# US 2006/0188667 A1 · Optical cellulose acylate film and a method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0188667 A1
- Document ID: US20060188667A1
- Status: Published application
- Kind: A1
- Application number: 11/344,196
- Filed: 2006-02-01
- Published: 2006-08-24
- Earliest claimed: 2005-02-01
- Assignees: Fuji Photo Film Co., Ltd.
- Inventors: Saisuke Watanabe; Zemin Shi
- Web page: https://patentgrep.com/patent/US20060188667A1

## CPC

- G02B 5/3083: {Birefringent or phase retarding elements (G02B5/3008, G02B5/3016 take precedence; systems for polarisation control G02B27/286; manufacturing phase modulating patterns by lithographic processes G03F7/001)}
- C08J 5/18: Manufacture of films or sheets
- G02F 1/133528: {Polarisers}
- C08J 2301/10: Esters of organic acids
- C09K 2323/035: Ester polymer, e.g. polycarbonate, polyacrylate or polyester
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

An optical cellulose acylate film satisfying (1)-(3) below, and showing a reduction of only 30% or less in both of its number-average and weight-average molecular weights when heated for 20 minutes at a temperature 10° C. higher than its melting point in an inert gas atmosphere: (1): 2.4≦A+B<3.0 (2): 0≦A≦1.5 (3): 0.9<B<3 wherein A represents the substitution degree of acetyl groups in cellulose acylate, and B represents the total substitution degree of acyl groups having 3 to 7 carbon atoms in cellulose acylate.

## Claims

### Claim 1

An optical cellulose acylate film satisfying the requirements of (1) to (3) below, and showing a reduction of only 30% or less in both of its number-average and weight-average molecular weights when heated for 20 minutes at a temperature 10° C. higher than its melting point in an inert gas atmosphere:
(1): 2.4≦A+B<3.0
(2): 0≦A≦1.5
(3): 0.9<B<3
wherein A represents the substitution degree of acetyl groups in cellulose acylate, and B represents the total substitution degree of acyl groups having 3 to 7 carbon atoms in cellulose acylate.

### Claim 2 (depends on 1)

The optical cellulose acylate film according to claim 1, satisfying the requirements of (4) to (6) below:
(4): Re≦Rth
(5): 0 nm≦Re≦300 nm
(6): 0 nm≦Rth≦500 nm
wherein Re represents an in-plane retardation of the film and Rth represents retardation of a thickness direction of the film.

### Claim 3 (depends on 1)

The optical cellulose acylate film according to claim 1, satisfying the requirements of (7) to (9) below:
(7): Re≦Rth
(8); 50 nm≦Re≦100 nm
(9): 150 nm≦Rth≦250 nm
wherein Re represents an in-plane retardation of the film and Rth represents retardation of a thickness direction of the film.

### Claim 4 (depends on 1)

The optical cellulose acylate film according to claim 1, having an breaking elongation of 150 to 300% when stretched at a temperature 10° C. higher than its glass transition point.

### Claim 5 (depends on 1)

The optical cellulose acylate film according to claim 1, wherein the amount of residual solvent in the film is 0.01% by mass or less.

### Claim 6 (depends on 1)

The optical cellulose acylate film according to claim 1, wherein the cellulose acylate is cellulose acetate propionate.

### Claim 7 (depends on 1)

The optical cellulose acylate film according to claim 1, wherein the cellulose acylate is cellulose acetate butyrate.

### Claim 8 (depends on 1)

The optical cellulose acylate film according to claim 1, having a thickness of 30 to 400 μm.

### Claim 9 (depends on 1)

A method of manufacturing an optical cellulose acylate film according to claim 1, comprising forming a film by a melt casting process from a composition comprising cellulose acylate satisfying the requirements of (1) to (3) below:
(1): 2.4≦A+B<3.0
(2): 0≦A≦1.5
(3): 0.9<B<3
wherein A represents the substitution degree of acetyl groups in cellulose acylate, and B represents the total substitution degree of acyl groups having 3 to 7 carbon atoms in cellulose acylate.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the melt casting process is carried out in an inert gas atmosphere.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the cellulose acylate has a melting point of 170 to 230° C.

### Claim 12 (depends on 1)

A polarizing plate comprising at least one cellulose acylate film according to claim 1.

### Claim 13 (depends on 1)

A retardation film comprising at least one cellulose acylate film according to claim 1.

### Claim 14 (depends on 1)

An optical compensation film comprising at least one cellulose acylate film according to claim 1.

### Claim 15 (depends on 1)

A reflection-preventing film comprising at least one cellulose acylate film according to claim 1.

### Claim 16 (depends on 1)

An image display device comprising a cellulose acylate film according to claim 1.

### Claim 17 (depends on 16)

The image display device according to claim 16, comprising a polarizing plate having the cellulose acylate film.

### Claim 18 (depends on 16)

The image display device according to claim 16, comprising a retardation film having the cellulose acylate film.

### Claim 19 (depends on 16)

The image display device according to claim 16, comprising an optical compensation film having the cellulose acylate film.

### Claim 20 (depends on 16)

The image display device according to claim 16, comprising a reflection-preventing film having the cellulose acylate film.