## CPC

- B29D 11/00211: {using heating means}
- B29C 33/44: with means for, or specially constructed to facilitate, the removal of articles, e.g. of undercut articles
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

The invention provides an improved process for manufacturing silicone-hydrogel contact lenses. The improvement includes use of a hot water in the step of dislodging (or removing or de-blocking) from a mold after lens being cured and before lens extraction. Hot water can be used efficiently to dislodge a hydrophobic silicone-hydrogel lens from its adhering mold half and to substantially reduce the stickiness (or tackiness) of the surfaces of the hydrophobic silicone-hydrogel lens.

## Claims

### Claim 1

A method for producing contact lenses, comprising the steps of:
a) providing a mold including a male mold half having a first molding surface and a female mold half having a second molding surface, wherein the male and female mold halves are configured to receive each other such that a mold cavity is formed between the first and second molding surfaces when the mold is closed;
b) dispensing a specific amount of a silicone hydrogel lens-forming material into one of the male and female mold halves;
c) mating the male and female mold halves to close the mold;
d) curing the silicone hydrogel lens-forming material located between the two mold halves, thereby forming a molded silicone hydrogel contact lens;
e) separating the mold into the male and female mold halves, with the silicone hydrogel contact lens adhered on one of the male and female mold halves, wherein the silicone hydrogel contact lens is hydrophobic and characterized by an average water contact angle of greater than about 100 degrees;
f) dispensing a hot water over the lens and/or in the lens-adhering mold half;
g) allowing the hot water to penetrate into interface between the lens and the lens-adhering mold half so as to reduce adhesion between the lens and the lens-adhering mold half; and
h) removing the lens from the lens-adhering mold half for further processing.

### Claim 2 (depends on 1)

The method of claim 1, wherein one of the female and male mold halves is subjected to a surface treatment prior to its use in order for the molded contact lens to adhere preferentially to one particular mold half when opening the mold.

### Claim 3 (depends on 2)

The method of claim 2, wherein the surface treatment is a corona treatment or a plasma treatment.

### Claim 4 (depends on 2)

The method of claim 2, wherein the female mold half is subjected to the surface treatment.

### Claim 5 (depends on 2)

The method of claim 2, wherein the male mold half is subjected to the surface treatment.

### Claim 6 (depends on 1)

The method of claim 1, wherein the hot water has a temperature of higher than about 80° C.

### Claim 7 (depends on 6)

The method of claim 6, wherein the hot water has a temperature of from about 90° C. to about 100° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the molded lens is adhered to the female mold half.

### Claim 9 (depends on 8)

The method of claim 8, wherein the hot water is dispensed in the female mold half in an amount sufficient to submerge the molded lens adhered on the female mold half.

### Claim 10 (depends on 9)

The method of claim 9, wherein in step g) at least about 5 seconds is allowed to let the hot water penetrate into interface between the lens and the lens-adhering mold half.

### Claim 11

A method for producing contact lenses, comprising the steps of:
a) providing a mold including a male mold half having a first molding surface and a female mold half having a second molding surface, wherein the male and female mold halves are configured to receive each other such that a mold cavity is formed between the first and second molding surfaces when the mold is closed;
b) dispensing a specific amount of a silicone hydrogel lens-forming material into one of the male and female mold halves;
c) mating the male and female mold halves to close the mold;
d) curing the silicone hydrogel lens-forming material located between the two mold halves, thereby forming a molded silicone hydrogel contact lens, wherein the silicone hydrogel contact lens is hydrophobic and characterized by an average water contact angle of greater than about 100 degrees;
e) separating the mold into the male and female mold halves, with the silicone hydrogel contact lens adhered on one of the male and female mold halves;
f) placing the lens and its adhering mold half in a well;
g) dispensing a hot water in the well in an amount sufficient to submerge at least the lens and a mold half portion with the lens adhered thereon;
h) allowing the hot water to penetrate into interface between the lens and the lens-adhering mold half so as to dislodge the lens from the lens-adhering mold half; and
i) transferring the lens from the well to a tray or a container for further processing

### Claim 12 (depends on 11)

The method of claim 11, wherein one of the female and male mold halves is subjected to a surface treatment prior to its use in order for the molded contact lens to adhere preferentially to one particular mold half when opening the mold.

### Claim 13 (depends on 12)

The method of claim 12, wherein the surface treatment is a corona treatment or a plasma treatment.

### Claim 14 (depends on 12)

The method of claim 12, wherein the female mold half is subjected to the surface treatment.

### Claim 15 (depends on 12)

The method of claim 12, wherein the male mold half is subjected to the surface treatment.

### Claim 16 (depends on 11)

The method of claim 11, wherein the hot water has a temperature of higher than about 80° C.

### Claim 17 (depends on 16)

The method of claim 16, wherein the hot water has a temperature of from about 90° C. to about 100° C.

### Claim 18 (depends on 11)

The method of claim 11, wherein the molded lens is adhered to the male mold half.

### Claim 19 (depends on 18)

The method of claim 18, wherein the hot water is dispensed in the well in an amount sufficient to submerge the molded lens adhered on the male mold half.

### Claim 20 (depends on 19)

The method of claim 19, wherein in step h) at least about 5 seconds is allowed to let the hot water penetrate into interface between the lens and the lens-adhering mold half.