Photocatalytic material, photocatalyst, photocatalytic product, lighting apparatus, and method of producing photocatalytic material
AssigneeToshiba Lighting & Technology Corporation
InventorsRyotaro Matsuda, Takaya Kamakura, Hideki Okawa, Ariyoshi Ishizaki
Life of this patent
Estimating the term…
Abstract
A photocatalytic material containing tungsten trioxide fine particles having an average particle diameter of 0.5 μm or smaller and a crystal structure of a monoclinic crystal system as a main component.
Claims7
A photocatalytic material containing tungsten trioxide fine particles having an average particle diameter of 0.5 μm or smaller and a crystal structure of a monoclinic crystal system as a main component.
A lighting apparatus comprising a light source, a light transmissive cover substrate enveloping the light source, and a photocatalyst layer formed on an outer face or an inner face of the cover substrate and containing tungsten trioxide fine particles having an average particle diameter of 0.1 μm or smaller and a crystal structure of a monoclinic crystal system.
A lighting apparatus comprising a light source, a reflection plate substrate set optically on the opposite to the light source, and a photocatalyst layer formed on the reflection plate substrate and containing tungsten trioxide fine particles having an average particle diameter of 0.1 μm or smaller and a crystal structure of a monoclinic crystal system.
A method of producing a photocatalytic material comprising the steps of producing a granular raw material by spraying an aqueous solution containing 1 to 20% by weight of ammonium para-tungstate in high temperature atmosphere, and forming tungsten trioxide fine particles having a crystal structure of a monoclinic crystal system by heating the granular raw material at 700 to 800° C. for 1 to 10 minutes.
A method of producing a photocatalytic material comprising the steps of dissolving ammonium para-tungstate in a water-based solvent and successively carrying out recrystallization, and forming a tungsten trioxide photocatalytic material by firing the obtained crystal in conditions of 600° C. or higher for 15 seconds or longer.