# US 2006/0186384 A1 · Composite materials having low filler percolation thresholds and methods of controlling filler interconnectivity

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0186384 A1
- Document ID: US20060186384A1
- Status: Published application
- Kind: A1
- Application number: 11/357,582
- Filed: 2006-02-16
- Published: 2006-08-24
- Earliest claimed: 2005-02-16
- Assignees: Georgia Tech Research Corporation
- Inventors: Rosario Gerhardt; Runqing Qu; Zhi Li; Robert Samuels; Charles Capozzi
- Web page: https://patentgrep.com/patent/US20060186384A1

## CPC

- H01B 1/24: the conductive material comprising carbon-silicon compounds, carbon or silicon
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

Composite materials are disclosed having low filler percolation thresholds for filler materials into the composite matrix material along with methods of controlling filler interconnectivity within the composite matrix material. Methods are, thus, disclosed that provide the ability to control the desired properties of the composites. The composites of the present disclosure are characterized by a “pseudo-crystalline” microstructure formed of matrix particles and filler particles where the matrix particles are faceted and substantially retain their individual particle boundaries and where the filler particles are interspersed between the matrix particles at the individual matrix particle boundaries such that the filler particles form a substantially interconnected network that substantially surrounds the individual faceted matrix particles. In an exemplary embodiment, the composites are formed by selecting matrix particles and filler particles wherein the ratio of the average size of the matrix particles to the average size of the filler particles is about 10 or more. The selected matrix particles exhibit a glass transition temperature. The matrix particles and the filler particles are mechanically mixed and then subjected to a temperature above the glass transition temperature of the matrix particles and a compression pressure for a period of time sufficient to cause the matrix particles to undergo deformation so as to compress them together eliminating void spaces between the particles without melting the matrix material. The method is also demonstrated to work in combination with more standard art methods such as solution mixing for the purposes of achieving additional control of the properties.

## Claims

### Claim 1

A method of making a composite material including a matrix material and a filler material comprising the steps of:
(a) providing particles of a matrix material, the matrix material having a glass transition temperature;
(b) providing particles of a filler material, the matrix material having an average particle size and the filler material having an average particle size, the average particle size of the matrix material being at least about 10 times larger than the average particle size of the filler material;
(c) mechanically mixing the matrix material and filler material;
(d) heating the mixture to a temperature above the glass transition temperature of the matrix material; and
(e) compression molding the mixture of matrix material and filler material at a temperature and at a pressure and for an amount of time sufficient to cause the matrix material to form a pseudo-crystalline structure and to achieve a desired amount of interconnectivity of the filler material, wherein the amount of interconnectivity of the filler material can be controlled by varying one or more of the time, temperature and pressure of the molding.

### Claim 2 (depends on 1)

The method of claim 1, wherein the filler material has a desired property, wherein the property is selected from: electrical conductivity, luminescence, electrical insulation, magnetic induction, transparency, optical transmission, and optical absorption, and wherein the composite material acquires the property of the filler material as a function of the amount of interconnectivity of the filler material.

### Claim 3 (depends on 1)

The method of claim 1, wherein the amount of interconnectivity of the filler particles is controlled by varying one or more processing conditions selected from: the amount of filler material in the polymer-filler mixture; an average particle size of the filler particles; an average particle size of the polymer particles; the ratio of the average particle size of the matrix material to the average particle size of the filler material; a method of mixing of the polymer particles with the filler particles; the temperature at which the polymer-filler mixture is molded; the pressure at which the polymer-filler mixture is molded; and the time for which the polymer-filler mixture is molded.

### Claim 4 (depends on 1)

The method of claim 1, wherein the time is between about 2 minutes and 25 minutes.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pressure is between about 2 kN and 24 kN.

### Claim 6 (depends on 1)

The method of claim 1, wherein the temperature is further below the melting point temperature of the matrix material.

### Claim 7 (depends on 6)

The method of claim 6, wherein the temperature is between about 140° C. and 190° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the matrix-filler mixture is molded at a first temperature and pressure for a first amount of time and then molded at a second temperature and pressure for a second amount of time, wherein at least one of the first temperature, pressure and time are different from at least one of the second temperature, pressure and time.

### Claim 9 (depends on 8)

The method of claim 8, wherein the second temperature and pressure are higher than the first temperature and pressure.

### Claim 10 (depends on 1)

The method of claim 1, wherein the mechanical dry mixing is selected from: shaking, stirring, mixing in a blender, and mixing with a mortar and pestle.

### Claim 11 (depends on 1)

The method of claim 1, wherein the step of mixing the matrix particles with the filler particles comprises a combination of mechanical dry mixing and solution mixing.

### Claim 12 (depends on 11)

The method of claim 11, wherein the solution mixing comprises the steps of:
(a) dissolving a portion of the matrix material in a solvent to produce a matrix solution;
(b) dispersing a portion of the particles of filler material in the matrix solution to provide a matrix-filler solution; and
(c) drying the matrix-filler solution to form a matrix-filler composite film or powder.

### Claim 13 (depends on 11)

The method of claim 11, wherein the combination of mechanical dry mixing and solution mixing comprises the steps of:
(a) preparing a matrix-filler mixture by mechanical dry mixing a portion of the matrix particles with a portion of the filler particles;
(b) preparing a matrix-filler composite film by solution mixing a portion of the matrix particles with a portion of the filler particles;
(c) breaking the matrix-filler composite film into a plurality of matrix-filler composite film pieces;
(d) mixing the matrix-filler composite film pieces with the mechanically mixed matrix-filler mixture to form a combined matrix-filler mixture;
(e) molding the combined matrix-filler mixture at a temperature and at pressure and for an amount of time sufficient to produce a composite material having a desired amount of interconnectivity of the filler particles that will result in the composite material having the desired property.

### Claim 14 (depends on 13)

The method of claim 13, wherein the solvent is selected from: ethyl acetate and butane-2-one.

### Claim 15 (depends on 1)

The method or claim 1, wherein the matrix material is a thermo-polymer.

### Claim 16 (depends on 1)

The method of claim 1, wherein the matrix material is a thermoplastic polymer selected from: poly(methyl methacrylate) (PMMA), poly(acrylonitrile-co-butadiene-co-styrene) (ABS), polystyrene (PS), or polyethylene oxide (PEO).

### Claim 17 (depends on 1)

The method of claim 1, wherein the desired property is electrical conductivity, and the filler material is selected from: carbon black (CB), indium tin oxide (ITO), Ag, Cu, and LiClO4.

### Claim 18 (depends on 1)

The method of claim 1, wherein the desired property is luminescence and the filler material is selected from red, green, and blue phosphors.

### Claim 19 (depends on 1)

The method of claim 1, wherein the desired property is magnetic inductance, and the filler material is selected from Dy2O3, and Gd2O3.

### Claim 20 (depends on 1)

The method of claim 1, wherein the desired property is electrical insulation, and the filler material is a dielectric material selected from CeO2, BaTiO3,, and Al2O3.

### Claim 21 (depends on 1)

A composite material formed according to the method of claim 1.

### Claim 22

A composite material comprising:
a matrix formed from a plurality of individual particles;
a substantially interconnected network of filler particles within the matrix, wherein the composite material has a pseudo-crystalline microstructure wherein the filler particles form a substantially interconnected network substantially surrounding the individual polymer particles.

### Claim 23 (depends on 22)

The composite material of claim 22, wherein the composite has a percolation threshold below about one percent volume of filler material.

### Claim 24 (depends on 22)

The composition of claim 22, wherein the filler particles comprise a desired property and wherein the composite material acquires an amount of the desired property as a function of the amount of interconnectivity of the network of filler particles.

### Claim 25 (depends on 24)

The composition of claim 24, wherein the amount of interconnectivity of the network of filler particles is a function of one or more conditions selected from: a ratio of an average size of the polymer particles to an average size of the filler particles; a volume fraction of filler particles in the composite material.

### Claim 26 (depends on 24)

The composition of claim 24, wherein the amount of interconnectivity of the network of filler particles is a function of one or more conditions under which the composite material was made, wherein the conditions are selected from: a method of mixing the polymer particles and the filler particles; a temperature at which the composite material was made; a pressure at which the composite material was compressed; an amount of time for which the composite material was compressed.