# US 2007/0249841 A1 · Band-Shaped High-Temperature Superconductor (HTSL) and Method of Producing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0249841 A1
- Document ID: US20070249841A1
- Status: Published application
- Kind: A1
- Application number: 11/735,540
- Filed: 2007-04-16
- Published: 2007-10-25
- Earliest claimed: 2006-04-20
- Assignees: Trithor GmbH
- Inventors: Michael Backer
- Web page: https://patentgrep.com/patent/US20070249841A1

## CPC

- H10N 60/0828: {Introducing flux pinning centres}
- H10N 60/0324: {from a solution}
- Y10S 505/741: Coating or casting onto a substrate, e.g. screen printing, tape casting
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A band-shaped high-temperature superconductor (HTSL) with high critical current density can be produced economically in a wet-chemical process. In the process, a first precursor solution is applied to a carrier, dried, and annealed. Additional precursor solutions may then be applied, with the first precursor solution contain little or no pinning centers, and any subsequent precursor solutions contains a higher concentration of pinning centers than the first precursor solutions.

## Claims

### Claim 1

A wet-chemical process for the production of a band-shaped HTSL with pinning centers, the method comprising:
(a) applying a base precursor solution to a carrier having a concentration of pinning centers, co;
(b) drying the precursor solution to form a layer;
(c) annealing the layer; and
(d) repeating at least the applying a second precursor solution (a) i times, wherein i is a natural number that is greater than 0,
wherein the concentration co of pinning centers in the base precursor solution is less than the concentration c1 of the second precursor solution applied in the repetition (d).

### Claim 2 (depends on 1)

The process of claim 1, wherein i=1 and 0≦co<c1.

### Claim 3 (depends on 2)

The process of claim 2, wherein co≦ 1/10c1.

### Claim 4 (depends on 3)

The process of claim 3, wherein co≈0.

### Claim 5 (depends on 1)

The process of claim 1, wherein a thickness of the second precursor solution applied in the repetition (d) is greater than the thickness of the base precursor layer applied in (a).

### Claim 6 (depends on 1)

The process of claim 1, wherein pinning centers comprise nanoparticles with a mean grain size of less than about 110 nm.

### Claim 7 (depends on 6)

The process of claim 6, wherein the mean grain size of the nanoparticles is between about 2 nm and about 80 nm,

### Claim 8 (depends on 6)

The process of claim 6, wherein the mean grain size of the nanoparticles is between about 5 nm and about 60 nm.

### Claim 9 (depends on 6)

The process of claim 6, wherein the nanoparticles are substantially inert compared to material forming the HTSL and its educts.

### Claim 10 (depends on 6)

The process of claim 6, wherein a length of at least one component of a lattice vector of the nanoparticles deviates no more than about 10% from a length of a component of a lattice vector of the HTSL.

### Claim 11 (depends on 1)

The process of claim 1, wherein at least a portion of the pinning centers is formed from a substance comprising one or more of zirconium oxide; stabilized zirconium oxide; cerium oxide; barium zirconate; lanthanum zirconate; yttrium oxide; and RE2Ba4CaMoy, wherein RE is any rare-earth metals; M is Zr, Nb, Mo, Ru, Hf, Ta, W or Sn; and y is a rational number that is greater than zero.

### Claim 12

A band-shaped HTSL comprising:
a carrier; and
wet chemical process HTSL layer comprising pinning centers,
wherein the concentration of the pinning centers in the HTSL layer decreases at least in the direction of the carrier.

### Claim 13 (depends on 12)

The band-shaped HTSL of claim 12, wherein:
the HTSL layer comprises:
a bottom surface in contact with the carrier, and
a top, outermost surface,
wherein the top surface of the HTSL layer comprises a greater concentration of pinning centers than the bottom surface of the HTSL layer.

### Claim 14 (depends on 13)

The band shaped HTSL of claim 13, wherein the bottom surface of the HTSL layer is substantially free of pinning centers.

### Claim 15 (depends on 12)

The band-shaped HTSL of claim 12, wherein the pinning centers comprise nanoparticles with a mean grain size of less than about 110 nm.

### Claim 16 (depends on 15)

The band-shaped HTSL of claim 15, wherein the mean grain size of the nanoparticles is between about 2 nm and about 80 nm

### Claim 17 (depends on 15)

The band-shaped HTSL of claim 15, wherein the mean grain size of the nanoparticles is between about 5 nm and about 60 nm.

### Claim 18 (depends on 15)

The band-shaped HTSL of claim 15, wherein the nanoparticles are substantially inert compared to material forming the HTSL layer material and its educts.

### Claim 19 (depends on 15)

The band-shaped HTSL of claim 15, wherein a length of at least one component of a lattice vector of the nanoparticles deviates no more than about 10% from a length of a component of the lattice vector of the HTSL layer.

### Claim 20 (depends on 12)

The band-shaped HTSL of claim 12, wherein a volume proportion of the pinning centers in the HTSL layer is between about 5% and about 25%.

### Claim 21 (depends on 12)

The band-shaped HTSL of claim 12, wherein a volume proportion of the pinning centers in the HTSL layer is between about 10 and about 20%.

### Claim 22 (depends on 12)

The band-shaped HTSL of claim 12, wherein at least a portion of the pinning centers is formed from a substance comprising one or more of zirconium oxide; stabilized zirconium oxide; cerium oxide; barium zirconate; lanthanum zirconate; yttrium oxide; and RE2Ba4CaMoy, wherein RE is any rare-earth metals; M is Zr, Nb, Mo, Ru, Hf, Ta, W or Sn; and y is a rational number that is greater than zero.

### Claim 23 (depends on 12)

The band-shaped HTSL of claim 12, wherein:
the HTSL layer comprises a first layer, a second layer, and a third layer; and
the concentration of the pinning centers in the layers alternate such that the pinning center concentration of the first layer is less than the pinning center concentration of the second layer, and the pinning center concentration of the second layer is greater than the pinning concentration of the third layer.

### Claim 24 (depends on 23)

The band-shaped HTSL of claim 23, wherein the thickness of the second layer is greater than the thicknesses of each the first layer and the third layer.

### Claim 25

A wet-chemical process for the production of a band-shaped HTSL layer with pinning centers, the method comprising:
(a) applying a first precursor solution to a carrier;
(b) drying the solution to form a first precursor layer;
(c) annealing the layer to form a first annealed layer; and
(d) applying a second precursor solution the first annealed layer,
wherein the concentration of pinning centers in the first precursor solution c1 is less than the concentration of the pinning centers in the second precursor solution c2.

### Claim 26 (depends on 25)

The process of claim 25, wherein the concentration of pinning centers in the first precursor solution c1 equals less than about 10% of the concentration of pinning centers in the second precursor solution c2.

### Claim 27 (depends on 25)

The process of claim 25, wherein the first precursor solution is substantially free of pinning centers.

### Claim 28 (depends on 25)

The process of claim 25, further comprising:
(e) drying the second precursor solution to for a second precursor layer;
(f) annealing the second precursor layer to form a second annealed layer; and
(g) applying a third precursor solution to the second annealed layer.
wherein the concentration of pinning centers in the third precursor solution C3 is less than the concentration of the pinning centers in the second precursor solution c2.

### Claim 29 (depends on 28)

The process of claim 28, wherein the thickness of the first precursor layer is less than the thickness of the second precursor layer.