking group having a valency of (p+q); Z represents an anionic group, a cationic group, a betaine group, or a nonionic polar group; Z′ represents a divalent nonionic polar group; p and q each independently represent an integer of from 1 to 3; and when (p+q) is 2, both of L and Y are not simultaneously a bond.

### Claim 2 (depends on 1)

The photothermographic material according to claim 1, wherein the mean grain size of the photosensitive silver halide is from 20 nm to 30 nm in terms of equivalent circular diameter.

### Claim 3 (depends on 1)

The photothermographic material according to claim 1, wherein the number of coated grains of the photosensitive silver halide is from 2000 grains/μm2 to 8000 grains/μm2.

### Claim 4 (depends on 1)

The photothermographic material according to claim 1, wherein, in formula (FC-1), (p+q) is 3.

### Claim 5 (depends on 1)

The photothermographic material according to claim 1, wherein Rf is represented by the following formula (FC-1-C):
-Rc-Re—W Formula (FC-1-C):
wherein Rc represents a bond or a straight-chain alkylene group having 4 or fewer carbon atoms; Re represents a perfluoroalkylene group having 2 to 6 carbon atoms; and W represents a hydrogen atom or a fluorine atom.

### Claim 6 (depends on 1)

The photothermographic material according to claim 1, wherein Rf is a C4F9 group.

### Claim 7 (depends on 1)

The photothermographic material according to claim 1, wherein Rf is a C9F17 group.

### Claim 8 (depends on 1)

The photothermographic material according to claim 1, wherein the reducing agent for silver ions is a compound represented by the following formula (R1):
wherein R1 and R1′ each independently represent an alkyl group having 1 to 20 carbon atoms; R2 and R2′ each independently represent a hydrogen atom or a substituent which substitutes for a hydrogen atom on a benzene ring; R3 represents a substituent which forms a 3- to 7-membered ring formed from atoms selected from among carbon, oxygen, nitrogen, sulfur, and phosphorus; and X and X′ each independently represent a hydrogen atom or a group substituting for a hydrogen atom on a benzene ring.

### Claim 9 (depends on 1)

The photothermographic material according to claim 1, wherein 50% by weight or more of the binder in the image forming layer is poly(vinyl butyral).

### Claim 10 (depends on 9)

The photothermographic material according to claim 9, wherein the poly(vinyl butyral) is a mixture of poly(vinyl acetal) of a low polymerization degree and poly(vinyl acetal) of a high polymerization degree.

### Claim 11 (depends on 10)

The photothermographic material according to claim 10, wherein the poly(vinyl acetal) of a low polymerization degree is poly(vinyl butyral) having a weight-average polymerization degree of from 200 to 600.

### Claim 12 (depends on 10)

The photothermographic material according to claim 10, wherein the poly(vinyl acetal) of a high polymerization degree is poly(vinyl butyral) having a weight-average polymerization degree of from 900 to 3000.

### Claim 13 (depends on 10)

The photothermographic material according to claim 10, wherein a weight ratio of the poly(vinyl acetal) of a low polymerization degree to the poly(vinyl acetal) of a high polymerization degree is from 5/95 to 95/5.

### Claim 14 (depends on 1)

The photothermographic material according to claim 1, wherein 50% by weight or more of the binder in the image forming layer is a polymer latex.

### Claim 15 (depends on 1)

The photothermographic material according to claim 1, wherein a mean particle size of the non-photosensitive organic silver salt is 0.4 μm or less in terms of equivalent spherical diameter.

### Claim 16 (depends on 15)

The photothermographic material according to claim 15, wherein the non-photosensitive organic silver salt is a silver salt formed by a reaction between a potassium salt of an organic acid and silver nitrate.

### Claim 17 (depends on 15)

The photothermographic material according to claim 15, wherein the non-photosensitive organic silver salt comprises nanoparticles.

### Claim 18 (depends on 17)

The photothermographic material according to claim 17, wherein the nanoparticles are particles prepared in the presence of at least one dispersing agent comprising polyacrylamide or a derivative thereof.

### Claim 19 (depends on 1)

The photothermographic material according to claim 1, wherein the photothermographic material comprises a compound represented by the following formula (1) on the side having the image forming layer:
wherein L1 represents a bond or a divalent linking group; R1 and R2 each independently represent a hydrogen atom, or a hydrocarbon group which may bond to each other to form a ring; X represents a hydrogen atom or a cation; and when X is a cation having a valency of 2 or more, the two carboxy groups may chelate with a single X.

### Claim 20 (depends on 19)

The photothermographic material according to claim 19, wherein the photothermographic material comprises the compound represented by formula (1) on the side having the image forming layer in an amount of from 0.2 g/m2 to 1.0 g/m2.

### Claim 21 (depends on 19)

The photothermographic material according to claim 19, wherein the photothermographic material comprises the compound represented by formula (1) in an amount of from 10 mol % to 30 mol % per 1 mol of silver on the side having the image forming layer.

### Claim 22 (depends on 19)

The photothermographic material according to claim 19, wherein the compound represented by formula (1) is a compound represented by the following formula (2):
wherein L2 represents a 6- to 8-membered, substituted or unsubstituted, saturated or unsaturated hydrocarbon ring.

### Claim 23 (depends on 19)

The photothermographic material according to claim 19, wherein the photothermographic material comprises at least two compounds represented by formula (1).

### Claim 24 (depends on 1)

An image forming method for forming an image by imagewise exposing and thermally developing the photothermographic material according to claim 1, wherein the imagewise exposure is executed by scanning exposure using a laser beam forming a beam spot diameter of 25 μm or less on the exposed surface of the photothermographic material, and the thermal development is executed by heating at 100° C. to 200° C. for a period of from 1 sec to 60 sec.

### Claim 25 (depends on 24)

The image forming method according to claim 24, wherein an obtained maximum image density is 4 or higher.