# US 2006/0188750 A1 · Magnetic sensing element including free layer having gradient composition and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0188750 A1
- Document ID: US20060188750A1
- Status: Published application
- Kind: A1
- Application number: 11/352,958
- Filed: 2006-02-13
- Published: 2006-08-24
- Earliest claimed: 2005-02-23
- Assignees: Alps Electric Co., Ltd.
- Inventors: Yosuke Ide; Masamichi Saito; Masahiko Ishizone; Naoya Hasegawa
- Web page: https://patentgrep.com/patent/US20060188750A1

## CPC

- H10N 50/85: Materials of the active region
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- B82Y 40/00: Manufacture or treatment of nanostructures
- C23C 14/025: {Metallic sublayers}
- C23C 14/165: {by cathodic sputtering}
- C23C 14/584: {Non-reactive treatment}
- G11B 5/3903: {using magnetic thin film layers or their effects, the films being part of integrated structures}
- H01F 10/3268: {the exchange coupling being asymmetric, e.g. by use of additional pinning, by using antiferromagnetic or ferromagnetic coupling interface, i.e. so-called spin-valve [SV] structure, e.g. NiFe/Cu/NiFe/FeMn}
- H01F 41/302: {for applying spin-exchange-coupled multilayers, e.g. nanostructured superlattices (spin-exchange-coupled multilayers H01F10/32)}
- H01F 10/1936: {Half-metallic, e.g. epitaxial CrO2 or NiMnSb films}
- Y10T 428/1121: Multilayer
- Y10T 428/115: Magnetic layer composition
- Y10T 428/1193: with interlaminar component [e.g., adhesion layer, etc.]
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A magnetic sensing element which allows a high reproduction output and reduction in asymmetry of reproduction waveform to become mutually compatible, as well as a method for manufacturing the same, is provided. In the inside of a second pinned magnetic layer and a free magnetic layer, the atomic percentage of an element Z is decreased in a region close to a non-magnetic material layer. Consequently, the ferromagnetic coupling magnetic field due to magnetostatic coupling (topological coupling) between the pinned magnetic layer and the free magnetic layer can be reduced. At the same time, in a region at a distance from the non-magnetic material layer, the atomic percentage of an element Z is increased, a spin-dependent bulk scattering coefficient is increased, and a product of the amount of change in magnetic resistance and the element area of the magnetic sensing element can be maintained at a high level.

## Claims

### Claim 1

A magnetic sensing element including a pinned magnetic layer, in which the magnetization direction is pinned in one direction, and a free magnetic layer disposed on the pinned magnetic layer with a non-magnetic material layer therebetween, the magnetic sensing element characterized in that:
the free magnetic layer includes a layer made of a metal compound represented by a compositional formula of (X0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent) or XdYeZf (where d, e, and f represent atomic percentages, and d+e+f=100 atomic percent); and
a region, in which the atomic percentage of the element Z in the metal compound is decreased with increasing proximity to the non-magnetic material layer side, is present in the free magnetic layer,
wherein the X is at least one element of Cu, Co, Ni, Rh, Pt, Au, Pd, Ir, Ru, Ag, Zn, Cd, and Fe, the Y is at least one element of Mn, Fe, Ti, V, Zr, Nb, Hf, Ta, Cr, Co, and Ni, and the Z is at least one element of Al, Sn, In, Sb, Ga, Si, Ge, Pb, and Zn.

### Claim 2 (depends on 1)

The magnetic sensing element according to claim 1, wherein when a virtual boundary is set in a direction parallel to the interface between the free magnetic layer and the non-magnetic material layer in the film thickness of the free magnetic layer, a first region is assumed to be from the virtual boundary to the interface, and a second region is assumed to be the region from the virtual boundary to a surface opposite to the interface, the atomic percentage of the element Z in the metal compound is decreased continuously or discontinuously from the second region toward the first region in regions sandwiching the virtual boundary.

### Claim 3

A magnetic sensing element including a pinned magnetic layer, in which the magnetization direction is pinned in one direction, and a free magnetic layer disposed on the pinned magnetic layer with a non-magnetic material layer therebetween, the magnetic sensing element characterized in that:
the pinned magnetic layer includes a layer made of a metal compound represented by a compositional formula of (X0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent) or XdYeZf (where d, e, and f represent atomic percentages, and d+e+f=100 atomic percent); and
a region, in which the atomic percentage of the element Z in the metal compound is decreased with increasing proximity to the non-magnetic material layer side, is present in the pinned magnetic layer,
wherein the X is at least one element of Cu, Co, Ni, Rh, Pt, Au, Pd, Ir, Ru, Ag, Zn, Cd, and Fe, the Y is at least one element of Mn, Fe, Ti, V, Zr, Nb, Hf, Ta, Cr, Co, and Ni, and the Z is at least one element of Al, Sn, In, Sb, Ga, Si, Ge, Pb, and Zn.

### Claim 4 (depends on 3)

The magnetic sensing element according to claim 3, wherein when a virtual boundary is set in a direction parallel to the interface between the pinned magnetic layer and the non-magnetic material layer in the film thickness of the pinned magnetic layer, a first region is assumed to be from the virtual boundary to the interface, and a second region is assumed to be the region from the virtual boundary to a surface opposite to the interface, the atomic percentage of the element Z in the metal compound is decreased continuously or discontinuously from the second region toward the first region in regions sandwiching the virtual boundary.

### Claim 5 (depends on 1)

The magnetic sensing element according to claim 1, wherein the atomic percentage of the element Z in the metal compound in the neighborhood of the center of the free magnetic layer or the pinned magnetic layer is more than 24 atomic percent and 26 atomic percent or less.

### Claim 6 (depends on 1)

The magnetic sensing element according to claim 1, wherein the atomic percentage of the element Z in the metal compound in the neighborhood of the interface of the free magnetic layer or the pinned magnetic layer to the non-magnetic material layer is 19 atomic percent or more and 24 atomic percent or less.

### Claim 7 (depends on 6)

The magnetic sensing element according to claim 6, wherein the atomic percentage of the element Z in the metal compound in the neighborhood of the interface of the free magnetic layer or the pinned magnetic layer to the non-magnetic material layer is 22 atomic percent or less.

### Claim 8 (depends on 1)

The magnetic sensing element according to claim 1, wherein the difference between the atomic percentage of the element Z in the metal compound in the neighborhood of the center of the free magnetic layer or the pinned magnetic layer and the atomic percentage of the element Z in the metal compound in the neighborhood of the interface of the free magnetic layer or the pinned magnetic layer to the non-magnetic material layer is 3 atomic percent or more.

### Claim 9 (depends on 1)

The magnetic sensing element according to claim 1, in which the metal compound is formed from a metal compound represented by a compositional formula of (Co0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent),
wherein the Y is at least one element of Mn, Fe, and Cr, and the Z is at least one element of Al, Ga, Si, and Ge.

### Claim 10 (depends on 9)

The magnetic sensing element according to claim 9, in which the metal compound is formed from a metal compound represented by a compositional formula of (Co0.67Mn0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent),
wherein the Z is Si or Ge.

### Claim 11 (depends on 10)

The magnetic sensing element according to claim 10, in which the metal compound is formed from a metal compound represented by a compositional formula of (Co0.67Mn0.33)aGeb (where a and b represent atomic percentages, and a+b=100 atomic percent).

### Claim 12 (depends on 1)

The magnetic sensing element according to claim 1, wherein the film thickness of the non-magnetic material layer is 18 angstroms or more and 50 angstroms or less.

### Claim 13 (depends on 1)

The magnetic sensing element according to claim 1, comprising an antiferromagnetic layer, the pinned magnetic layer which is disposed in contact with the antiferromagnetic layer and in which the magnetization direction is pinned by an exchange anisotropic magnetic field with the antiferromagnetic layer, and the free magnetic layer disposed on the pinned magnetic layer with the non-magnetic material layer therebetween.

### Claim 14 (depends on 1)

The magnetic sensing element according to claim 1, comprising non-magnetic material layers laminated on and under the free magnetic layer, and pinned magnetic layers located on one of the non-magnetic material layers and under the other non-magnetic material layer.

### Claim 15 (depends on 14)

The magnetic sensing element according to claim 14, comprising antiferromagnetic layers which are located on one of the pinned magnetic layers and under the other pinned magnetic layer and which pin the magnetization directions of the respective pinned magnetic layers in constant directions by exchange anisotropic magnetic fields.

### Claim 16 (depends on 1)

The magnetic sensing element according to claim 1, wherein a sensing current is passed in a direction perpendicular to film surfaces of the pinned magnetic layer, the non-magnetic material layer, and the free magnetic layer.

### Claim 17

A method for manufacturing a magnetic sensing element including a pinned magnetic layer, in which the magnetization direction is pinned in one direction, and a free magnetic layer disposed on the pinned magnetic layer with a non-magnetic material layer therebetween, the method characterized by comprising the steps of:
forming the free magnetic layer as a laminate of a first free magnetic layer in contact with the non-magnetic material layer and a second free magnetic layer stacked on the first free magnetic layer;
forming the first free magnetic layer and the second free magnetic layer from metal compounds represented by (X0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent) or XdYeZf (where d, e, and f represent atomic percentages, and d+e+f=100 atomic percent); and
specifying the atomic percentage of the element Z in the metal compound constituting the first free magnetic layer to be smaller than the atomic percentage of the element Z in the metal compound constituting the second free magnetic layer, wherein the X is at least one element of Cu, Co, Ni, Rh, Pt, Au, Pd, Ir, Ru, Ag, Zn, Cd, and Fe, the Y is at least one element of Mn, Fe, Ti, V, Zr, Nb, Hf, Ta, Cr, Co, and Ni, and the Z is at least one element of Al, Sn, In, Sb, Ga, Si, Ge, Pb, and Zn.

### Claim 18 (depends on 17)

The method for manufacturing a magnetic sensing element according to claim 17, wherein the atomic percentage of the element Z in the metal compound of the second free magnetic layer is specified to be more than 24 atomic percent and 26 atomic percent or less.

### Claim 19 (depends on 17)

The method for manufacturing a magnetic sensing element according to claim 17, wherein the atomic percentage of the element Z in the metal compound of the first free magnetic layer is specified to be 19 atomic percent or more and 24 atomic percent or less.

### Claim 20 (depends on 19)

The method for manufacturing a magnetic sensing element according to claim 19, wherein the atomic percentage of the element Z in the metal compound of the first free magnetic layer is specified to be 22 atomic percent or less.

### Claim 21 (depends on 17)

The method for manufacturing a magnetic sensing element according to claim 17, wherein the difference between the atomic percentage of the element Z in the metal compound of the second free magnetic layer and the atomic percentage of the element Z in the metal compound of the first free magnetic layer is specified to be 3 atomic percent or more.

### Claim 22

A method for manufacturing a magnetic sensing element including a pinned magnetic layer, in which the magnetization direction is pinned in one direction, and a free magnetic layer disposed on the pinned magnetic layer with a non-magnetic material layer therebetween, the method characterized by comprising the steps of:
forming the pinned magnetic layer as a laminate of a first pinned magnetic layer in contact with the non-magnetic material layer and a second pinned magnetic layer stacked on the first pinned magnetic layer;
forming the first pinned magnetic layer and the second pinned magnetic layer from metal compounds represented by (X0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent) or XdYeZf (where d, e, and f represent atomic percentages, and d+e+f=100 atomic percent); and
specifying the atomic percentage of the element Z in the metal compound constituting the first pinned magnetic layer to be smaller than the atomic percentage of the element Z in the metal compound constituting the second pinned magnetic layer,
wherein the X is at least one element of Cu, Co, Ni, Rh, Pt, Au, Pd, Ir, Ru, Ag, Zn, Cd, and Fe, the Y is at least one element of Mn, Fe, Ti, V, Zr, Nb, Hf, Ta, Cr, Co, and Ni, and the Z is at least one element of Al, Sn, In, Sb, Ga, Si, Ge, Pb, and Zn.

### Claim 23 (depends on 22)

The method for manufacturing a magnetic sensing element according to claim 22, wherein the atomic percentage of the element Z in the metal compound of the second pinned magnetic layer is specified to be more than 24 atomic percent and 26 atomic percent or less.

### Claim 24 (depends on 22)

The method for manufacturing a magnetic sensing element according to claim 22, wherein the atomic percentage of the element Z in the metal compound of the first pinned magnetic layer is specified to be 19 atomic percent or more and 24 atomic percent or less.

### Claim 25 (depends on 24)

The method for manufacturing a magnetic sensing element according to claim 24, wherein the atomic percentage of the element Z in the metal compound of the first pinned magnetic layer is specified to be 22 atomic percent or less.

### Claim 26 (depends on 22)

The method for manufacturing a magnetic sensing element according to claim 22, wherein the difference between the atomic percentage of the element Z in the metal compound of the second pinned magnetic layer and the atomic percentage of the element Z in the metal compound of the first pinned magnetic layer is specified to be 3 atomic percent or more.

### Claim 27

A method for manufacturing a magnetic sensing element including a pinned magnetic layer, in which the magnetization direction is pinned in one direction, and a free magnetic layer disposed on the pinned magnetic layer with a non-magnetic material layer therebetween, the method characterized by comprising the steps of:
forming the free magnetic layer by a sputtering process in which the target is a metal compound represented by (X0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent) or XdYeZf (where d, e, and f represent atomic percentages, and d+e+f=100 atomic percent); and
conducting film formation of the free magnetic layer at this time in such a way that the atomic percentage of the element Z in the metal compound is decreased with increasing proximity to the non-magnetic material layer side,
wherein the X is at least one element of Cu, Co, Ni, Rh, Pt, Au, Pd, Ir, Ru, Ag, Zn, Cd, and Fe, the Y is at least one element of Mn, Fe, Ti, V, Zr, Nb, Hf, Ta, Cr, Co, and Ni, and the Z is at least one element of Al, Sn, In, Sb, Ga, Si, Ge, Pb, and Zn.

### Claim 28

A method for manufacturing a magnetic sensing element including a pinned magnetic layer, in which the magnetization direction is pinned in one direction, and a free magnetic layer disposed on the pinned magnetic layer with a non-magnetic material layer therebetween, the method characterized by comprising the steps of:
forming the pinned magnetic layer by a sputtering process in which the target is a metal compound represented by (X0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent) or XdYeZf (where d, e, and f represent atomic percentages, and d+e+f=100 atomic percent); and
conducting film formation of the pinned magnetic layer at this time in such a way that the atomic percentage of the element Z in the metal compound is decreased with increasing proximity to the non-magnetic material layer side,
wherein the X is at least one element of Cu, Co, Ni, Rh, Pt, Au, Pd, Ir, Ru, Ag, Zn, Cd, and Fe, the Y is at least one element of Mn, Fe, Ti, V, Zr, Nb, Hf, Ta, Cr, Co, and Ni, and the Z is at least one element of Al, Sn, In, Sb, Ga, Si, Ge, Pb, and Zn.

### Claim 29 (depends on 27)

The method for manufacturing a magnetic sensing element according to claim 27, wherein the atomic percentage of the element Z in the metal compound in the neighborhood of the center of the free magnetic layer or the pinned magnetic layer is specified to be more than 24 atomic percent and 26 atomic percent or less.

### Claim 30 (depends on 27)

The method for manufacturing a magnetic sensing element according to claim 27, wherein the atomic percentage of the element Z in the metal compound in the neighborhood of the interface of the free magnetic layer or the pinned magnetic layer to the non-magnetic material layer is specified to be 19 atomic percent or more and 24 atomic percent or less.

### Claim 31 (depends on 30)

The method for manufacturing a magnetic sensing element according to claim 30, wherein the atomic percentage of the element Z in the metal compound in the neighborhood of the interface of the free magnetic layer or the pinned magnetic layer to the non-magnetic material layer is specified to be 22 atomic percent or less.

### Claim 32 (depends on 27)

The method for manufacturing a magnetic sensing element according to claim 27, wherein the difference between the atomic percentage of the element Z in the metal compound in the neighborhood of the center of the free magnetic layer or the pinned magnetic layer and the atomic percentage of the element Z in the metal compound in the neighborhood of the interface of the free magnetic layer or the pinned magnetic layer to the non-magnetic material layer is specified to be 3 atomic percent or more.

### Claim 33 (depends on 17)

The method for manufacturing a magnetic sensing element according to claim 17, wherein the metal compound is formed from a metal compound represented by a compositional formula of (Co0.67Y0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent),
wherein the Y is at least one element of Mn, Fe, and Cr, and the Z is at least one element of Al, Ga, Si, and Ge.

### Claim 34 (depends on 33)

The method for manufacturing a magnetic sensing element according to claim 33, wherein the metal compound is formed from a metal compound represented by a compositional formula of (Co0.67Mn0.33)aZb (where a and b represent atomic percentages, and a+b=100 atomic percent),
wherein the Z is Si or Ge.

### Claim 35 (depends on 34)

The method for manufacturing a magnetic sensing element according to claim 34, wherein the metal compound is formed from a metal compound represented by a compositional formula of (Co0.67Mn0.33)aGeb (where a and b represent atomic percentages, and a+b=100 atomic percent).

### Claim 36 (depends on 17)

The method for manufacturing a magnetic sensing element according to claim 17, wherein the film thickness of the non-magnetic material layer is 18 angstroms or more and 50 angstroms or less.