# US 2006/0154143 A1 · Coin type battery and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154143 A1
- Document ID: US20060154143A1
- Status: Published application
- Kind: A1
- Application number: 11/374,685
- Filed: 2006-03-13
- Published: 2006-07-13
- Earliest claimed: 2001-08-10
- Assignees: Matsushita Electric Industrial Co., Ltd.
- Inventors: Tetsuya Hayashi; Kazuyuki Hiranaga; Takahiro Teraoka; Shinichi Sakamoto; Satoshi Ogawa
- Web page: https://patentgrep.com/patent/US20060154143A1

## CPC

- H01M 10/0431: {Cells with wound or folded electrodes (H01M10/045 takes precedence)}
- H01M 4/06: Electrodes for primary cells
- H01M 6/06: Dry cells, i.e. cells wherein the electrolyte is rendered non-fluid
- H01M 10/0427: {Button cells}
- H01M 50/109: of button or coin shape
- H01M 2006/106: {Elliptic wound cells}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/49108: Electric battery cell making
- Y10T 29/4911: including sealing
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A positive electrode plate (11) and a negative electrode plate (12) are coiled around into a flat shape such that positive electrode layer faces (22a-22e) and negative electrode layer faces (23a-23f) are alternately layered upon one another with a separator interposed therebetween. Positional discrepancy detecting holes (41a, 41b, 42, 43, 44) are formed in the positive electrode layer faces (22a, 22b) and negative electrode layer face (23a) facing each other at the coiling start end, and in the positive electrode layer face (22e) and negative electrode layer face (23f) facing each other at the coiling finish end. The electrode plates are coiled into an electrode plate group, which is subjected to X-ray inspection for detecting positional displacement based on a discrepancy in the positions of the holes.

## Claims

### Claim at position 1

-12. (canceled)

### Claim 13

A method of manufacturing a coin type battery, comprising:
folding a strip of positive electrode plate formed of a plurality of positive electrode layer faces coupled together by a plurality of connecting pieces, and a strip of negative electrode plate formed of a plurality of negative electrode layer faces coupled together by a plurality of connecting pieces at the respective connecting pieces and coiling it around into an electrode plate group of flat form such that the positive electrode layer faces and the negative electrode layer faces are alternately layered upon one another with a separator interposed therebetween;
accommodating the electrode plate group into a sealing case;
injecting liquid electrolyte thereinto;
placing a cap case onto the sealing case via a gasket; and
crimping the cap case to seal the inside of the sealing case, characterized in that
the positive electrode plate and the negative electrode plate are respectively formed with positional discrepancy detecting cut-outs for detecting positional displacement between the positive electrode layer faces and the negative electrode layer faces when both electrode plates are coiled around;
after coiling around the positive electrode plate and the negative electrode plate into the electrode plate group, X-rays are irradiated thereto in a direction in which the electrode plates are layered so as to obtain transmitted X-ray images of the electrode plate group;
a positional discrepancy is detected, by processing the images, between the positional discrepancy detecting cut-outs in the positive electrode layer faces and the positional discrepancy detecting cut-outs in the negative electrode layer faces; and
when the detected positional discrepancy is within a predetermined permissible range, the electrode plate group is accommodated in the sealing case.