- Web page: https://patentgrep.com/patent/US20060218770A1

## CPC

- B29C 33/56: Coatings {, e.g. enameled or galvanised}; Releasing, lubricating or separating agents {(in-mould coating B29C37/0028; using or applying separating agents B29C37/0067)}
- B22D 17/2209: {Selection of die materials (for permanent moulds B22C9/061)}
- C23C 24/10: with intermediate formation of a liquid phase in the layer
- C23C 24/103: {Coating with metallic material, i.e. metals or metal alloys, optionally comprising hard particles, e.g. oxides, carbides or nitrides}
- C23C 28/00: Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- C23C 28/321: {with at least one metal alloy layer}
- C23C 28/322: {only coatings of metal elements only}
- C23C 28/34: {including at least one inorganic non-metallic material layer, e.g. metal carbide, nitride, boride, silicide layer and their mixtures, enamels, phosphates and sulphates}
- Y10T 29/49982: Coating
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A thermal insulation method more an internal surface of an injection molding casting die includes forming a thermal insulation blanket on the internal surface using laser cladding. One or more layers of a metal material having suitable thermal emittance and melting point characteristics is applied to the internal surface using laser cladding. Because the impact area of the injected molten metal is subject to greater stress and temperature gradients than the remainder of the surface, laser cladding can be used to apply the thermal insulation blanket only to areas that require additional protection.

## Claims

### Claim 1

A thermal insulation method for an internal surface of an injection molding casting die comprising:
forming at least one carbon-carbon mesh layer on the internal surface;
selecting at least one metal material having a thermal emittance that is approximately equal to or less than 0.25 and a melting point that is greater than 1000° C.; and
forming at least one outer layer with the at least one metal material on the internal surface using laser cladding, wherein the at least one carbon carbon mesh layer is located between the at least one outer layer and the internal surface.

### Claim 2 (depends on 1)

The method of claim 1 further comprising:
selecting at least one second metal material having a thermal emittance that is approximately equal to or less than 0.25; and
forming at least one second outer layer with the at least one second metal material on the at least one outer layer using laser cladding.

### Claim 3 (depends on 1)

The method of claim 1 wherein the at least one metal material is one of molybdenum and a molybdenum alloy.

### Claim 4 (depends on 1)

The method of claim 1 wherein the at least one metal material is one of titanium nitride and a titanium nitride alloy.

### Claim 5 (depends on 2)

The method of claim 2 wherein the at least one metal material and the at least one second metal material are one of molybdenum, a molybdenum alloy, titanium nitride, and a titanium nitride alloy.

### Claim 6 (depends on 1)

The method of claim 1 wherein the at least one outer layer is approximately 1 mm thick.

### Claim 7

A thermal insulation method for an internal surface of an injection molding casting die comprising:
selecting at least one metal material having a thermal emittance that is approximately equal to or less than 0.25 and a melting point that is approximately equal to or greater than 1000° C.;
forming a first thermal insulation layer with the at least one metal material on the internal surface using laser cladding, wherein an area of the first thermal insulation layer is substantially equal to an area of the internal surface;
determining an impact point for injection molding on the internal surface;
determining a location of the first thermal insulation layer that corresponds to the impact point; and
forming a second thermal insulation layer with the at least one metal material at the corresponding location using laser cladding, wherein an area of the second thermal Insulation layer is less than the area of the first thermal insulation layer.

### Claim 8 (depends on 6)

The method of claim 6 further comprising forming a carbon-carbon mesh layer on the internal surface.

### Claim 9

A thermal insulation method for an internal surface of an injection molding casting die comprising:
forming at least one offset region in the internal surface of the injection molding casting die;
selecting at least one metal material having a thermal emittance that is approximately equal to or less than 0.25 and a melting point that is approximately equal to or greater than 1000° C.; and
forming a thermal insulation layer with the at least one metal material in the at least one offset region, wherein a thickness of the first thermal insulation layer is substantially equal to a depth of the at least one offset region.

### Claim 10

An injection molding casting die that includes a thermal insulation blanket, the injection molding casting die comprising:
at least one internal surface;
at least one offset region formed in the at least one internal surface; and
a thermal insulation layer formed in the at least one offset region, wherein the thermal insulation layer is formed from at least one metal material having a thermal emittance that is approximately equal to or less than 0.25 and a melting point that is approximately equal to or greater than 1000° C., and wherein a thickness of the thermal insulation layer is substantially equal to a depth of the at least one offset region.

### Claim 11 (depends on 10)

The injection molding casung die of claim 10 wherein the thermal insulation layer is formed from the at least one metal material and a carbon-carbon mesh layer.

### Claim 12 (depends on 10)

The injection molding casting die of claim 10 wherein the at least one metal material is one of molybdenum, a molybdenum alloy, titanium nitride, and a titanium nitride alloy.