# US 2007/0259108 A1 · Ultra low residual reflection, low stress lens coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0259108 A1
- Document ID: US20070259108A1
- Status: Published application
- Kind: A1
- Application number: 11/789,646
- Filed: 2007-04-25
- Published: 2007-11-08
- Earliest claimed: 2003-05-23
- Assignees: Optima, Inc.
- Inventors: Glen Koenig; Nicholas Niejelow
- Web page: https://patentgrep.com/patent/US20070259108A1

## CPC

- G02B 1/115: Multilayers
- C03C 17/245: by deposition from the vapour phase
- C03C 17/30: with silicon-containing compounds
- C03C 17/3417: {all coatings being oxide coatings}
- C09D 7/42: Gloss-reducing agents
- C09D 7/61: inorganic
- C23C 14/547: {using optical methods}
- G02B 1/10: Optical coatings produced by application to, or surface treatment of, optical elements (G02B1/08 takes precedence)
- G02B 1/11: Anti-reflection coatings
- C03C 2217/214: Al2O3
- C03C 2217/228: Other specific oxides
- C03C 2217/23: Mixtures
- C03C 2218/15: from the vapour phase
- C03C 2218/154: by sputtering
- C08K 3/22: of metals
- C08K 3/36: Silica
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A method is provided for coating optical lenses and other optical articles with anti-reflection (AR) coatings. The lenses have low reflectivity, provide a substantially white light reflection and have a low stress AR coating and are ideally suited for optical lenses made using a molding procedure which provides a low stress lens substrate. In one aspect the method uses special coating compositions with one being a high index of refraction composition and the other being a low index of refraction composition. In another aspect a method is also disclosed using an optical monitor in conjunction with a conventional vapor deposition apparatus whereby an optical reference lens is used and a particular light frequency of reflected light is measured and this measurement is then used to determine when the desired optical coating is achieved. In a still further aspect the method also preferably calculates the optical thickness of each layer using a specific ratio of blue to green to red colors in the reflected light. The stress of the AR coating is also controlled by adjusting the optical thickness for each layer, if necessary, to minimize the difference in the tensile stresses and compressive stresses between low index/high index layers.

## Claims

### Claim 1

(canceled)

### Claim 2

(canceled)

### Claim 3

(canceled)

### Claim 4

A method for making optical lenses having an anti-reflection (AR) coating comprising the steps of:
supplying an optical lens;
positioning the lens in a vacuum chamber of a vacuum deposition apparatus;
providing in the vacuum chamber a source of at least one high index of refraction AR composition and at least low index of refraction AR composition wherein one of the high index materials comprises a mixture of cerium and titanium oxides and one of the low index materials comprises SiO2;
applying a layer of the high index material on the lens until the desired optical thickness coating is applied;
applying a layer of the low index material on the lens until the desired optical thickness coating is applied; and
repeating the application steps until the desired anti-reflection coating is applied.

### Claim 5 (depends on 4)

The method of claim 4 wherein the cerium oxide is less than about 25% by weight of the composition.

### Claim 6 (depends on 5)

The method of claim 5 wherein the aluminum oxide is less than about 10% by weight of the composition.

### Claim 7

(canceled)

### Claim 8

(canceled)

### Claim 9

(canceled)

### Claim 10

(canceled)

### Claim 11

(canceled)

### Claim 12

(canceled)

### Claim 13

(canceled)

### Claim 14

(canceled)

### Claim 15

(canceled)

### Claim 16

(canceled)

### Claim 17

(canceled)

### Claim 18

(canceled)