# US 2007/0072320 A1 · Process for producing an epitalixal layer of galium nitride

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0072320 A1
- Document ID: US20070072320A1
- Status: Published application
- Kind: A1
- Application number: 11/519,702
- Filed: 2006-09-11
- Published: 2007-03-29
- Earliest claimed: 2000-07-07
- Assignees: Lumilog
- Inventors: Eric Frayssinet; Bernard Beaumont; Jean-Pierre Faurie; Pierre Gibart
- Web page: https://patentgrep.com/patent/US20070072320A1

## CPC

- C30B 25/02: Epitaxial-layer growth
- C30B 25/18: characterised by the substrate
- C30B 29/40: AIIIBV compounds {wherein A is B, Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C30B 29/406: {Gallium nitride}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10P 14/3438: {Doping during depositing}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a low defect density GaN material comprising at least two step of growing epitaxial layers of GaN with differences in growing conditions, (a.) a first step of growing an epitaxial layer GaN on an epitaxially compentent layer under first growing conditions selected to induce island features formation, followed by (b.) a second step of growing an epitaxial layer of GaN under second growing conditions selected to enhance lateral growth until coalescence.

## Claims

### Claim 1

A method of manufacturing a low defect density GaN material comprising at least two step of growing epitaxial layers of GaN with differences in growing conditions,
a. a first step of growing an epitaxial layer GaN on an epitaxially competent layer under first growing conditions selected to induce island features formation, followed by
b. a second step of growing an epitaxial layer of GaN under second growing conditions selected to enhance lateral growth until coalescence.

### Claim 2 (depends on 1)

The method of claim 1, wherein the differences in growing conditions are selected among the group consisting of differences in temperature and differences in composition of the vapour phase and combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the temperature of the said second growing conditions is higher than the temperature of the said first growing conditions.

### Claim 4 (depends on 3)

The method of claim 3, wherein the temperature of the first growing conditions is below 1060° C.

### Claim 5 (depends on 3)

The method of claim 3, wherein the temperature of the first growing conditions is below 1000° C.

### Claim 6 (depends on 3)

The method of claim 3 wherein the temperature of the first growing conditions is comprised between about 950° C. and about 1060° C.

### Claim 7 (depends on 3)

The method of claim 3, wherein the temperature of the first growing conditions is below 950° C.

### Claim 8 (depends on 3)

The method of claim 3, wherein the temperature of the first growing conditions is comprised between about 500° C. and about 1000° C.

### Claim 9 (depends on 3)

The method of claim 3, wherein the temperature of the second growing conditions is above 1000° C.

### Claim 10 (depends on 3)

The method of claim 3, wherein the temperature of the second growing conditions is comprised between about 1015° C. and about 1020° C.

### Claim 11 (depends on 3)

The method of claim 3, wherein the temperature of the second growing conditions is above 1060° C.

### Claim 12 (depends on 3)

The method of claim 3, wherein the temperature of the second growing conditions is about 1080° C.

### Claim 13 (depends on 3)

The method of claim 3, wherein the temperature of the first growing conditions is about 1060° C. and the temperature of the second growing conditions is about 1080° C.

### Claim 14 (depends on 3)

The method of claim 3, wherein the temperature of the first growing conditions is comprised between about 900° C. and about 950° C. and the temperature of the second growing conditions is comprised between about 1015° C. and 1020° C.

### Claim 15 (depends on 3)

The method of claim 3, wherein the temperature of the first growing conditions is comprised between 450° C. and 600° C. and the temperature of the second growing conditions is about 1080° C.

### Claim 16 (depends on 3)

The method of claim 3, wherein oxygen is added to the vapour phase of the first growing conditions to induce island features formation.

### Claim 17 (depends on 16)

The method of claim 16, wherein oxygen is excluded from the second growing conditions to induce enhanced lateral growth.

### Claim 18 (depends on 1)

The method of claim 1, wherein oxygen pressure in the vapour phase of the first growing conditions is above oxygen pressure in the vapour phase of the second growing conditions.

### Claim 19 (depends on 17)

The method of claim 17, wherein oxygen is excluded from the second growing conditions to induce enhanced lateral growth.

### Claim 20 (depends on 1)

The method of claim 1, wherein the first growing conditions comprise a temperature of between 900° C. and 950° C. and an oxygen pressure Pose in the vapour phase such that the ratio Pox/PGaCl is greater than 0.0005, and the second growing conditions comprise a temperature of between about 1000° C. and 1050° C. without oxygen in the vapour phase.

### Claim 21 (depends on 1)

The method of claim 1, wherein Mg and/or Sb is added to the vapour phase of the second growing conditions.

### Claim 22 (depends on 1)

The method of claim 1, wherein the substrate comprises a base layer and an upper crystalline layer compatible with the growth of the nitride crystal.

### Claim 23 (depends on 22)

The method of claim 22, wherein the upper crystalline layer is chosen among the group consisting of sapphire, spinel, GaN, AlN, GaAs, Si, SiC (6H—, 4H—, 3C—), LiAlO2, LiGaO2, ZrB2, HfB2 and mixtures thereof.

### Claim 24 (depends on 23)

The method of claim 23, wherein the upper layer is an AlN or GaN crystalline material.

### Claim 25 (depends on 22)

The method of claim 22, wherein the base layer is a sapphire layer.

### Claim 26 (depends on 22)

The method of one of claim 22, wherein the substrate comprises at least one sacrificial layer between the base layer and the upper layer.

### Claim 27 (depends on 1)

The method of claim 1, wherein the low defect density GaN material is a single crystal.

### Claim 28 (depends on 27)

The method of claim 27, wherein the single crystal has a thickness of more than 1 μm.

### Claim 29 (depends on 27)

The method of claim 27, wherein the single crystal has a thickness ranging from 100 μm to 10 cm.

### Claim 30 (depends on 27)

The method of claim 27, wherein the single crystal has a thickness ranging from 500 μm to 3 mm.

### Claim 31 (depends on 1)

The method of one of claims 1, wherein the low defect density GaN material is removed from the substrate layer.

### Claim 32 (depends on 31)

The method of claim 31, wherein it comprises a further step of wafering of the low defect density GaN material.

### Claim 33 (depends on 1)

A low defect density GaN material obtainable by the method of claim 1.

### Claim 34 (depends on 1)

A free standing GaN obtainable by a method of claim 1, wherein the measured lifetime of time resolved photoluminescence (TPRL) of the PL peak corresponding to electron-hole plasma under high excitation 0.4 mJ/cm2 at room temperature is higher than 400 ps.

### Claim 35 (depends on 34)

The free standing GaN of claim 34, wherein the measured lifetime of time resolved photoluminescence (TPRL) of the PL peak corresponding to electron-hole plasma under high excitation 0.4 mJ/cm2 at room temperature is higher than 800 ps.

### Claim 36 (depends on 34)

The free standing GaN according to claim 34, where the TD densities are 106 cm−2.