# US 2007/0267350 A1 · Pumice Stone with a Carbon Content, Process for Its Production and Its Applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0267350 A1
- Document ID: US20070267350A1
- Status: Published application
- Kind: A1
- Application number: 11/569,678
- Filed: 2005-05-27
- Published: 2007-11-22
- Earliest claimed: 2004-05-28
- Assignees: Sem Stone
- Inventors: Jean-Pierre Camp; Serge Bensaid
- Web page: https://patentgrep.com/patent/US20070267350A1

## CPC

- B01J 20/2803: {Sorbents comprising a binder, e.g. for forming aggregated, agglomerated or granulated products}
- B01J 20/10: comprising silica or silicate
- B01J 20/20: comprising free carbon; comprising carbon obtained by carbonising processes
- B01J 20/28004: {Sorbent size or size distribution, e.g. particle size}
- B01J 20/28011: {Other properties, e.g. density, crush strength}
- B01J 20/28097: {being coated, filled or plugged with specific compounds}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/324: {containing free carbon, e.g. activated carbon}
- C02F 1/681: {by addition of solid materials for removing an oily layer on water}
- C09K 3/32: for absorbing liquids to remove pollution, e.g. oil, gasoline, fat
- C02F 1/281: {using inorganic sorbents}
- C02F 2101/32: Hydrocarbons, e.g. oil
- Y10S 210/925: using chemical agent
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

This pumice stone, which has a carbon content of between 5 and 15% by weight, is capable of adsorbing hydrocarbons but is hydrophobic. It can be applied in decontaminating a sheet of water.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim 8

Pumice stone which has a carbon content of between 5 and 15% by weight, wherein it has a particle size of between 3 and 8 mm and it has a density of less than or equal to 570 kg/m3 and greater than 500 kg/m3.

### Claim 9 (depends on 8)

Pumice stone according to claim 8, wherein it has a mean particle size of 6 mm.

### Claim 10 (depends on 8)

Pumice stone according to claim 8, wherein it has an SiO2 content ranging from 60 to 70% by weight and an Al2O3 content of approximately 17% by weight, the remainder being heterogeneous products.

### Claim 11

Process for the production of a pumice stone which has a carbon content of between 5 and 15% by weight, wherein it has a particle size of between 3 and 8 mm and it has a density of less than or equal to 570 kg/m3 and greater than 500 kg/m3, which comprises causing a pumice stone to adsorb a hydrocarbon and igniting the pumice stone which has adsorbed hydrocarbon in order to incinerate the latter, and freeing the pumice stone, before causing it to adsorb a hydrocarbon, from the fines, basalt, magnetite and volcanic ash which obstruct the pores thereof, by projecting jets of water through a sieve on which the pumice stone is deposited.

### Claim 12

Process for decontaminating a sheet of water contaminated by a hydrocarbon, wherein a pumice stone, which has a carbon content of between 5 and 15% by weight, wherein it has a particle size of between 3 and 8 mm and it has a density of less than or equal to 570 kg/m3 and greater than 500 kg/m3, is spread over the sheet of water, it is left there between two minutes and eight hours (and preferably between three minutes and two hours), then the pumice stone is gathered up and ignited in order to incinerate therefrom the hydrocarbons which it comprises, and these operations are repeated.

### Claim 13 (depends on 12)

Process according to claim 12, wherein the pumice stone is spread in a thickness of 1 to 4 cm.

### Claim 14 (depends on 8)

The pumice stone of claim 8, which has a carbon content of between 10 and 13% by weight.