# US 2006/0154428 A1 · Increasing doping of well compensating dopant region according to increasing gate length

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154428 A1
- Document ID: US20060154428A1
- Status: Published application
- Kind: A1
- Application number: 10/905,591
- Filed: 2005-01-12
- Published: 2006-07-13
- Earliest claimed: 2005-01-12
- Assignees: International Business Machines Corporation
- Inventors: Omer Dokumaci
- Web page: https://patentgrep.com/patent/US20060154428A1

## CPC

- H10P 30/222: {characterised by the angle between the ion beam and the crystal planes or the main crystal surface (characterised by the angle between the ion beam and the mask H10P30/221)}
- H10D 30/0217: {forming self-aligned punch-through stoppers or threshold implants under gate regions}
- H10P 30/221: {characterised by the angle between the ion beam and the mask}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods and resulting structure of implementing a compensating implant that creates more compensation doping as the gate length is increased are disclosed. In particular, the invention performs an angled compensation implant through a gate opening during the damascene process such that the compensating dopant concentration increases as the gate length increases. In this fashion, the threshold voltage of a longer device is reduced much more than the threshold voltage of a shorter device, thereby reducing the threshold voltage of the longer device to acceptable levels without affecting the threshold voltage of the shorter device. The invention is especially advantageous relative to super-steep retrograde wells.

## Claims

### Claim 1

A method of implementing a compensating dopant region, the method comprising the steps of:
providing a gate electrode including a spacer surrounding a gate material area and a gate dielectric, the gate electrode being positioned over a well in a substrate;
forming a planar dielectric layer about the gate electrode;
removing the gate material area and the gate dielectric from the gate electrode to form a gate opening;
performing an angled implant into the gate opening to form the compensating dopant region in the well, wherein the formed compensating dopant region provides compensation as a function of a length of the gate opening; and
annealing to activate the compensating dopant region.

### Claim 2 (depends on 1)

The method of claim 1, wherein an amount of dopant implanted during the performing step increases with the length of the gate opening.

### Claim 3 (depends on 1)

The method of claim 1, wherein an amount of reduction of a threshold voltage created by the compensating dopant region increases with the length of the gate opening.

### Claim 4 (depends on 1)

The method of claim 1, wherein the planar dielectric layer includes one of: silicon dioxide (SiO2) and silicon nitride (Si3N4).

### Claim 5 (depends on 1)

The method of claim 1, wherein the removing step includes performing an isotropic etch.

### Claim 6 (depends on 1)

The method of claim 1, wherein the annealing step includes one of exposing the gate opening to a laser and performing a flash anneal.

### Claim 7 (depends on 1)

The method of claim 1, further comprising the step of re-forming the gate dielectric and the gate material area.

### Claim 8 (depends on 6)

The method of claim 6, wherein the gate dielectric includes at least one of silicon dioxide (SiO2), oxynitride (ON), silicon nitride (Si3N4) and a high dielectric constant material.

### Claim 9 (depends on 1)

The method of claim 1, wherein the well includes a super-steep retrograde well.

### Claim 10

A semiconductor device structure comprising:
a gate electrode including a spacer surrounding a gate material area and a gate dielectric;
a super-steep retrograde well positioned under the gate electrode in a substrate; and
a compensating dopant region positioned with the super-steep retrograde well, wherein an amount of dopant in the compensating dopant region is based on a length of the gate material area.

### Claim 11 (depends on 10)

The semiconductor device structure of claim 10, wherein an amount of reduction of a threshold voltage created by the compensating dopant region increases with a length of the gate material area.

### Claim 12 (depends on 10)

The semiconductor device structure of claim 10, wherein the super-steep retrograde well has a dopant concentration greater than 5.0e18/cm3.

### Claim 13 (depends on 10)

The semiconductor device structure of claim 10, wherein the compensation dopant region has a dopant concentration of no less than 1.0e18/cm3 and no greater than 1.0e19/cm3.

### Claim 14 (depends on 10)

The semiconductor device structure of claim 10, wherein the gate material area includes one of: doped polysilicon, metal and metal silicide.

### Claim 15 (depends on 10)

The semiconductor device structure of claim 10, wherein the gate dielectric includes at least one of silicon dioxide (SiO2), oxynitride (ON), silicon nitride (Si3N4) and a high dielectric constant material.

### Claim 16

A method of forming a gate electrode including a compensating dopant region, the method comprising the steps of:
providing a gate electrode including a spacer surrounding a gate material area and a gate dielectric, the gate electrode being positioned over a super-steep retrograde well in a substrate;
forming a planar dielectric layer about the gate electrode;
removing the gate material area and the gate dielectric from the gate electrode to form a gate opening;
performing an angled implant into the gate opening to form the compensating dopant region in the super-steep retrograde well, wherein the formed compensating dopant region provides compensation as a function of a length of the gate opening, such that an amount of dopant implanted increases with the length of the gate opening;
annealing to activate the compensating dopant region; and
re-forming the gate dielectric and the gate material area in the gate opening.

### Claim 17 (depends on 16)

The method of claim 16, wherein an amount of reduction of a threshold voltage created by the compensating dopant region increases with the length of the gate opening.

### Claim 18 (depends on 16)

The method of claim 16, wherein the planar dielectric layer includes one of: silicon dioxide (SiO2) and silicon nitride (Si3N4).

### Claim 19 (depends on 16)

The method of claim 16, wherein the removing step includes performing an isotropic etch.

### Claim 20 (depends on 16)

The method of claim 16, wherein the annealing step includes one of exposing the gate opening to a laser and performing a flash anneal.