# US 2007/0087244 A1 · Membrane-electrode assembly, polymer membranes for a membrane-electrode assembly, polymer electrolyte fuel cells, and methods for the production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0087244 A1
- Document ID: US20070087244A1
- Status: Published application
- Kind: A1
- Application number: 11/183,873
- Filed: 2005-07-19
- Published: 2007-04-19
- Earliest claimed: 2003-01-20
- Assignees: Sartorius AG
- Inventors: Dieter Melzner; Annette Reiche; Ulrich Maehr; Suzana Kiel
- Web page: https://patentgrep.com/patent/US20070087244A1

## CPC

- H01M 8/1081: starting from solutions, dispersions or slurries exclusively of polymers
- H01M 8/0289: Means for holding the electrolyte (solid polymer electrolytes H01M8/1018)
- H01M 8/1027: having carbon, oxygen and other atoms, e.g. sulfonated polyethersulfones [S-PES]
- H01M 8/103: having nitrogen, e.g. sulfonated polybenzimidazoles [S-PBI], polybenzimidazoles with phosphoric acid, sulfonated polyamides [S-PA] or sulfonated polyphosphazenes [S-PPh]
- H01M 8/1032: having sulfur, e.g. sulfonated-polyethersulfones [S-PES]
- H01M 8/1048: Ion-conducting additives, e.g. ion-conducting particles, heteropolyacids, metal phosphate or polybenzimidazole with phosphoric acid
- H01M 8/1067: characterised by their physical properties, e.g. porosity, ionic conductivity or thickness
- H01M 2300/0082: Organic polymers
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 156/10: Methods of surface bonding and/or assembly therefor
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A membrane-electrode assembly and polymer electrolyte fuel cells and methods of production thereof, in which a polymer membrane, containing at least one basic polymer membrane, is sandwiched between two flat gas diffusion electrodes each of which is loaded with a dopant, whereby after reaching a mass transport equilibrium for the exchange of the dopant between the gas diffusion electrodes and the polymer membrane, the polymer membrane has a conductivity of at least 0.1 S/m at a temperature of no less than 25° C.

## Claims

### Claim 1

A membrane-electrode assembly comprising
two flat gas diffusion electrodes each loaded with a dopant, and
a polymer membrane comprising at least one basic polymer, the polymer membrane sandwiched between said electrodes,
wherein after reaching a mass transport equilibrium for the exchange of the dopant between the gas diffusion electrodes and the polymer membrane, the polymer membrane has a conductivity of at least 0.1 S/m at a temperature of no less than 25° C .

### Claim 2 (depends on 1)

The membrane-electrode assembly as claimed in claim 1, wherein at least one basic polymer is selected from the group consisting of polybenzimidazoles, polypyridines, polypyrimidines, polyimidazoles, polybenzthiazoles, polybenzoxazoles, polyoxadizoles, polyquinoxalines, polythiadiazoles, poly(tetraazapyrenes) and a copolymer.

### Claim 3 (depends on 2)

The membrane-electrode assembly as claimed in claim 2, wherein at least one basic polymer is polybenzimidazole.

### Claim 4 (depends on 1)

The membrane-electrode assembly as claimed in claim 1, wherein the polymer membrane is a dry undoped polymer membrane produced by industrial machine drawing.

### Claim 5 (depends on 4)

The membrane-electrode assembly as claimed in claim 4, wherein the polymer membrane is crosslinked by reaction with polyfunctional crosslinking agents.

### Claim 6 (depends on 5)

The membrane-electrode assembly as claimed in claim 5, wherein the crosslinking agent comprises one or more of epoxy groups and isocyanate groups.

### Claim 7 (depends on 1)

The membrane-electrode assembly as claimed in claim 1, wherein the polymer membrane is a plasticized polymer membrane comprising no more than 40 wt % plasticizer.

### Claim 8 (depends on 7)

The membrane-electrode assembly as claimed in claim 7, wherein the plasticizer is a reaction product of at least a dibasic acid and an organic compound.

### Claim 9 (depends on 7)

The membrane-electrode assembly as claimed in claim 7, wherein the organic compound is phosphoric acid diester.

### Claim 10 (depends on 8)

The membrane-electrode assembly as claimed in claim 8, wherein the organic compound is phosphoric acid diester.

### Claim 11 (depends on 8)

The membrane-electrode assembly as claimed in claim 8, wherein the phosphoric acid diester is one or more of di-(2-ethylhexyl)phosphoric acid ester and diphenyl phosphoric acid ester.

### Claim 12 (depends on 1)

The membrane-electrode assembly as claimed in claim 1, wherein the dopant content in the gas diffusion electrodes is 60% to 120% of the weight of the basic polymer in the polymer membrane.

### Claim 13 (depends on 12)

The membrane-electrode assembly as claimed in claim 12, wherein the dopant is a polybasic inorganic acid.

### Claim 14 (depends on 13)

The membrane-electrode assembly as claimed in claim 13, wherein the acid is phosphoric acid.

### Claim 15

A polymer membrane for a membrane-electrode assembly comprising at least one basic polymer with a stress at failure of more than 110 N/mm2 at room temperature and an elongation of more than 6%.

### Claim 16 (depends on 15)

The polymer membrane as claimed in claim 15, wherein the polymer membrane is crosslinked with a bifunctional crosslinking agent.

### Claim 17 (depends on 16)

The polymer membrane as claimed in claim 16, wherein the polymer membrane is plasticized with a plasticizer, wherein the plasticizer is a reaction product of at least a dibasic acid and an organic compound.

### Claim 18 (depends on 17)

The polymer membrane as claimed in claim 17, wherein the polymer membrane consists of polybenzimidazole and 1,4-butanediol diglycidyl ether and wherein the plasticizer is di-(2-ethylhexyl)phosphate.

### Claim 19

A polymer electrolyte fuel cell comprising a membrane-electrode assembly arranged between bipolar plates, the membrane electrode assembly comprising:
two flat gas diffusion electrodes each loaded with a dopant, and
a polymer membrane comprising at least one basic polymer, the polymer membrane sandwiched between said electrodes,
wherein after reaching a mass transport equilibrium for the exchange of the dopant between the gas diffusion electrodes and the polymer membrane, the polymer membrane has a conductivity of at least 0.1 S/m at a temperature of no less than 25° C.

### Claim 20

A method for producing a membrane-electrode assembly comprising:
a) impregnating each of two flat gas diffusion electrodes with a dopant up to a dopant content of 60% to 120% of the weight of a basic polymer in a polymer membrane,
b) sandwiching the polymer membrane between the impregnated gas diffusion electrodes,
c) arranging the sandwiched structure between two press plates,
d) hot pressing the arrangement at a temperature of about 50° C. to 250° C. and a pressure of at least 1 bar for between about 5 seconds to 60 minutes.

### Claim 21 (depends on 20)

The method for producing a membrane-electrode assembly as claimed in claim 20, wherein the steps (a) through (d) are performed in a continuous process.

### Claim 22

A method for producing a dry undoped polymer membrane comprising:
casting a polymer casting solution on a substrate of a membrane drawing machine, wherein the polymer casting solution comprises at least one basic polymer and a solvent,
evaporating the solvent at a first element temperature, and
after drying the membrane at a second temperature higher than the first element temperature.

### Claim 23 (depends on 22)

The method as claimed in claim 22, further comprising adding a polyfinctional crosslinking agent to the polymer casting solution.

### Claim 24 (depends on 23)

The method as claimed in claim 23, wherein the crosslinking agent comprises one or more of epoxy groups and isocyanate groups.

### Claim 25 (depends on 22)

The method as claimed in claim 22, further comprising adding a plasticizer to the casting solution after about 5 to 15 minutes and heating the casting solution to a temperature between about 60° C. and 140° C. over a period of time between 12 minutes and 2 hours.

### Claim 26 (depends on 22)

The method as claimed in claim 22, further comprising adding a plasticizer to the casting solution after 8 to 12 minutes and heating the casting solution to a temperature between 60 ° C. and 140° C. over a period of time between 12 minutes and 2 hours.

### Claim 27 (depends on 25)

The method as claimed in claim 25, wherein the plasticizer is a reaction product of at least dibasic acid and an organic compound.

### Claim 28 (depends on 26)

The method as claimed in claim 26, wherein the plasticizer is a reaction product of at least a dibasic acid and an organic compound.

### Claim 29 (depends on 25)

The method as claimed in claim 25, wherein the plasticizer is di-(2-ethylhexyl) phosphate or diphenyl phosphoric acid ester.

### Claim 30 (depends on 26)

The method as claimed in claim 26, wherein the plasticizer is di-(2-ethylhexyl) phosphate or diphenyl phosphoric acid ester.

### Claim 31 (depends on 27)

The method as claimed in claim 27, wherein the plasticizer is di-(2-ethylhexyl) phosphate or diphenyl phosphoric acid ester.

### Claim 32 (depends on 28)

The method as claimed in claim 28, wherein the plasticizer is di-(2-ethylhexyl) phosphate or diphenyl phosphoric acid ester.

### Claim 33

A method for producing a polymer electrolyte fuel cell comprising:
a) impregnating each of two flat gas diffusion electrodes with a dopant up to a dopant content of 60% to 120% of the weight of a basic polymer in a polymer membrane,
b) sandwiching the polymer membrane between the doped gas diffusion electrodes,
c) arranging the sandwiched structure between two bipolar plates of a polymer electrolyte fuel cell,
d) applying a contact pressure on the polymer membrane-electrode sandwiched in the fuel cell at a temperature of about 50° C. and 250° C. and exposing the fuel cell to reactive gases over a period of time between about one minute and ten hours.

### Claim 34 (depends on 33)

The method for producing a polymer electrolyte fuel cell as claimed in claim 33, wherein the reactive gases are hydrogen and air.