# US 2006/0154481 A1 · Decreasing Metal-Silicide Oxidation During Wafer Queue Time

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154481 A1
- Document ID: US20060154481A1
- Status: Published application
- Kind: A1
- Application number: 10/905,517
- Filed: 2005-01-07
- Published: 2006-07-13
- Earliest claimed: 2005-01-07
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Zhen-Cheng Wu; Cheng-Hung Chang; Yu-Lien Huang; Shwang-Ming Cheng
- Web page: https://patentgrep.com/patent/US20060154481A1

## CPC

- H10W 20/065: {by making at least a portion of the conductive part non-conductive, e.g. by oxidation}
- H10D 30/0212: {using self-aligned silicidation}
- H10P 95/94: {Hydrogenation or deuterisation, e.g. using atomic hydrogen from a plasma}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed herein are various embodiments of semiconductor devices and related methods of manufacturing a semiconductor device. In one embodiment, a method includes providing a semiconductor substrate and forming a metal silicide on the semiconductor substrate. In addition, the method includes treating an exposed surface of the metal silicide with a hydrogen/nitrogen-containing compound to form a treated layer on the exposed surface, where the composition of the treated layer hinders oxidation of the exposed surface. The method may then further include depositing a dielectric layer over the treated layer and the exposed surface of the metal silicide.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, the method comprising:
providing a semiconductor substrate;
forming a metal silicide on the semiconductor substrate; and
treating an exposed surface of the metal silicide with a hydrogen/nitrogen-containing compound to form a treated layer on the exposed surface, the treated layer hindering oxidation of the exposed surface.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the treating further comprises treating the exposed surface for less than 30 seconds.

### Claim 3 (depends on 2)

The method according to claim 2, wherein treating further comprises treating the exposed surface for about 10 seconds.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the hydrogen/nitrogen-containing compound is a hydrogen/nitrogen-containing plasma.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the hydrogen/nitrogen-containing compound is selected from the group consisting of NH3, H2+N2, and NH3+N2.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the treating further comprises treating the exposed surface at a temperature of about 200-500° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the treating further comprises treating the exposed surface using a flow rate of 3200-4000 sccm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the treating further comprises treating the exposed surface at a pressure of about 3.5 Torr.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the treating further comprises treating the exposed surface using a high frequency/low frequency radio frequency of about 300-600 W/0 W.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising treating the exposed surface after performing a contact etch to create a trench down to the metal silicide.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising depositing a contact etch stop layer over the treated layer.

### Claim 12 (depends on 1)

The method according to claim 1, wherein forming a metal silicide comprises forming a metal silicide selected from the group consisting of nickel silicide, cobalt silicide, titanium silicide, tantalum silicide, and tungsten silicide.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the forming comprises forming nickel silicide, and the treating comprises treating an exposed surface of the nickel silicide with NH3 plasma to form a Ni—Si—N treated layer on the exposed surface, the treated layer hindering the formation of NiO on the exposed surface.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the treating further comprises treating the exposed surface for less than about 30 seconds, at a temperature of about 200-500° C., using a flow rate of 3200-4000 sccm, at a pressure of about 3.5 Torr, and using a high frequency/low frequency radio frequency of about 300-600 W/0 W.

### Claim 15

A semiconductor device, comprising:
a semiconductor substrate;
a metal silicide formed on the semiconductor substrate;
a treated layer formed from an exposed surface of the metal silicide by treating the exposed surface with a hydrogen/nitrogen-containing compound, the treated layer hindering oxidation of the exposed surface.

### Claim 16 (depends on 15)

The device according to claim 15, wherein the treated layer is a nitrogen-containing layer.

### Claim 17 (depends on 15)

The device according to claim 15, further comprising a contact etch stop layer deposited over the treated layer.

### Claim 18 (depends on 15)

The device according to claim 15, wherein the metal silicide is selected from the group consisting of nickel silicide, cobalt silicide, titanium silicide, tantalum silicide, and tungsten silicide.

### Claim 19 (depends on 15)

The device according to claim 15, wherein the semiconductor device is a transistor.

### Claim 20 (depends on 15)

The device according to claim 15, wherein the metal silicide comprises nickel silicide, and the treated layer comprises Ni—Si—N formed by treating the exposed surface of the nickel silicide with NH3 plasma, the treated layer hindering the formation of NiO on the exposed surface.