# US 2007/0243372 A1 · Aqueous adhesive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0243372 A1
- Document ID: US20070243372A1
- Status: Published application
- Kind: A1
- Application number: 11/734,808
- Filed: 2007-04-13
- Published: 2007-10-18
- Earliest claimed: 2006-04-13
- Inventors: Douglas Mowrey; James Williams; Stuart Armstrong; Thomas Gaadt
- Web page: https://patentgrep.com/patent/US20070243372A1

## CPC

- C09J 5/02: involving pretreatment of the surfaces to be joined
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 15/06: of {natural rubber or synthetic} rubber
- B32B 15/18: comprising iron or steel {(B32B15/011, B32B15/012 and B32B15/013 take precedence)}
- B32B 25/14: comprising {synthetic rubber copolymers (B32B25/18 and B32B25/20 take precedence)}
- C09J 109/00: Adhesives based on homopolymers or copolymers of conjugated diene hydrocarbons
- C09J 161/06: of aldehydes with phenols
- B32B 2255/06: on metal layer
- B32B 2255/26: Polymeric coating
- B32B 2255/28: Multiple coating on one surface
- B32B 2307/752: Corrosion inhibitor
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L 23/22: Copolymers of isobutene; Butyl rubber; Homopolymers or copolymers of other iso-olefins
- C08L 61/06: of aldehydes with phenols
- C08L 2666/06: Homopolymers or copolymers of unsaturated hydrocarbons; Derivatives thereof
- C08L 2666/16: Addition or condensation polymers of aldehydes or ketones according to C08L59/00 - C08L61/00; Derivatives thereof
- C09J 2409/00: Presence of diene rubber
- C09J 2461/00: Presence of condensation polymers of aldehydes or ketones
- Y10T 428/265: 1 mil or less
- Y10T 428/31877: Phenol-aldehyde
- Y10T 428/31931: Polyene monomer-containing
- Y10T 428/31946: Next to second aldehyde or ketone condensation product
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A two coat adhesive system containing an undercoat having a flexibilizer, a phenolic resin, and an acid; and, a covercoat containing an aqueous phenolic resin, and an aqueous butadiene polymer latex prepared by emulsion polymerization of at least one butadiene monomer in the presence of a polyvinvyl alcohol.

## Claims

### Claim 1

A two coat adhesive system comprising:
an undercoat comprising a flexibilizer, a phenolic resin, and an acid; and,
a covercoat comprising an aqueous phenolic resin, and an aqueous butadiene polymer latex prepared by emulsion polymerization of at least one butadiene monomer in the presence of a polyvinvyl alcohol.

### Claim 2 (depends on 2)

The two coat adhesive system of claim 2, wherein the undercoat further comprises a corrosion inhibitor.

### Claim 3 (depends on 1)

The two coat adhesive system of claim 1, wherein the corrosion inhibitor comprises 5-nitroisophthalic acid.

### Claim 4 (depends on 1)

The two coat adhesive system of claim 1, wherein the acid comprises phosphoric acid.

### Claim 5 (depends on 1)

The two coat adhesive system of claim 1, wherein the aqueous phenolic resin in the covercoat comprises a polyvinyl alcohol stabilized aqueous dispersion of a resole.

### Claim 6 (depends on 1)

The two coat adhesive system of claim 1, wherein the phenolic resin in the undercoat comprises a novolak resin.

### Claim 7 (depends on 1)

The two coat adhesive system of claim 1, wherein the phenolic resin in the undercoat comprises a reaction product of:
(a) a phenolic resin precursor; and
(b) a modifying agent wherein the modifying agent comprises:
(i) at least one functional moiety that enables the modifying agent to react with the phenolic resin precursor; and,
(ii) at least one ionic moiety.

### Claim 8 (depends on 1)

The two coat adhesive system of claim 1, wherein the flexibilizer comprises nitrile rubber latex.

### Claim 9 (depends on 1)

The two coat adhesive system of claim 1, wherein the butadiene polymer is prepared through polymerization of 2,3-dichloro-1,3-butadiene.

### Claim 10 (depends on 1)

The two coat adhesive system of claim 1, wherein the butadiene polymer is prepared by copolymerization of dichlorobutadiene with at least one copolymerizable monomer.

### Claim 11 (depends on 10)

The two coat adhesive system of claim 10, wherein the copolymerizable monomer comprised an α-haloacrylonitrile.

### Claim 12 (depends on 1)

The two coat adhesive system of claim 1, wherein the covercoat is substantially free of a cross linking agent.

### Claim 13 (depends on 1)

The two coat adhesive system of claim 1, wherein the covercoat is substantially free of dinitrosobenzene.

### Claim 14 (depends on 1)

The two coat adhesive system of claim 1, wherein the covercoat thickness ranges from 0.2 to 1.0 mils.

### Claim 15

A method for bonding together two substrates, one of said two substrates comprises a surface containing an electrochemically active metal, said method comprising autodepositing on said metallic substrate an undercoat composition comprising a flexibilizer, a phenolic novolak resin, an acid, and a corrosion inhibitor; drying the undercoat composition; autodepositing a covercoat composition comprising an aqueous phenolic resin, and an aqueous butadiene polymer latex, drying the covercoat composition, and contacting the other of said two substrates with said adhesive-coated one of said two substrates for sufficient time for bonding said two substrates together.

### Claim 16 (depends on 15)

The method of claim 15, wherein the other of said two substrates is an elastomeric material.

### Claim 17 (depends on 15)

The method according to claim 15, further comprising the step of heating the adhesive-coated coated metallic substrate for approximately 10 minutes at 400° F. prior to contacting the other of said two substrates.

### Claim 18 (depends on 15)

The method of claim 15, wherein the acid comprises hydrofluoric acid, phosphoric acid, sulfuric acid, hydrochloric acid or nitric acid.

### Claim 19 (depends on 15)

The method of claim 15, wherein the acid comprises phosphoric acid.

### Claim 20 (depends on 15)

The method of claim 15, wherein the undercoat and covercoat compositions additionally comprise water and are substantially free of volatile organic compounds.

### Claim 21 (depends on 15)

The method of claim 15, dipping the metallic substrate into the undercoat and covercoat compositions to effect autodeposition of the adhesive composition.

### Claim 22 (depends on 15)

The method of claim 15, wherein the dipping is performed at room temperature.