# US 2006/0223217 A1 · Photodiode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0223217 A1
- Document ID: US20060223217A1
- Status: Published application
- Kind: A1
- Application number: 10/556,460
- Filed: 2004-05-14
- Published: 2006-10-05
- Earliest claimed: 2003-05-14
- Assignees: University College Cork, National University of Ireland, Cork
- Inventors: John Jackson; John Alderman; Alan Mathewson
- Web page: https://patentgrep.com/patent/US20060223217A1

## CPC

- H10F 30/225: the potential barrier working in avalanche mode, e.g. avalanche photodiodes
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

The invention provides a method of manufacturing an avalanche diode comprising the steps of applying a mask (6) over an active diode region (5) in a wafer (1), and damaging the region the surrounding the active diode region by breaking bonds in the semiconductor lattice to provide gettering sites in this surrounding region.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A method of manufacturing an avalanche diode comprising the steps of;
applying a mask over an active diode region in a wafer,
damaging the region surrounding the active diode region by breaking bonds in the semiconductor lattice to provide gettering sites in this surrounding region.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the surrounding region is damaged by subjecting it to doping.

### Claim 16 (depends on 14)

The method as claimed in claim 14, wherein the surrounding region is damaged by subjecting both the mask and the surrounding region to doping.

### Claim 17 (depends on 14)

The method as claimed in claim 14, comprising the further step of heating to cause diffusion of cathode ions from the mask into the underlying material to form a cathode.

### Claim 18 (depends on 14)

The method as claimed in claim 14, comprising the further step of heating to cause diffusion of cathode ions from the mask into the underlying material to form a cathode; and wherein the mask is of a material which acts to draw defects from the underlying material during the process.

### Claim 19 (depends on 14)

The method as claimed in claim 14, comprising the further step of heating to cause diffusion of cathode ions from the mask into the underlying material to form a cathode; and wherein the mask is of a material which acts to draw defects from the underlying material during the process; and wherein the doping is performed so that a top layer of the mask has a high concentration of defects which have diffused from the underlying material.

### Claim 20 (depends on 18)

The method as claimed in claim 18, wherein the mask is of a polycrystalline material.

### Claim 21 (depends on 18)

The method as claimed in claim 18, wherein the mask is of polysilicon material.

### Claim 22 (depends on 14)

The method as claimed in claim 14, wherein the surrounding region has the same doping as the anode.

### Claim 23 (depends on 14)

The method as claimed in claim 14, wherein the surrounding region is damaged by subjecting it to doping; and wherein the doping is performed by arsenic implanting.

### Claim 24 (depends on 14)

The method as claimed in claim 14, comprising the further steps of growing an oxide ring around the diode active region.

### Claim 25 (depends on 14)

The method as claimed in claim 14, comprising the further steps of growing an oxide ring around the diode active region; and wherein doping is performed within the oxide ring.

### Claim 26 (depends on 14)

The method as claimed in claim 14, comprising the further steps of growing an oxide ring around the diode active region; and comprising the further steps of applying a bridge from the mask to the oxide to form an Ohmic contact for the diode.