# US 2006/0154439 A1 · Method of fabricating semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154439 A1
- Document ID: US20060154439A1
- Status: Published application
- Kind: A1
- Application number: 11/330,747
- Filed: 2006-01-12
- Published: 2006-07-13
- Earliest claimed: 2005-01-13
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Chung-Ho Lim
- Web page: https://patentgrep.com/patent/US20060154439A1

## CPC

- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In a method of fabricating a semiconductor device, trenches are formed defining active regions at predetermined portions of a semiconductor substrate. A thermal oxide layer and a liner layer are sequentially formed covering inner walls of the trenches and upper surfaces of the active regions. Device isolation patterns are formed filling the trenches, in which the liner layer is formed, and an upper portion of the liner layer at the upper portions of the active regions are exposed. The exposed liner layer is dry etched to expose an upper portion of the thermal oxide layer at the upper portions of the active regions. The exposed thermal oxide layer is etched to expose the upper surfaces of the active regions.

## Claims

### Claim 1

A method of fabricating a semiconductor device, comprising:
forming trenches defining active regions at predetermined portions of a semiconductor substrate;
sequentially forming a thermal oxide layer and a liner layer covering inner walls of the trenches and upper surfaces of the active regions;
forming device isolation patterns filling the trenches, in which the liner layer is formed, and exposing an upper portion of the liner layer at the upper portions of the active regions;
dry etching the exposed liner layer to expose an upper portion of the thermal oxide layer at the upper portions of the active regions; and
etching the exposed thermal oxide layer to expose the upper surfaces of the active regions.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the trenches includes:
forming mask patterns at the upper portions of the active regions;
forming the trenches defining the active regions by anisotropic etching of the semiconductor substrate using the mask patterns as an etch mask; and
removing the mask patterns to expose the active regions.

### Claim 3 (depends on 2)

The method of claim 2, wherein removing the mask patterns completely exposes an entire surface of the semiconductor substrate in which the trenches are formed.

### Claim 4 (depends on 1)

The method of claim 1, wherein the thermal oxide layer is formed following complete exposure of an entire surface of the semiconductor substrate in which the trenches are formed.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming the liner layer includes conformally forming a silicon nitride layer with an etch selectivity with respect to the thermal oxide layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming the device isolation patterns includes:
forming a device isolation layer filling the trenches on the resulting structure in which the liner layer is formed; and
dry etching the device isolation layer using an etch recipe with high etch selectivity with respect to the liner layer until the upper portion of the liner layer is exposed.

### Claim 7 (depends on 6)

The method of claim 6, wherein forming the device isolation patterns further includes, before the dry etching of the device isolation layer, planarizing the device isolation layer to an extent such that the upper portion of the line layer is not exposed.

### Claim 8 (depends on 6)

The method of claim 6, wherein an etch stop point of the dry etching of the device isolation layer is determined using a dry etching recipe with high etch selectivity with respect to the liner layer by controlling composition of an etch reaction gas.

### Claim 9 (depends on 1)

The method of claim 1, wherein an etch stop point of the dry etching of the liner layer is determined using a dry etching recipe with high etch selectivity with respect to the thermal oxide layer by controlling composition of an etch reaction gas.

### Claim 10 (depends on 1)

The method of claim 1, further comprising, before etching the thermal oxide layer, performing an ion implantation process of implanting impurities into the active regions by using the thermal oxide layer as a buffer layer.

### Claim 11 (depends on 1)

The method of claim 1, further comprising, after etching the thermal oxide layer, forming a gate oxide layer on the exposed upper portion of the active regions using a thermal oxidation process.

### Claim 12

A method of fabricating a semiconductor memory device, comprising:
forming mask patterns on a semiconductor substrate;
forming trenches defining active regions by anisotropic etching of the semiconductor substrate using the mask patterns as an etch mask;
removing the mask patterns to expose the active regions;
sequentially forming a thermal oxide layer and a liner layer covering upper portions of the active regions and inner walls of the trenches on the resulting structure in which the upper portions of the active regions are exposed;
forming a device isolation layer filling the trenches on the liner layer;
etching the device isolation layer to expose an upper surface of the liner layer and to form device isolation patterns filling the trenches;
dry etching the liner layer to expose the upper portion of the thermal oxide layer at the upper portions of the active regions;
etching the exposed thermal oxide layer to expose the upper portions of the active regions; and
forming a gate oxide layer on the exposed upper portions of the active regions.

### Claim 13 (depends on 12)

The method of claim 12, wherein removing the mask patterns completely exposes an entire surface of the semiconductor substrate in which the trenches are formed, and wherein the thermal oxide layer is formed following complete exposure of an entire surface of the semiconductor substrate in which the trenches are formed.

### Claim 14 (depends on 12)

The method of claim 12, wherein forming the device isolation patterns includes:
planarizing the device isolation layer to an extent such that the upper portion of the liner layer is not exposed; and
dry etching the planarized device isolation layer using an etch recipe with high etch selectivity with respect to the liner layer until the upper portion of the liner is exposed.

### Claim 15 (depends on 14)

The method of claim 14, wherein dry etching the planarized device isolation layer determines an etch stop point thereof by controlling composition of an etch reaction gas.

### Claim 16 (depends on 12)

The method of claim 12, wherein an etch stop point of the dry etching of the liner layer is determined using a dry etching recipe with high etch selectivity with respect to the thermal oxide layer by controlling composition of an etch reaction gas.