# US 2006/0154037 A1 · Polyimide-copper composite laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0154037 A1
- Document ID: US20060154037A1
- Status: Published application
- Kind: A1
- Application number: 11/052,829
- Filed: 2005-02-09
- Published: 2006-07-13
- Earliest claimed: 2005-01-07
- Assignees: Ube Industries, Ltd.
- Inventors: Hiroto Shimokawa; Kohji Narui; Toshinori Hosoma; Toshihiko Anno
- Web page: https://patentgrep.com/patent/US20060154037A1

## CPC

- B32B 9/005: {comprising one layer of ceramic material, e.g. porcelain, ceramic tile (layered products with at least two ceramic layers composed mainly of ceramic B32B18/00)}
- B32B 9/041: {of metal}
- B32B 15/08: of synthetic resin
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 27/281: {comprising polyimides}
- B32B 27/34: comprising polyamides
- H05K 3/025: {by transfer of thin metal foil formed on a temporary carrier, e.g. peel-apart copper}
- B32B 2250/05: 5 or more layers
- B32B 2250/40: Symmetrical or sandwich layers, e.g. ABA, ABCBA, ABCCBA
- B32B 2274/00: Thermoplastic elastomer material
- B32B 2307/306: Resistant to heat
- B32B 2307/732: Dimensional properties
- B32B 2457/08: PCBs, i.e. printed circuit boards
- H05K 1/0346: {containing N}
- H05K 2201/0154: Polyimide
- H05K 2203/0152: Temporary metallic carrier, e.g. for transferring material
- Y10T 428/24975: No layer or component greater than 5 mils thick
- Y10T 428/31681: Next to polyester, polyamide or polyimide [e.g., alkyd, glue, or nylon, etc.]
- Y10T 428/31721: Of polyimide
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A polyimide-copper composite laminate is composed of a metallic carrier having a thickness of 10-35 μm and a thin copper film having a thickness of 1-8 μm, and an intervening heat-resistant layer and an aromatic polyimide film directly fixed to the thin copper film without adhesive.

## Claims

### Claim 1

A polyimide-copper composite laminate comprising a metallic carrier having a thickness in the range of 10 to 35 μm and a thin copper film having a thickness in the range of 1 to 8 μm, and an intervening heat-resistant layer placed between the metallic carrier and the thin copper film and an aromatic polyimide film directly fixed to the thin copper film without adhesive.

### Claim 2 (depends on 1)

The polyimide-copper composite laminate of claim 1, in which the intervening heat-resistant layer is made of ceramic material or metal.

### Claim 3 (depends on 1)

The polyimide-copper composite laminate of claim 1, in which the aromatic polyimide film is fixed to the copper film at a peel strength of 0.7 N/mm or higher and the copper film is fixed to the metallic carrier at a peel strength of not higher than 0.2 N/mm.

### Claim 4 (depends on 1)

The polyimide-copper composite laminate of claim 1, in which the metallic carrier has a thickness in the range of 10 to 22 μm.

### Claim 5 (depends on 1)

The polyimide-copper composite laminate of claim 1, in which the metallic carrier has a thickness in the range of 15 to 22 μm.

### Claim 6 (depends on 1)

The polyimide-copper composite laminate of claim 1, in which the copper film has a thickness in the range of 1 to 3 μm.

### Claim 7 (depends on 1)

The polyimide-copper composite laminate of claim 1, in which the polyimide film is a multi-layer film comprising two thermoplastic aromatic polyimide layers and an intervening heat-resistant aromatic polyimide layer having no glass transition temperature below 300° C.

### Claim 8 (depends on 7)

The polyimide-copper composite laminate of claim 7, which further comprises a metallic carrier having a thickness in the range of 10 to 35 μm and a thin copper film having 1 to 8 μm, and an intervening heat-resistant layer placed between the metallic carrier and the thin copper film, the thin copper film is fixed to a free side of the aromatic polyimide film.

### Claim 9 (depends on 3)

The polyimide-copper composite laminate of claim 3, in which the peel strength between the aromatic polyimide film and the copper film shows no decrease after heat treatment at 150° C. for 168 hours.

### Claim 10 (depends on 3)

The polyimide-copper composite laminate of claim 3, being subjected to 300° C. for 0.1 min. or longer in the heat treatment in the course of a laminating procedure and which shows no foaming.

### Claim 11 (depends on 1)

A polyimide-copper composite laminate comprising a thin copper film having a thickness in the range of 1 to 8 μm and an aromatic polyimide film directly fixed to the thin copper film without adhesive, obtained by separating the carrier film from the polyimide-copper composite laminate of claim 1.

### Claim 12 (depends on 11)

The polyimide-copper composite laminate of claim 11, being subjected to an etching procedure.

### Claim 13 (depends on 11)

The polyimide-copper composite laminate of claim 11, which has pin-holes in numbers of at most 350/m2.