Back to results
US 2006/0290023 A1Published application
Method of manufacturing a rubber woven rug
OwnerSanjeev Suseelaninventor
Life of this patent
Estimating the term…
Abstract
A method of manufacturing a rubber woven rug, the method comprising the steps of: mixing raw materials; extruding the raw materials through at least one mould to produce a rubber yarn; vulcanizing the rubber yarn in a steam chamber to provide vulcanized yarn; loading vulcanized yarn on a loom; and weaving said vulcanized yarn to provide a rubber woven rug.
Claims23
A method of manufacturing a rubber woven rug, said method comprising the steps of:
- mixing raw materials;
- extruding said raw materials through at least one mould to produce a rubber yarn;
- vulcanizing said rubber yarn in a steam chamber to provide vulcanized yarn;
- loading said vulcanized yarn on a loom;
- and
- weaving said vulcanized yarn to provide a rubber woven rug.
3 more elements
A method of manufacturing a rubber woven rug, said method comprising the steps of:
- mixing raw materials, wherein said raw materials are between 15 and 20 percent natural rubber, between 15 and 20 percent reclaimed rubber, between 0.1 and 1.0 percent stearic acid, between 0.1 and 1 percent zinc oxide, between 0.1 and 1.0 percent sulphur, between 20 and 40 percent barites, between 0.1 and 1.0 percent mer cure, between 5 and 15 percent rubber process oil and between 10 and 20 percent tyre powder;
- extruding said raw materials through at least one mould to produce a rubber yarn;
- vulcanizing said rubber yarn in a steam chamber to provide vulcanized yarn;
- loading said vulcanized yarn on a loom;
- and
- weaving said vulcanized yarn to provide a rubber woven rug.
3 more elements
A method of manufacturing a rubber woven rug, said method comprising the steps of:
- mixing raw materials wherein said raw materials are about 17.5 percent natural rubber, 17.5 percent reclaimed rubber, 0.65 percent stearic acid, 0.60 percent zinc oxide, 0.45 percent sulphur, 35 percent barites, 0.3 percent mer cure, 10.5 percent rubber process oil and 17.5 percent tyre powder;
- extruding said raw materials through at least one mould to produce a rubber yarn;
- vulcanizing said rubber yarn in a steam chamber to provide vulcanized yarn;
- loading said vulcanized yarn on a loom;
- and
- weaving said vulcanized yarn to provide a rubber woven rug.
3 more elements
Dependencies are inferred from the claim text.