# US 2007/0062479 A1 · Piston for internal combustion engine

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0062479 A1
- Document ID: US20070062479A1
- Status: Published application
- Kind: A1
- Application number: 11/524,271
- Filed: 2006-09-21
- Published: 2007-03-22
- Earliest claimed: 2005-09-21
- Assignees: Honda Motor Co., Ltd.
- Inventors: Akito Tanihata; Naoko Sato; Hisayasu Kojima; Kouji Katsumata; Takashi Shiraishi
- Web page: https://patentgrep.com/patent/US20070062479A1

## CPC

- B22D 17/2069: {Exerting after-pressure on the moulding material}
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- F02B 75/08: Engines with means for preventing corrosion in gas-swept spaces
- F02F 3/0084: {the pistons being constructed from specific materials}
- F02F 2200/06: Casting
- F05C 2201/903: Aluminium alloy, e.g. AlCuMgPb F34,37
- Y10T 29/49261: by composite casting or molding
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- F02B: INTERNAL-COMBUSTION PISTON ENGINES; COMBUSTION ENGINES IN GENERAL (gas-turbine plants F02C; hot-gas or combustion-product positive-displacement engine plants F02G)
- F02F: CYLINDERS, PISTONS OR CASINGS, FOR COMBUSTION ENGINES; ARRANGEMENTS OF SEALINGS IN COMBUSTION ENGINES
- F05C: INDEXING SCHEME RELATING TO MATERIALS, MATERIAL PROPERTIES OR MATERIAL CHARACTERISTICS FOR MACHINES, ENGINES OR PUMPS OTHER THAN NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A piston for internal combustion engine has both fatigue strength and wear resistance without increased production cost. At least one of a combustion chamber surface, a skirt rib, a pin boss rib which connects a pin boss and a crown, a lower portion of the pin boss casting surface, and a surface layer including the casting surface is a first eutectic structure in which primary crystal Si does not crystallize. A top ring groove and a pin holing of a piston pin are finished surfaces obtained by eliminating the surface layer by means of machining. The layer including the finished surface is a second eutectic structure in which the primary crystal Si crystallizes.

## Claims

### Claim 1

A piston for internal combustion engine obtained by die-casting a hypereutectic Al—Si alloy comprising 11 to 18 wt % of Si, the piston comprising:
a piston crown whose top face is a combustion chamber surface;
a piston skirt portion;
a pin holing of a piston pin;
a pin boss which the pin holing of a piston pin pierces; and
a top ring groove formed on an outer peripheral surface,
wherein at least one of the combustion chamber surface, a pin boss rib which connects the pin boss and the crown, an outer peripheral surface of a lower portion of the pin boss, and a skirt rib which connects the pin boss and the piston skirt portion is a casting surface,
a surface layer including the casting surface is composed of a first eutectic structure in which the primary crystal Si does not crystallize,
at least one of the top ring groove and the pin holing of a piston pin is a finished surface which is obtained by eliminating the surface layer, and
a layer including the finished surface is composed of a second eutectic structure in which the primary crystal Si crystallizes.

### Claim 2 (depends on 1)

The piston for internal combustion engine according to claim 1, wherein the piston further comprises at least one of 1.0 to 6.0 wt % of Cu, 1.0 to 6.0 wt % of Ni, 0.5 to 2.0 wt % of Mg, 0.1 to 2.0 wt % of Fe and 30 to 200 ppm of P, and the remainder is composed of Al and unavoidable impurities.

### Claim 3 (depends on 1)

The piston for internal combustion engine according to claim 1, wherein the piston further comprises 0.01 to 0.3 wt % of at least one of Mn, Cr, Ti, V and Zr in total.

### Claim 4 (depends on 2)

The piston for internal combustion engine according to claim 2, wherein the piston further comprises 0.01 to 0.3 wt % of at least one of Mn, Cr, Ti, V and Zr in total.

### Claim 5

A method of manufacturing a piston for internal combustion engine of a die-cast hypereutectic Al—Si alloy containing 11 to 18 wt % of Si, the method comprising the step of repressurizing molten metal rapidly after injection of the molten metal into a mold is completed.

### Claim 6 (depends on 5)

The method of manufacturing a piston for internal combustion engine according to claim 5, wherein the molten metal is repressurized within 1.5 seconds after the injection of the molten metal into the mold is completed.