# US 2007/0227728 A1 · Method and lightweight composition for sealing pipe and wellbores

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0227728 A1
- Document ID: US20070227728A1
- Status: Published application
- Kind: A1
- Application number: 11/692,544
- Filed: 2007-03-28
- Published: 2007-10-04
- Earliest claimed: 2006-03-30
- Inventors: Don E. Chambers
- Web page: https://patentgrep.com/patent/US20070227728A1

## CPC

- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C09K 8/473: Density reducing additives, e.g. for obtaining foamed cement compositions
- C04B 2103/0031: {Type C}
- C04B 2103/0036: {Type H}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention provides a method and composition for sealing pipe in wellbores. The composition includes cement, water, gel and laminate particles. The laminate particles are added in a proportion to the cement to provide a weight to the slurry of between 12.5-14.5 pounds per gallon. The cement slurry is pumped down through pipe, such as casing, into the annulus and back up towards the surface. The cement slurry can extend from the producing formation to a location above the producing formation to form a seal. By utilizing the light weight cement slurry, the pipe such as casing can be sealed in a single stage operation.

## Claims

### Claim 1

A method of sealing pipe in a wellbore that penetrates a formation, comprising the steps of:
a) providing a cement slurry comprised of cement, water, gel and laminate particles;
b) locating the cement slurry in an annulus around the pipe;
c) allowing the cement slurry to harden.

### Claim 2 (depends on 1)

The method of claim 1 wherein the step of providing a cement slurry further comprises the step of providing the cement slurry at a weight of 12.5-14.5 pounds per gallon.

### Claim 3 (depends on 1)

The method of claim 1 wherein the step of providing a cement slurry further comprises the step of providing a ratio of laminate particles to cement of 4:94 to 8:94 by weight.

### Claim 4 (depends on 1)

The method of claim 1 wherein the step of providing a cement slurry further comprises the step of providing laminate particles of 250-2000 microns in size.

### Claim 5 (depends on 1)

The method of claim 1 wherein the step of locating the cement slurry further comprises the step of locating the cement slurry in the annulus at the formation and above the formation in order to provide a seal and to protect the pipe from corrosive fluids in the wellbore.

### Claim 6 (depends on 1)

The method of claim 1 wherein:
a) the step of locating the cement slurry further comprises the step of locating the cement slurry, which is a first cement slurry, in the annulus above the formation;
b) locating a second cement slurry that is heavier than the first cement slurry in the annulus at the formation.

### Claim 7 (depends on 6)

The method of claim 6 wherein the step of locating a second cement slurry further comprises the step of providing a second cement slurry having a weight of between 13.5 to 16 pounds per gallon.

### Claim 8 (depends on 6)

The method of claim 6 wherein the second cement slurry further comprises laminate particles.

### Claim 9 (depends on 1)

The method of claim 1 wherein: the step of providing a cement slurry further comprises the steps of providing laminate particles of 250-2000 microns in size, the cement slurry having a weight 12.5-14.5 pounds per gallon and the ratio of laminate particles to cement being in between 4:94 to 8:94 by weight.

### Claim 10

In a wellbore having a pipe that penetrates a formation, the pipe having an annulus, a sealing composition for use in the sealing of the pipe in the wellbore, comprising: cement, water, gel and laminate particles, the sealing composition located in the annulus.

### Claim 11 (depends on 10)

The wellbore of claim 10 wherein the cement is selected from the group containing Type C or Type H Portland cement.

### Claim 12 (depends on 10)

The wellbore of claim 10 wherein the sealing composition forms a slurry having a weight of 12.5-14.5 pounds per gallon.

### Claim 13 (depends on 10)

The wellbore of claim 10 wherein the ratio of laminate particles to cement is 4:94 to 8:94 by weight.

### Claim 14 (depends on 10)

The wellbore of claim 10 wherein the laminate particles are sized between 250-2000 microns.

### Claim 15 (depends on 10)

The wellbore of claim 10, wherein:
a) the sealing composition forms a slurry having a weight of 12.5-14.5 pounds per gallon;
b) the ratio of laminate particles to cement is 4:94 to 8:94 by weight;
c) the laminate particles are sized between 250-2000 microns.

### Claim 16 (depends on 10)

The wellbore of claim 10 wherein the cement slurry extends in the annulus from the formation to a location above the formation so as to protect the pipe from corrosive fluids.

### Claim 17 (depends on 10)

The wellbore of claim 10 wherein the cement slurry is a fist cement slurry and is located in the annulus above the formation, further comprising a second cement slurry that comprises cement, water, gel and laminate particles, the second cement slurry, being heavier than the first cement slurry, the second cement slurry being located in the annulus at the formation.