# US 2006/0154454 A1 · Method for fabricating gaN-based nitride layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154454 A1
- Document ID: US20060154454A1
- Status: Published application
- Kind: A1
- Application number: 10/543,318
- Filed: 2004-08-21
- Published: 2006-07-13
- Earliest claimed: 2003-11-28
- Assignees: Epivalley Co., Ltd.; Samsung Electro-Mechanics Co., Ltd.
- Inventors: Soo Jeon; Moon Jang
- Web page: https://patentgrep.com/patent/US20060154454A1

## CPC

- C30B 29/403: {AIII-nitrides}
- C30B 25/02: Epitaxial-layer growth
- C30B 29/36: Carbides
- C30B 29/406: {Gallium nitride}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3208: {Silicon carbide}
- H10P 14/3216: {Nitrides}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3416: {Nitrides}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

The present invention relates to a method for fabricating a gallium nitride(GaN) based nitride layer including a step of forming a wetting layer having of forming a wetting layer having a composition of In(x1)Ga(y1)N (0<x1≦1, 0≦y1<1, x1+y1=1) on the silicon carbide buffer layer, and a step of forming a nitride layer containing gallium and nitrogen on the wetting layer, thereby can implement an opto-electronic device of high efficiency and high reliability.

## Claims

### Claim 1

A method for fabricating a GaN-based nitride layer including:
a first step of forming a non-single crystalline silicon carbide buffer layer having a thickness of 5 Å to 200 Å on a sapphire substrate;
a second step of forming a wetting layer having a composition of In(x1)Ga(y1)N (0≦x1≦1, 0≦y1<1, x1+y1=1) on the silicon carbide buffer layer; and
a third step of forming a nitride layer comprising gallium and nitrogen on the wetting layer.

### Claim 2 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein in the first step, at least one of CBr4 or CxHy (where x are y are integers) is used as a carbon precursor.

### Claim 3 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein the growth temperature (T) of the silicon carbide buffer layer is within a range of 600° C.≦T<990° C.

### Claim 4 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein the wetting layer is formed in a single layer.

### Claim 5 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein the wetting layer is formed in a combination of two or more layers.

### Claim 6 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein the growth temperature of the wetting layer is within a range of 400° C. to 900° C.

### Claim 7 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein the wetting layer has a thickness of 100 Å to 500 Å.

### Claim 8 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein in the second step, the V/III ratio has a value and the value is within a range of 1 to 5000 and is lower than a V/III ratio causing hillocks to occur in the nitride layer.

### Claim 9 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein the nitride layer is made of a combination of two or more layers.

### Claim 10 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein the growth temperature of the nitride layer is within a range of 800° C. to 1200° C.

### Claim 11 (depends on 1)

The method for fabricating a GaN-based nitride layer of claim 1, wherein in the third step, the V/III ratio has a value of 500 to 20000.

### Claim 12

A method for fabricating a GaN-based nitride layer above a substrate including:
a step of forming a non-single crystalline silicon carbide buffer layer on the substrate prior to growing the GaN-based nitride layer.

### Claim 13 (depends on 12)

The method for fabricating a GaN-based nitride layer of claim 12 further including:
a step of forming a wetting layer having a, composition of In(x1)Ga(y1)N (0≦x1≦1, 0≦y1<1, x1+y1=1) on the silicon carbide buffer layer prior to growing the GaN-based nitride layer.

### Claim 14

A method for fabricating a GaN-based nitride layer including:
a first step of forming a silicon carbide buffer layer on a substrate;
a second step of forming a wetting layer having a composition of In(x1)Ga(y1)N (0<x1≦1, 0≦y1≦1, x1+y1=1) on the silicon carbide buffer layer at a first temperature; and
a third step of forming a nitride layer containing gallium and nitrogen on the wetting layer at a temperature higher than the first temperature.

### Claim 15

A method for fabricating a GaN-based nitride layer above a substrate including:
a step of forming a silicon carbide buffer layer on the substrate at a temperature of 600° C. to 990° C. prior to growing the GaN-based nitride layer.

### Claim 16 (depends on 15)

The method for fabricating a GaN-based nitride layer of claim 15 further including:
a step of forming a wetting layer having a composition of In(x1)Ga(y1)N (0≦x1≦1, 0≦y1<1, x1+y1=1) on the silicon carbide buffer layer prior to growing the GaN-based nitride layer.

### Claim 17

A method for fabricating a GaN-based nitride layer above a substrate including:
a step of forming a silicon carbide buffer layer of 5 Å to 200 Å in thickness on the substrate prior to growing the GaN-based nitride layer.

### Claim 18 (depends on 17)

The method for fabricating a GaN-based nitride layer of claim 17 further including:
a step of forming a wetting layer having a composition of In(x1)Ga(y1)N (0≦x1≦1, 0≦y1<1, x1+y1=1) on the silicon carbide buffer layer prior to growing the GaN-based nitride layer.