# US 2006/0154470 A1 · Integrated circuit having structural support for a flip-chip interconnect pad and method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154470 A1
- Document ID: US20060154470A1
- Status: Published application
- Kind: A1
- Application number: 11/033,009
- Filed: 2005-01-11
- Published: 2006-07-13
- Earliest claimed: 2005-01-11
- Assignees: Freescale Semiconductor, Inc.
- Inventors: Scott Pozder; Kevin Hess; Pak Leung; Edward Travis; Brett Wilkerson; David Wontor; Jie-Hua Zhao
- Web page: https://patentgrep.com/patent/US20060154470A1

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 20/40: Interconnections external to wafers or substrates, e.g. back-end-of-line [BEOL] metallisations or vias connecting to gate electrodes
- H10W 72/90: Bond pads, in general
- H10W 72/07251: {characterised by changes in properties of the bump connectors during connecting}
- H10W 72/251: {Materials}
- H10W 72/29: Bond pads specially adapted therefor
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A technique for alleviating the problems of defects caused by stress applied to bond pads (32) includes, prior to actually making an integrated circuit (10), adding dummy metal lines (74, 76) to interconnect layers (18, 22, 26) to increase the metal density of the interconnect layers. These problems are more likely when the interlayer dielectrics (16, 20, 24) between the interconnect layers are of a low-k material. A critical area or force area (64) around and under each bond pad defines an area in which a defect may occur due to a contact made to that bond pad. Any interconnect layer in such a critical area that has a metal density below a certain percentage can be the cause of a defect in the interconnect layers. Any interconnect layer that has a metal density below that percentage in the critical area has dummy metal lines added to it.

## Claims

### Claim 1

An integrated circuit, comprising:
a substrate having active circuitry;
a bond pad over the substrate;
a force region around and under the bond pad characterized by being susceptible to defects due to contacts to the bond pad;
a stack of interconnect layers, wherein each interconnect layer has a portion in the force region; and
a plurality of interlayer dielectrics separating the interconnect layers of the stack of interconnect layers and having vias for interconnecting the interconnect layers of the stack of interconnect layers;
wherein at least one interconnect layer of the stack of interconnect layers comprises functional metal lines and dummy metal lines in the portion that is in the force region to obtain a predetermined metal density in the portion that is in the force region.

### Claim 2 (depends on 1)

The integrated circuit of claim 1, further comprising a conductive ball on the bond pad.

### Claim 3 (depends on 1)

The integrated circuit of claim 1, wherein the dummy metal lines run in two directions orthogonal to each other.

### Claim 4 (depends on 1)

The integrated circuit of claim 1, wherein each of the functional metal lines is one of a signal line or a power line.

### Claim 5 (depends on 1)

The integrated circuit of claim 1, wherein the predetermined metal density is less than forty percent.

### Claim 6

A method of making an integrated circuit, comprising:
providing a circuit design having a layout comprising:
a substrate having active circuitry;
a stack of interconnect layers for interconnecting the active circuitry;
a plurality of interlayer dielectrics for insulating the interconnect layers of the stack of interconnect layers and for connecting the interconnect layers of the stack of interconnect layers with vias;
a bond pad;
defining a force region under and around the bond pad;
determining which interconnect layers of the stack of interconnect layers have a metal density that is a less than a predetermined percentage;
obtaining a modified design by adding dummy metal lines to the interconnect layers of the stack of interconnect layers that were determined to have less than the predetermined percentage sufficient to raise the metal density to at least the predetermined percentage; and
making the integrated circuit according to the modified design.

### Claim 7 (depends on 6)

The method of claim 6, wherein the predetermined percentage is not greater than forty percent.

### Claim 8 (depends on 6)

The method of claim 6, wherein the predetermined percentage is not greater than fifty-five percent.

### Claim 9 (depends on 6)

The method of claim 6, wherein the force region is a region in which the interconnect layers of the stack of interconnect layers are susceptible to stress from the bond pad due to assembly or other processes.

### Claim 10 (depends on 6)

The method of claim 6, wherein the interconnect layers of the stack of interconnect layers comprise copper and the plurality of interlayer dielectrics are characterized as comprising dielectric layers having a relative permittivity less than four.

### Claim 11

A method of making an integrated circuit having a plurality of bond pads, comprising:
developing a circuit design of the integrated circuit;
developing a layout of the integrated circuit according to the circuit design, wherein the layout comprises a plurality of interconnect layers;
defining a force region around and under a first bond pad of the plurality of bond pads, wherein the force region comprises a first portion of each of the plurality of interconnect layers;
identifying a first interconnect layer of the plurality of interconnect layers in which the first portion of the first interconnect layer has a metal density below a predetermined percentage;
modifying the layout by adding dummy metal lines to the first portion of the first interconnect layer to increase the metal density of the first portion of the first interconnect layer; and
making the integrated circuit comprising the dummy metal lines.

### Claim 12 (depends on 11)

The method of claim 11, wherein each of the plurality of interconnect layers comprises copper.

### Claim 13 (depends on 11)

The method of claim 11, wherein the layout comprises low-k dielectric layers separating the plurality of interconnect layers, wherein the low-k dielectric layers have vias for interconnecting the plurality of interconnect layers.

### Claim 14 (depends on 11)

The method of claim 11, wherein the making the integrated circuit further comprises forming conductive balls on the plurality of bond pads.

### Claim 15 (depends on 11)

The method of claim 11, wherein the plurality of interconnect layers comprise copper.

### Claim 16 (depends on 11)

The method of claim 11, wherein the predetermined percentage is not greater than fifty-five percent.

### Claim 17 (depends on 11)

The method of claim 11, wherein the predetermined percentage is not greater than forty percent.

### Claim 18 (depends on 11)

The method of claim 11, wherein the dummy metal lines run in one of two directions in which the two directions are orthogonal to each other.

### Claim 19 (depends on 11)

The method of claim 11, wherein the first portion of the first interconnect layer comprises functional metal lines.

### Claim 20

A method of making an integrated circuit having a plurality of bond pads, comprising:
developing a circuit design of the integrated circuit;
developing a layout of the integrated circuit according to the circuit design, wherein the layout comprises a plurality of metal-containing interconnect layers that extend under the plurality of bond pads;
modifying the layout by adding dummy metal lines to the plurality of metal-containing interconnect layers to achieve a metal density of at least forty percent for each of the plurality of metal-containing interconnect layers; and
forming the integrated circuit comprising the dummy metal lines.