# US 2007/0059943 A1 · Ion-assisted oxidation methods and the resulting structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2007/0059943 A1
- Document ID: US20070059943A1
- Status: Published application
- Kind: A1
- Application number: 11/545,017
- Filed: 2006-10-09
- Published: 2007-03-15
- Earliest claimed: 1998-09-03
- Assignees: Micron Technology, Inc.
- Inventors: Li Li; Pai-Hung Pan
- Web page: https://patentgrep.com/patent/US20070059943A1

## CPC

- H10P 14/6539: {by exposure to corpuscular radiation, e.g. exposure to electrons, alpha-particles, protons or ions}
- H10D 30/0223: {having source and drain regions or source and drain extensions self-aligned to sides of the gate}
- H10D 64/013: {of electrodes having a conductor capacitively coupled to a semiconductor by an insulator}
- H10D 64/516: {the thicknesses being non-uniform}
- H10P 14/6304: {Formation by oxidation, e.g. oxidation of the substrate}
- H10W 10/0125: {comprising introducing electrical impurities in local oxidation regions, e.g. to alter LOCOS oxide growth characteristics}
- H10W 10/13: formed using local oxidation of silicon [LOCOS], e.g. sealed interface localised oxidation [SILO] or side-wall mask isolation [SWAMI]
- H10D 84/0128: {Manufacturing their channels}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/208: {of electrically inactive species}
- Y10S 148/116: Oxidation, differential
- Y10S 148/118: Oxide films
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Oxidation methods and resulting structures including providing an oxide layer on a substrate and then re-oxidizing the oxide layer by vertical ion bombardment of the oxide layer in an atmosphere containing at least one oxidant. The oxide layer may be provided over diffusion regions, such as source and drain regions, in a substrate. The oxide layer may overlie the substrate and is proximate a gate structure on the substrate. The at least one oxidant may be oxygen, water, ozone, or hydrogen peroxide, or a mixture thereof. These oxidation methods provide a low-temperature oxidation process, less oxidation of the sidewalls of conductive layers in the gate structure, and less current leakage to the substrate from the gate structure.

## Claims

### Claim 1

An oxidation method, comprising:
providing a semiconductor substrate including silicon oxide on a portion of a surface thereof; and
bombarding at least one of oxygen atoms of the silicon oxide and oxygen atoms proximate to the silicon oxide with at least one inert ion in an atmosphere consisting essentially of the at least one ion of an inert atom, hydrogen, and at least one oxidant to energize the oxygen atoms and to increase a thickness of the silicon oxide.

### Claim 2 (depends on 1)

The oxidation method of claim 1, wherein providing the semiconductor substrate comprises providing a silicon substrate.

### Claim 3 (depends on 1)

The oxidation method of claim 1, further comprising:
forming the silicon oxide.

### Claim 4 (depends on 1)

The oxidation method of claim 1, wherein bombarding comprises bombarding a region of the silicon oxide with krypton, helium, or argon ions.

### Claim 5 (depends on 1)

The oxidation method of claim 1, wherein bombarding is effected in the presence of at least one oxidant comprising at least one of oxygen, water, ozone, and hydrogen peroxide.

### Claim 6 (depends on 5)

The oxidation method of claim 5, wherein bombarding is effected in the presence of at least water and the hydrogen results from oxidizing effected with the water.

### Claim 7 (depends on 1)

The oxidation method of claim 1, wherein bombarding is effected at a temperature of about 25° C. to about 700° C.

### Claim 8 (depends on 1)

The oxidation method of claim 1, wherein bombarding is effected for a duration of from about 5 minutes to about 500 minutes.

### Claim 9 (depends on 1)

The oxidation method of claim 1, wherein bombarding is effected at an energy of from about 1 eV to about 300 eV.

### Claim 10 (depends on 1)

The oxidation method of claim 1, further comprising:
forming at least one diffusion region in the semiconductor substrate beneath the silicon oxide.

### Claim 11 (depends on 10)

The oxidation method of claim 10, wherein forming is effected before the bombarding.

### Claim 12 (depends on 1)

The oxidation method of claim 1, wherein bombarding comprises vertical ion bombardment.

### Claim 13 (depends on 1)

The oxidation method of claim 1, wherein providing comprises providing a semiconductor substrate with a damaged silicon oxide region.

### Claim 14 (depends on 1)

The oxidation method of claim 1, including flowing the hydrogen through the atmosphere at a rate ranging from about 1 sccm to about 200 sccm.

### Claim 15 (depends on 1)

The oxidation method of claim 1, bombarding is effected with the hydrogen present in the atmosphere in a concentration sufficient to passivate growth of oxide on surfaces that are substantially parallel to a direction of bombardment.

### Claim 16

An oxidation method, comprising:
providing a semiconductor device structure comprising:
a semiconductor substrate with at least one diffusion region formed therein;
silicon oxide positioned on the semiconductor substrate and over the at least one diffusion region; and
a structure positioned on the semiconductor substrate, laterally adjacent to the at least one diffusion region; and
bombarding oxygen atoms located substantially over the at least one diffusion region with at least one ion of an inert atom in an atmosphere consisting essentially of the at least one ion, hydrogen, and at least one oxidant.

### Claim 17 (depends on 16)

The oxidation method of claim 16, wherein bombarding increases a thickness of the silicon oxide without substantially oxidizing the structure.

### Claim 18 (depends on 16)

The oxidation method of claim 16, wherein providing the semiconductor device structure comprises providing a semiconductor device structure comprising a silicon substrate.

### Claim 19 (depends on 16)

The oxidation method of claim 16, wherein providing the semiconductor device structure comprises providing a semiconductor device structure with the structure comprising at least a portion of a transistor gate structure.

### Claim 20 (depends on 16)

The oxidation method of claim 16, further comprising:
oxidizing the semiconductor substrate to form the silicon oxide.

### Claim 21 (depends on 16)

The oxidation method of claim 16, wherein bombarding comprises bombarding the oxygen atoms with krypton, helium, or argon ions.

### Claim 22 (depends on 16)

The oxidation method of claim 16, wherein bombarding is effected in the presence of at least one oxidant comprising at least one of oxygen, water, ozone, and hydrogen peroxide.

### Claim 23 (depends on 22)

The oxidation method of claim 22, wherein bombarding is effected in the presence of at least water, and the hydrogen results from oxidizing effected with the water.

### Claim 24 (depends on 16)

The oxidation method of claim 16, wherein bombarding is effected at a temperature of from about 25° C. to about 700° C.

### Claim 25 (depends on 16)

The oxidation method of claim 16, wherein bombarding is effected for a duration of about 5 minutes to about 50 minutes.

### Claim 26 (depends on 16)

The oxidation method of claim 16, wherein bombarding is effected at an energy of from about 1 eV to about 300 eV.

### Claim 27 (depends on 16)

The oxidation method of claim 16, wherein bombarding comprises vertical ion bombardment.

### Claim 28 (depends on 16)

The oxidation method of claim 16, wherein providing the semiconductor substrate comprises providing a semiconductor substrate having a region of damaged silicon oxide on a surface thereof.

### Claim 29 (depends on 16)

The oxidation method of claim 16, including flowing the hydrogen into the atmosphere at a rate ranging from about 1 sccm to about 200 sccm.

### Claim 30 (depends on 16)

The oxidation method of claim 16, wherein bombarding is effected with the hydrogen present in the atmosphere in a concentration sufficient to passivate the growth of oxide on surfaces substantially parallel to a direction of bombardment.