# US 2008/0041300 A1 · Preparation of single-crystalline polyalkylthiophene structures by surface-induced self-assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0041300 A1
- Document ID: US20080041300A1
- Status: Published application
- Kind: A1
- Application number: 11/894,169
- Filed: 2007-08-20
- Published: 2008-02-21
- Earliest claimed: 2006-08-21
- Assignees: Postech Foundation
- Inventors: Kilwon Cho; Do Hwan Kim
- Web page: https://patentgrep.com/patent/US20080041300A1

## CPC

- C30B 29/58: Macromolecular compounds
- C08G 61/126: {with a five-membered ring containing one sulfur atom in the ring}
- C30B 7/06: using non-aqueous solvents
- C08G 2261/1412: Saturated aliphatic units
- C08G 2261/3223: containing one or more sulfur atoms as the only heteroatom, e.g. thiophene
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A high quality single-crystalline polyalkylthiophene structure can be easily prepared by the inventive method which comprises: (i) dissolving polyalkylthiophene in an organic solvent at a temperature ranging from 50 to 100° C., sequentially quenching the polyalkylthiophene solution at a temperature ranging from 25 to 40° C. and then at −5 to 15° C., to obtain a self-seeding polyalkylthiophene solution; and (ii) applying the self-seeding polyalkylthiophene solution obtained in step (i) to one surface of a nano-template having a hydrophobic supramolecule coating layer formed thereon to induce self-assembly and crystallization of polyalkylthiophene on the surface.

## Claims

### Claim 1

A method for preparing a single-crystalline polyalkylthiophene structure, which comprises:
(i) (i-a) dissolving polyalkylthiophene in an organic solvent at a temperature ranging from 50 to 100° C., quenching the polyalkylthiophene solution at a temperature ranging from 25 to 40° C. and keeping the quenched solution at that temperature for at least 1 hr, and (i-b) further quenching the solution obtained in step (i-a) at a temperature ranging from −5 to 15° C., followed by stirring at that temperature for a period of 10 to 48 hrs, to obtain a self-seeding polyalkylthiophene solution; and
(ii) applying the self-seeding polyalkylthiophene solution obtained in step (i) to one surface of a nano-template having a hydrophobic supramolecule coating layer formed thereon to induce self-assembly of polyalkylthiophene on the surface and allowing the growth of polyalkylthiophene crystals thereon.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polyalkylthiophene solution used in step (i) has a concentration ranging from 0.1 to 1 mg/ml.

### Claim 3 (depends on 1)

The method of claim 1, wherein the organic solvent used in step (i) is selected from the group consisting of chloroform, toluene, xylene, chlorobenzene, dichlorobenzene, trichlorobenzene and a mixture thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the nano-template used in step (ii) is prepared by coating one surface of a silicon dioxide plate with a hydrophobic supramolecule solution and inducing a condensation reaction thereof at a temperature ranging from 110 to 120° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the hydrophobic supramolecule used in step (ii) is selected from the group consisting of octadecyltrichlorosilane, dodecyltrichlorosilane, hexadecyltrichlorosilane and a mixture thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the nano-template is maintained at a temperature ranging from 10 to 50° C. during the self-seeding solution-application process of step (ii).

### Claim 7 (depends on 1)

The method of claim 1, wherein the process of step (ii) is performed within an air-tight reactor maintained under an Ar atmosphere.

### Claim 8 (depends on 1)

A single-crystalline polyalkylthiophene structure prepared by the method of claim 1.

### Claim 9 (depends on 8)

The single-crystalline polyalkylthiophene structure of claim 8, which has a length of 30 nm to 200 μm and a thickness of 20 nm to 1 μm.

### Claim 10 (depends on 8)

A supramolecular optoelectronic device comprising the single-crystalline polyalkylthiophene structure of claim 8.