# US 2006/0213038 A1 · Zipper and the packaging therewith

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0213038 A1
- Document ID: US20060213038A1
- Status: Published application
- Kind: A1
- Application number: 11/087,872
- Filed: 2005-03-24
- Published: 2006-09-28
- Earliest claimed: 2005-03-24
- Assignees: C.I. Sanplus Co., Ltd.
- Inventors: Tatsushi Takatori; Yoshio Ohya; Naoki Hatakeyama
- Web page: https://patentgrep.com/patent/US20060213038A1

## CPC

- B65D 33/2508: {using slide fasteners with interlocking members having a substantially uniform section throughout the length of the fastener; Sliders therefor}
- B65D 33/2541: {characterised by the slide fastener, e.g. adapted to interlock with a sheet between the interlocking members having sections of particular shape}
- Y10T 24/2532: having interlocking surface with continuous cross section
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

[PROBLEM] To provide a interlocking device and a packaging bag therewith wherein the interlocking device has sufficient heat stability against retort sterilization treatment and deformational change after said treatment small enough not to be impaired its reopenability. [SOLUTION MEANS] A interlocking device having a pair of male and female profiles wherein: said male and female profiles have non-heat-sealing part to bag body and heat-sealing part to bag body; where said non-heat-sealing part consists of polypropylene type resin composition (A) having main melting peak temperature observed by differential scanning calorimetry less than 150 degree C. and the melt flow rate at 230 degree C. from 0.5 g/10 min to 20 g/10 min; and said heat-sealing part consists of polypropylene type resin composition (B) having main melting peak temperature observed by DSC, not less than 140 degree C. and the melt flow rate at 230 degree C. from 0.1 g/10 min to 20 g/10 min; and the main melting peak temperature of polypropylene type resin composition (B) is at least 10 degree C. lower than that of polypropylene type resin composition (A), and a packaging bag with interlocking device wherein the aforesaid interlocking device is heat-sealed to the bag body via said heat sealing part.

## Claims

### Claim 1

An interlocking device having a pair of male and female profiles wherein:
said male and female profiles have non-heat-sealing part to bag body and heat-sealing part to bag body; where
said non-heat-sealing part consists of polypropylene type resin composition (A) having main melting peak temperature observed by differential scanning calorimetry (DSC), not less than 150 degree C. and the melt flow rate at 230 degree C. from 0.5 g/10 min to 20 g/10 min; and
said heat-sealing part consists of polypropylene type resin composition (B) having main melting peak temperature observed by DSC, not less than 140 degree C. and the melt flow rate at 230 degree C. from 0.1 g/10 min to 20 g/10 min; and
the main melting peak temperature of polypropylene type resin composition (B) is at least 10 degree C. lower than that of polypropylene type resin composition (A).

### Claim at position 2 (depends on 1)

2 A interlocking device of claim 1 wherein:
Its dimensional change against its original dimension before the treatment is not more than 3% where:
Said treatment is to immerse the interlocking device to a glycerin bath whose temperature is controlled at 135 degree C. for 15 min and then to take out, leave for cooling down for 30 min.

### Claim at position 3 (depends on 1, 2)

3 A packaging bag having the interlocking device of claims 1 or 2 which is heat-sealed to said bag body via said heat-sealing-part.