Flip-chip semiconductor package and method for fabricating the same
AssigneeSiliconware Precision Industries Co., Ltd.
InventorsKuo-Hua Yu, Chin-Te Chen, Han-Ping Pu, Cheng-Hsu Hsiao
Life of this patent
Estimating the term…
Abstract
A flip-chip semiconductor package and a method for fabricating the same are proposed. A flux is formed on surfaces of solder bumps mounted on an active surface of a semiconductor chip, wherein the acid number of the flux is greater than 20 and the viscosity of the flux is greater than 40. When the chip is electrically connected to a lead frame via the solder bumps by a reflowing process, the flux allows the chip to be effectively fixed to the lead frame and makes the solder bumps not easily wetted to the lead frame during the reflowing process, so as to prevent over-collapsing of the solder bumps.
Claims14
A flip-chip semiconductor package, comprising:
- a lead frame;
- and
- at least one semiconductor chip having an active surface and an opposed inactive surface, with solder bumps being formed on the active surface, wherein the chip is electrically connected to the lead frame via the solder bumps that are subjected to reflowing;
- wherein before the chip is electrically connected to the lead frame via the solder bumps, a flux is formed on surfaces of the solder bumps, with an acid number of the flux being greater than 20 and viscosity of the flux being greater than 40, such that the flux allows the chip to be effectively fixed to the lead frame and makes the solder bumps incapable of being easily wetted to the lead frame when the solder bumps are subjected to reflowing, so as to prevent over-collapsing of the solder bumps.
A method for fabricating a flip-chip semiconductor package, comprising the steps of:
- preparing at least one semiconductor chip having solder bumps formed on an active surface thereof, and forming a flux on surfaces of the solder bumps, wherein an acid number of the flux is greater than 20 and viscosity of the flux is greater than 40;
- and
- electrically connecting the chip to a lead frame via the solder bumps by a reflowing process, wherein the flux allows the chip to be effectively fixed to the lead frame and makes the solder bumps incapable of being easily wetted to the lead frame during the reflowing process, so as to prevent over-collapsing of the solder bumps.