# US 2006/0186806 A1 · Light-emitting apparatus and method for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0186806 A1
- Document ID: US20060186806A1
- Status: Published application
- Kind: A1
- Application number: 11/395,117
- Filed: 2006-03-31
- Published: 2006-08-24
- Earliest claimed: 2003-05-16
- Inventors: Tetsuya Utsumi; Masaaki Arima; Masayuki Harada; Mari Funada
- Web page: https://patentgrep.com/patent/US20060186806A1

## CPC

- H10K 59/875: {Arrangements for extracting light from the devices}
- Y10T 428/24347: From both sides
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

In a light-emitting apparatus, a face of a substrate on which a light-emitting device is formed is an uneven surface having a plurality of asperities. The mean spacing Sm of adjacent asperities or the mean spacing S of peaks of adjacent projections of the asperities is no less than three times the longest wavelength of light generated by a light-emitting layer and no more than two hundred times the longest wavelength. The arithmetic mean slope Δa of the uneven surface is in a range between 4° and 30°, inclusive. Therefore, the apparatus emits substantially a greater amount of light from a light extraction side and has less brightness unevenness than a light-emitting apparatus with no uneven surface.

## Claims

### Claim 1

A light-emitting apparatus comprising a substrate, a middle layer provided on the substrate, and a light-emitting device provided on the middle layer,
wherein the device includes a light-emitting layer located between a pair of electrodes, a face of the middle layer on which the light-emitting device is formed is an uneven surface having a plurality of asperities, the mean spacing Sm of adjacent asperities or the mean spacing S of peaks of adjacent projections of the asperities is no less than three times the longest wavelength of light generated by the light-emitting layer and no more than two hundred times the longest wavelength, wherein at least one of the following requirements (i)-(vi) is satisfied:
(i) the arithmetic mean slope Δa of the uneven surface is in a range between 4° and 30°, inclusive;
(ii) the root mean square slope Δq of the uneven surface is in a range between 4° and 35;
(iii) the ratio Ra/Sm of the arithmetic mean roughness Ra of the uneven surface to the mean spacing Sm of asperities is in a range between 0.008 and 0.09, inclusive;
(iv) the ratio Ra/S of the arithmetic mean roughness Ra to the mean spacing S of peaks is in a range between 0.009 and 0.10, inclusive;
(v) the ratio Rz/Sm of the ten-point height of irregularities Rz of the uneven surface to the mean spacing Sm of asperities is in a range between 0.05 and 0.22, inclusive; and
(vi) the ratio Rz/S of the ten-point height of irregularities Rz to the mean spacing S of peaks is in a range between 0.05 and 0.25, inclusive.

### Claim 2 (depends on 1)

The apparatus according to claim 1, wherein at least the requirement (i) is satisfied.

### Claim 3 (depends on 1)

The apparatus according to claim 1, wherein at least the requirement (ii) is satisfied.

### Claim 4 (depends on 1)

The apparatus according to claim 1, wherein at least the requirement (iii) is satisfied.

### Claim 5 (depends on 1)

The apparatus according to claim 1, wherein at least the requirement (iv) is satisfied.

### Claim 6 (depends on 1)

The apparatus according to claim 1, wherein at least the requirement (v) is satisfied.

### Claim 7 (depends on 1)

The apparatus according to claim 1, wherein at least the requirement (vi) is satisfied.

### Claim 8 (depends on 1)

The apparatus according to claim 1, wherein the light-emitting device is curved along the uneven surface.

### Claim 9 (depends on 8)

The apparatus according to claim 8, wherein the light-emitting layer has a first face at a side facing the substrate and a second face that is opposite from the first face, wherein the first and second faces are curved along the uneven surface, and the projections of the first face correspond to the depressions of the second face, and the depressions of the first face correspond to the projections of the second face.

### Claim 10 (depends on 8)

The apparatus according to claim 8, wherein the electrodes and the light-emitting layer are each formed to have a constant thickness.

### Claim 11 (depends on 1)

The apparatus according to claim 1, wherein a prism sheet is provided on a side where light generated by the light-emitting layer is extracted.

### Claim 12 (depends on 1)

The apparatus according to claim 1, wherein the light-emitting device is an organic electroluminescent device.

### Claim 13

A light-emitting apparatus comprising a substrate and a light-emitting device provided on the substrate,
wherein the device includes a light-emitting layer located between a pair of electrodes, one of the electrodes that is closer to the substrate has a face that faces the light-emitting layer and is an uneven surface having a plurality of asperities, the mean spacing Sm of adjacent asperities or the mean spacing S of peaks of adjacent projections of the asperities is no less than three times the longest wavelength of light generated by the light-emitting layer and no more than two hundred times the longest wavelength, wherein at least one of the following requirements (i)-(vi) is satisfied:
(i) the arithmetic mean slope Δa of the uneven surface is in a range between 4° and 30°, inclusive;
(ii) the root mean square slope Δq of the uneven surface is in a range between 4° and 35°;
(iii) the ratio Ra/Sm of the arithmetic mean roughness Ra of the uneven surface to the mean spacing Sm of asperities is in a range between 0.008 and 0.09, inclusive;
(iv) the ratio Ra/S of the arithmetic mean roughness Ra to the mean spacing S of peaks is in a range between 0.009 and 0.10, inclusive;
(v) the ratio Rz/Sm of the ten-point height of irregularities Rz of the uneven surface to the mean spacing Sm of asperities is in a range between 0.05 and 0.22, inclusive; and
(vi) the ratio Rz/S of the ten-point height of irregularities Rz to the mean spacing S of peaks is in a range between 0.05 and 0.25, inclusive.

### Claim 14 (depends on 13)

The apparatus according to claim 13, wherein at least the requirement (i) is satisfied.

### Claim 15 (depends on 13)

The apparatus according to claim 13, wherein at least the requirement (ii) is satisfied.

### Claim 16 (depends on 13)

The apparatus according to claim 13, wherein at least the requirement (iii) is satisfied.

### Claim 17 (depends on 13)

The apparatus according to claim 13, wherein at least the requirement (iv) is satisfied.

### Claim 18 (depends on 13)

The apparatus according to claim 13, wherein at least the requirement (v) is satisfied.

### Claim 19 (depends on 13)

The apparatus according to claim 13, wherein at least the requirement (vi) is satisfied.

### Claim 20 (depends on 13)

The apparatus according to claim 13, wherein the light-emitting layer is curved along the uneven surface.

### Claim 21 (depends on 20)

The apparatus according to claim 20, wherein the light-emitting layer has a first face at a side facing the substrate and a second face that is opposite from the first face, wherein the first and second faces are curved along the uneven surface, and the projections of the first face correspond to the depressions of the second face, and the depressions of the first face correspond to the projections of the second face.

### Claim 22 (depends on 20)

The apparatus according to claim 20, wherein one of the electrodes, which is opposite to the substrate, and the light-emitting layer are each formed to have a constant thickness.

### Claim 23 (depends on 13)

The apparatus according to claim 13, wherein a prism sheet is provided on a side where light generated by the light-emitting layer is extracted.

### Claim 24 (depends on 13)

The apparatus according to claim 13, wherein the light-emitting device is an organic electroluminescent device.

### Claim 25

A light-emitting apparatus comprising a substrate and a light-emitting device provided on the substrate,
wherein the device includes a light-emitting layer located between a pair of electrodes, the light-emitting layer has a first face at a side facing the substrate and a second face that is opposite from the first face, wherein the first and second faces are each uneven surface having a plurality of asperities, the projections of the first face correspond to the depressions of the second face, and the depressions of the first face correspond to the projections of the second face, and wherein, on each face, the mean spacing Sm of adjacent asperities or the mean spacing S of peaks of adjacent projections of the asperities is no less than three times the longest wavelength of light generated by the light-emitting layer and no more than two hundred times the longest wavelength, wherein at least one of the following requirements (i)-(vi) is satisfied:
(i) the arithmetic mean slope Δa of the uneven surface is in a range between 4° and 30°, inclusive;
(ii) the root mean square slope Δq of the uneven surface is in a range between 4° and 35°;
(iii) the ratio Ra/Sm of the arithmetic mean roughness Ra of the uneven surface to the mean spacing Sm of asperities is in a range between 0.008 and 0.09, inclusive;
(iv) the ratio Ra/S of the arithmetic mean roughness Ra to the mean spacing S of peaks is in a range between 0.009 and 0.10, inclusive;
(v) the ratio Rz/Sm of the ten-point height of irregularities Rz of the uneven surface to the mean spacing Sm of asperities is in a range between 0.05 and 0.22, inclusive; and
(vi) the ratio Rz/S of the ten-point height of irregularities Rz to the mean spacing S of peaks is in a range between 0.05 and 0.25, inclusive.

### Claim 26

A method for manufacturing a light-emitting apparatus having a light-emitting layer, comprising:
preparing a substrate;
forming a middle layer on the substrate;
forming an uneven surface having a plurality of asperities on a face of the middle layer, wherein the mean spacing Sm of adjacent asperities or the mean spacing S of peaks of adjacent projections of the asperities is no less than three times the longest wavelength of light generated by the light-emitting layer and no more than two hundred times the longest wavelength, wherein the uneven surface is formed such that at least one of the following requirements (i)-(vi) is satisfied:
(i) the arithmetic mean slope Δa of the uneven surface is in a range between 4° and 30° inclusive;
(ii) the root mean square slope Δq of the uneven surface is in a range between 4° and 35°;
(iii) the ratio Ra/Sm of the arithmetic mean roughness Ra of the uneven surface to the mean spacing Sm of asperities is in a range between 0.008 and 0.09, inclusive;
(iv) the ratio Ra/S of the arithmetic mean roughness Ra to the mean spacing S of peaks is in a range between 0.009 and 0.10, inclusive;
(v) the ratio Rz/Sm of the ten-point height of irregularities Rz of the uneven surface to the mean spacing Sm of asperities is in a range between 0.05 and 0.22, inclusive; and
(vi) the ratio Rz/S of the ten-point height of irregularities Rz to the mean spacing S of peaks is in a range between 0.05 and 0.25, inclusive, and
forming on the uneven surface a light-emitting device having the light-emitting layer and a pair of electrodes between which the light-emitting layer is located such that the light-emitting device is curved along the uneven surface.

### Claim 27

A method for manufacturing a light-emitting apparatus having a light-emitting layer, comprising:
preparing a substrate;
forming a first electrode on the substrate;
forming an uneven surface having a plurality of asperities on a face of the first electrode, wherein the mean spacing Sm of adjacent asperities or the mean spacing S of peaks of adjacent projections of the asperities is no less than three times the longest wavelength of light generated by the light-emitting layer and no more than two hundred times the longest wavelength, wherein the uneven surface is formed such that at least one of the following requirements (i)-(vi) is satisfied:
(i) the arithmetic mean slope Δa of the uneven surface is in a range between 4° and 30°, inclusive;
(ii) the root mean square slope Δq of the uneven surface is in a range between 4° and 35°;
(iii) the ratio Ra/Sm of the arithmetic mean roughness Ra of the uneven surface to the mean spacing Sm of asperities is in a range between 0.008 and 0.09, inclusive;
(iv) the ratio Ra/S of the arithmetic mean roughness Ra to the mean spacing S of peaks is in a range between 0.009 and 0.10, inclusive;
(v) the ratio Rz/Sm of the ten-point height of irregularities Rz of the uneven surface to the mean spacing Sm of asperities is in a range between 0.05 and 0.22, inclusive; and
(vi) the ratio Rz/S of the ten-point height of irregularities Rz to the mean spacing S of peaks is in a range between 0.05 and 0.25, inclusive,
forming on the uneven surface the light-emitting layer such that the light-emitting layer is curved along the uneven surface; and
forming a second electrode on the light-emitting layer so that the light-emitting layer is located between the first electrode and the second electrode, thereby forming a light emitting device.