# US 2006/0154456 A1 · Crystallized semicoductor thin film manufacturing method and its manufacturing apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154456 A1
- Document ID: US20060154456A1
- Status: Published application
- Kind: A1
- Application number: 10/542,447
- Filed: 2004-01-13
- Published: 2006-07-13
- Earliest claimed: 2003-01-15
- Assignees: Sharp Kabushiki Kaisha
- Inventors: Yoshihiro Taniguchi; Hiroshi Tsunazawa; Shinya Okazaki; Tetsuya Inui
- Web page: https://patentgrep.com/patent/US20060154456A1

## CPC

- H10P 14/3816: {Pulsed laser beam}
- B23K 26/04: Automatically aligning, aiming or focusing the laser beam, e.g. using the back-scattered light
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3238: {being insulating materials}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3456: {Polycrystalline}
- H10P 14/381: {Beam shaping, e.g. using a mask}
- H10P 14/3812: {Shape of mask}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A fabrication method of a crystallized semiconductor thin film is such that: by performing pulse irradiation of energy beams in a minute slit shape to a semiconductor thin film (5), the semiconductor thin film (5) of an region to which the energy beams are irradiated is fused and solidified over the whole area in a thickness direction so as to be crystallized, a main beam (6) and a sub beam (7), having smaller energy per unit area than that of the main beam (6), which adjoins the main beam (6), being irradiated to the semiconductor thin film (5).

## Claims

### Claim 1

A method for fabricating a crystallized semiconductor thin film, comprising the step of irradiating a main energy beam and a sub energy beam, whose energy per unit area is smaller than that of the main energy beam and lower than an energy threshold at which a semiconductor thin film fuses, to the semiconductor thin film formed on a substrate, so as to fuse the semiconductor thin film over a whole area in a thickness direction and crystallize the semiconductor thin film, wherein
the sub energy beam is irradiated so as to adjoin the main energy beam.

### Claim 2 (depends on 1)

The method as set forth in claim 1, wherein there is performed pulse irradiation of the main energy beam and/or the sub energy beam to the semiconductor thin film.

### Claim 3 (depends on 1)

The method as set forth in claim 1, wherein irradiation of the main energy beam is started at a time when energy per unit area with which the sub energy beam is irradiated to a surface of the semiconductor thin film reaches a maximum.

### Claim 4 (depends on 1)

The method as set forth in claim 1, wherein the main energy beam and the sub energy beam are irradiated so as to be different from each other in terms of a wavelength.

### Claim 5 (depends on 4)

The method as set forth in claim 4, wherein a laser light whose wavelength is 532 nm is irradiated to the semiconductor thin film as the main energy beam and a laser light whose wavelength is 308 nm is irradiated to the semiconductor thin film as the sub energy beam.

### Claim 6 (depends on 1)

The method as set forth in claim 1, wherein:
the substrate has a thermal conductive insulator film formed between the substrate and the semiconductor thin film, and
the thermal conductive insulator film is made of at least one material selected from aluminum nitride, silicon nitride, aluminum oxide, magnesium oxide, and cerium oxide.

### Claim 7

A fabrication device for fabricating a crystallized semiconductor thin film, comprising energy beam irradiating means for performing pulse irradiation so that a main energy beam and a sub energy beam, whose energy per unit area is smaller than that of the main energy beam and lower than an energy threshold at which a semiconductor thin film fuses, are irradiated to a semiconductor thin film formed on a substrate, wherein
the energy beam irradiating means irradiates the sub energy beam so that the sub energy beam adjoins the main energy beam.

### Claim 8 (depends on 7)

The fabrication device as set forth in claim 7, wherein:
the energy beam irradiating means includes (i) a mask for forming patterns of the main energy beam and the sub energy beam irradiated to the semiconductor thin film and (ii) an imaging lens for imaging said main energy beam and sub energy beam, which have penetrated said mask, on the semiconductor thin film, and
the mask forms a pattern of the main energy beam and a pattern of the sub energy beam adjoining the pattern of the main energy beam.

### Claim 9 (depends on 7)

The fabrication device as set forth in claim 7, wherein the energy beam irradiating means performs pulse irradiation of the main energy beam and/or the sub energy beam.

### Claim 10 (depends on 7)

The fabrication device as set forth in claim 7, wherein the energy beam irradiating means irradiates a laser light.

### Claim 11

A fabrication device for fabricating a crystallized semiconductor thin film, comprising:
a first beam irradiating section for irradiating a main energy beam;
a first mask for forming a pattern of the main energy beam irradiated by the first beam irradiating section;
a second beam irradiating section for irradiating a sub energy beam whose energy per unit area is smaller than that of the main energy beam and lower than an energy threshold at which a crystallized semiconductor thin film fuses;
a second mask for forming a pattern of the sub energy beam irradiated by the second beam irradiating section; and
an imaging lens for imaging patterns, respectively formed by the first mask and the second mask, on a semiconductor thin film, wherein
the first mask and the second mask form patterns by which the sub energy beam is irradiated to the semiconductor thin film so as to adjoin the main energy beam.

### Claim 12 (depends on 11)

The fabrication device as set forth in claim 11, comprising:
controlling means for controlling a timing at which the main energy beam is irradiated by the first beam irradiating section and a timing at which the sub energy beam is irradiated by the second beam irradiating section; and
adjusting means for respectively adjusting energy per unit area with which the main energy beam is irradiated by the first beam irradiating section and energy per unit area with which the sub energy beam is irradiated by the second beam irradiating section.

### Claim 13 (depends on 11)

The fabrication device as set forth in claim 11, wherein the first beam irradiating section and the second beam irradiating section irradiate energy beams different from each other in terms of a wavelength.

### Claim 14 (depends on 11)

The fabrication device as set forth in claim 11, wherein the first beam irradiating section and/or the second beam irradiating section perform pulse irradiation of energy beams.