# US 2006/0213077 A1 · Manufacturing method of optical film, and optical film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0213077 A1
- Document ID: US20060213077A1
- Status: Published application
- Kind: A1
- Application number: 11/385,752
- Filed: 2006-03-22
- Published: 2006-09-28
- Earliest claimed: 2005-03-28
- Assignees: Konica Minolta Opto, Inc.
- Inventors: Takeshi Tanaka; Takashi Murakami
- Web page: https://patentgrep.com/patent/US20060213077A1

## CPC

- F26B 13/10: Arrangements for feeding, heating or supporting materials; Controlling movement, tension or position of materials (heating processes F26B3/00)
- F26B 3/28: by radiation, e.g. from the sun
- F26B: DRYING SOLID MATERIALS OR OBJECTS BY REMOVING LIQUID THEREFROM (drying devices for combines A01D41/133; racks for drying fruit or vegetables A01F25/12; drying foodstuffs A23; drying hair A45D20/00; body-drying implements A47K10/00; drying household articles A47L; drying gases or vapours B01D; chemical or physical processes for dewatering or like separating liquids from solids B01D43/00; centrifugal apparatus B04; drying ceramics C04B33/30; drying yarns or fabrics in association with some other form of treatment D06C; drying frames for laundry without heating or positive air circulation, domestic laundry-or spin-driers, wringing or hot pressing laundry D06F; furnaces, kilns, ovens F27)

## Abstract

A washing process to sufficiently remove contaminants attached on the surface of an optical film is proposed. Specifically, disclosed is a method of manufacturing an optical film, wherein the method possesses the steps of spraying onto at least one surface of a transparent film a solidified blast material via cooling that is a gas or a liquid at normal temperature and pressure, washing the at least one surface of the transparent film, and coating at least one optically functional layer on the washed surface of the transparent film.

## Claims

### Claim 1

A method of manufacturing an optical film,
wherein the method comprises the steps of:
(a) spraying onto at least one surface of a transparent film a solidified blast material via cooling that is a gas or a liquid at normal temperature and pressure;
(b) washing the at least one surface of the transparent film; and;
(c) coating at least one optically functional layer on the surface of the transparent film that has been washed via step (b).

### Claim 2 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the blast material is sprayed onto the transparent film from an opposite direction with respect to a predetermined direction, when the transparent film is moving in the predetermined direction.

### Claim 3 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the blast material is sprayed in a plurality of separate batches onto the transparent film.

### Claim 4 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein a surface temperature of the transparent film is set to 20-120° C. to spray the blast material onto the transparent film.

### Claim 5 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the surface temperature of the transparent film is arranged to a temperature of 20-120° C. via a hot-air blast to the transparent film before spraying the blast material.

### Claim 6 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the surface temperature of the transparent film is maintained at a temperature of 20-120° C. by holding the transparent film on a support member.

### Claim 7 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein one surface of the transparent film is held by the support member, and the blast material is sprayed onto the opposite surface of the support member.

### Claim 8 (depends on 7)

The method of manufacturing an optical film of claim 7,
wherein the support member is composed of a roller member to wind the transparent film, or a belt member on which the transparent film is placed.

### Claim 9 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein contaminants removed by spraying after spraying the blast material are aspirated from the periphery of the sprayed portion.

### Claim 10 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the transparent film is discharged by a discharging device.

### Claim 11 (depends on 10)

The method of manufacturing an optical film of claim 10,
wherein a charging amount of the transparent film immediately after spraying the blast material is arranged to not more than 1 kV by discharging the transparent film with the discharging device.

### Claim 12 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the blast material contains carbon dioxide.

### Claim 13 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the blast material is made of dry ice.

### Claim 14 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the blast material is sprayed onto the optical film under reduced pressure.

### Claim 15 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein contaminants on the transparent film are removed employing at least one cleaner of an air type cleaner, an adhesion type cleaner and a brush type cleaner.

### Claim 16 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the transparent film is a film formed by coating a curable resin onto a resin film substrate prepared via film formation by solution-casting or melt-casting, to be cured and the method comprises the steps of:
(a) spraying the blast material onto at least one surface of the resin film substrate; and
(b) washing the at least one surface of the resin film substrate, before coating the curable resin.

### Claim 17 (depends on 1)

The method of manufacturing an optical film of claim 1,
wherein the transparent film is a film formed by coating the curable resin onto the resin film substrate prepared via film formation by solution-casting or melt-casting, to be cured, and subsequently wound by a winding roller, and the method comprises the steps of:
(a) spraying the blast material onto at least one surface of the resin film substrate; and
(b) washing the at least one surface of the resin film substrate, before the winding process after curing the curable resin.

### Claim 18

An optical film,
wherein a solidified blast material via cooling that is a gas or a liquid at normal temperature and pressure is sprayed onto at least one surface of a transparent film, and the at least one surface of the transparent film is washed.