# US 2006/0154483 A1 · Method of providing a structure using self-aligned features

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154483 A1
- Document ID: US20060154483A1
- Status: Published application
- Kind: A1
- Application number: 11/277,340
- Filed: 2006-03-23
- Published: 2006-07-13
- Earliest claimed: 2000-08-22
- Assignees: Micron Technology, Inc.
- Inventors: Dinesh Chopra; Kevin Donohoe; Cem Basceri
- Web page: https://patentgrep.com/patent/US20060154483A1

## CPC

- H10D 64/01316: {the conductor comprising a layer of elemental metal contacting the insulator, e.g. Ta, W, Mo or Al}
- H10D 1/042: {using deposition processes to form electrode extensions}
- H10D 1/716: {having vertical extensions}
- H10D 30/0225: {using an initial gate mask complementary to the prospective gate location, e.g. using dummy source and drain electrodes}
- H10P 14/47: Electrolytic deposition, i.e. electroplating; Electroless plating
- H10P 52/403: {of conductive or resistive materials}
- H10W 20/057: {by selectively depositing, e.g. by using selective CVD or plating}
- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In a copper plating process, a seed layer is uniformly deposited over a surface, including lining a high aspect ratio trench defined by that surface. A mask layer is provided using a process that fails to deposit in the trench. In one exemplary embodiment, the failure is due to the decrease in the isotropic flux of neutrals toward the bottom of the trench. Copper is subsequently electroplated. Because the seed layer is exposed only within the trench, copper deposits only therein. The self-aligned mask prevents plating outside of the trench. A chemical-mechanical planarization step removes the mask and the seed layer extending beyond the trench, leaving a copper structure within the trench. The structure may serve as a conductive line, an interconnect, or a capacitor plate.

## Claims

### Claim 1

A method of depositing a conductive material into a trench defined by a surface of a semiconductor device, said method comprising:
covering said surface of said semiconductor device with a seed layer, wherein a portion of said seed layer lines said trench;
depositing a mask over said seed layer in a manner that exposes said portion of said seed layer; and
plating said conductive material onto said portion of said seed layer.

### Claim 2 (depends on 1)

The method in claim 1, wherein said step of plating said conductive material comprises plating a selection of copper, platinum, silver, gold, cobalt, and nickel.

### Claim 3 (depends on 2)

The method in claim 2, wherein said depositing step comprises providing a plasma.

### Claim 4 (depends on 3)

The method in claim 3, wherein said step of depositing a mask comprises depositing a dielectric.

### Claim 5

A method of selectively depositing a conductive material over a surface of a semiconductor device, said method comprising:
selectively depositing a mask over a seed layer on said surface of said semiconductor device; and
plating a metal over said surface, wherein said plating step is guided by said mask.

### Claim 6 (depends on 5)

The method in claim 5, wherein said step of plating a metal comprises plating a metal over at least one unmasked portion of said surface.

### Claim 7 (depends on 6)

The method in claim 6, wherein said depositing step comprises depositing a mask onto the seed layer outside a trench, wherein said seed layer is configured to encourage plating of said metal.

### Claim 8 (depends on 7)

The method in claim 7, wherein said step of depositing a mask onto the seed layer comprises depositing said mask onto the seed layer comprising said metal.

### Claim 9

A method of processing a semiconductor substrate comprising a first portion and a complementary second portion, said comprising:
selectively depositing a first material over said first portion of said semiconductor substrate;
selectively depositing a second material over a second portion of said semiconductor substrate;
wherein said step of selectively depositing a first material comprises depositing said first material over said first portion to the exclusion of said second portion; and
wherein said step of selectively depositing a second material comprises depositing said second material over said second portion to the exclusion of said first portion.

### Claim 10 (depends on 9)

The method in claim 9, wherein:
said step of selectively depositing a first material comprises depositing said first material only over said first portion; and
said step of selectively depositing a second material comprises depositing said second material only over said second portion.

### Claim 11 (depends on 9)

The method in claim 9, wherein:
said step of selectively depositing a first material comprises depositing said first material at a first elevation over said semiconductor substrate; and
said step of selectively depositing a second material comprises depositing said second material at at least a second elevation under said first elevation.

### Claim 12

A method of processing a circuit device comprising a surface defining a trench, said method comprising:
depositing a non-patterned layer over said surface of said circuit device, wherein said layer exposes said trench; and
adding a material within said trench, wherein said material avoids said layer.

### Claim 13 (depends on 12)

The method in claim 12, wherein said depositing step comprises:
refraining from affirmatively patterning said layer; and
allowing at least one factor that inhibits conformal deposition to affect said depositing step.

### Claim 14 (depends on 13)

The method in claim 13, wherein said allowing step comprises allowing an aspect ratio defined by said trench to inhibit conformal deposition of said layer.

### Claim 15

A method of managing a plurality of slurries comprising a first slurry configured to react with copper at a first rate and not with tantalum, a second slurry configured to react with tantalum and not with copper, and a third slurry configured to react with tantalum and with copper at a second rate slower than said first rate, said method comprising:
providing a semiconductor workpiece comprising:
a material defining a trench,
a tantalum layer inside and outside of said trench,
a seed layer inside and outside of said trench, wherein said seed layer comprises copper,
a mask layer outside of said trench and avoiding said inside of said trench, and
copper inside of said trench and avoiding an area immediately outside of said trench;
refraining from exposing said workpiece to said first slurry and said second slurry; and
chemically-mechanically planarizing said workpiece using said third slurry.

### Claim 16

A method of providing tantalum and copper in a trench defined by a support surface, said method comprising:
depositing tantalum inside said trench and immediately outside said trench, depositing a first amount of copper inside said trench and immediately outside said trench;
depositing a second amount of copper inside said trench to the exclusion of depositing immediately outside of said trench; and
removing copper and tantalum immediately outside of said trench in a single CMP step.

### Claim 17 (depends on 16)

The method in claim 16, further comprising:
depositing a mask immediately outside of said trench to the exclusion of depositing inside said trench, wherein said step of depositing a mask comprises depositing said mask after said step of depositing a first amount of copper and before said step of depositing a second amount of copper; and
removing said mask after said step of depositing a second amount of copper.

### Claim 18 (depends on 17)

The method of claim 17, wherein said step of depositing a first amount of copper comprises depositing a copper layer about 1000 angstroms thick.

### Claim 19 (depends on 17)

The method in claim 17, wherein said removing step comprises removing copper outside of said trench at a rate of about 1000 angstroms per minute.

### Claim 20 (depends on 17)

The method in claim 17, wherein said removing step comprises removing copper outside of said trench at a rate of at most 1000 angstroms per minute.

### Claim 21 (depends on 20)

The method in claim 20, wherein said removing step comprises removing copper outside of said trench at a rate of about 650 angstroms per minute.