# US 2006/0152152 A1 · Organic electroluminescent device comprising electron shower treated hole injection layer and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0152152 A1
- Document ID: US20060152152A1
- Status: Published application
- Kind: A1
- Application number: 11/302,448
- Filed: 2005-12-14
- Published: 2006-07-13
- Earliest claimed: 2005-01-08
- Assignees: Samsung SDI Co., Ltd.
- Inventors: Mu-Gyeom Kim; Jong-Jin Park; Sang-Yeol Kim; Tae-Woo Lee
- Web page: https://patentgrep.com/patent/US20060152152A1

## CPC

- H10K 85/1135: {Polyethylene dioxythiophene [PEDOT]; Derivatives thereof}
- H10K 50/17: Carrier injection layers
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

An organic electroluminescent device has an anode formed on a substrate, a hole injection layer formed on the anode, wherein the hole injection layer is subjected with an electron shower treatment, an emitting layer formed on the hole injection layer, and a cathode formed on the emitting layer. With the electron shower treatment, impurities from the hole injection layer can be removed, and electrical surface resistance of the hole injection layer cab be increased so that performance and life characteristics of the organic electroluminescent device are improved.

## Claims

### Claim 1

An organic electroluminescent device, comprising:
an anode formed on a substrate;
an electron shower treated hole injection layer formed on the anode;
an emitting layer formed on the electron shower treated hole injection layer; and
a cathode formed on the emitting layer.

### Claim 2 (depends on 1)

The organic electroluminescent device of claim 1, wherein the electron shower treated hole injection layer is produced by carrying out a side electron shower method.

### Claim 3 (depends on 1)

The organic electroluminescent device of claim 1, wherein the electron shower treated hole injection layer is produced by an electron shower treatment carried out with an electron energy of 10 eV to 100 eV.

### Claim 4 (depends on 1)

The organic electroluminescent device of claim 1, wherein surface resistance of the electron shower treated hole injection layer is not greater than 110% initial surface resistance of a hole injection layer which is not treated with an electron shower.

### Claim 5 (depends on 1)

The organic electroluminescent device of claim 1, wherein the electron shower treated hole injection layer is produced by an electron shower treatment with a blowing treatment carried out in a nitrogen atmosphere.

### Claim 6 (depends on 1)

The organic electroluminescent device of claim 1, wherein the electron shower treated hole injection layer is produced by an electron shower treatment with heating under vacuum or in a nitrogen atmosphere.

### Claim 7 (depends on 1)

The organic electroluminescent device of claim 1, wherein the electron shower treated hole injection layer is made of copper phthalocyanine, starburst-type amines, poly(3,4-ethylenedioxythiophene) (PEDOT), or a mixture thereof.

### Claim 8 (depends on 1)

The organic electroluminescent device of claim 1, further comprising an electron transport layer stacked on the emitting layer.

### Claim 9 (depends on 8)

The organic electroluminescent device of claim 8, further comprising an electron injection layer stacked on the electron transport layer.

### Claim 10 (depends on 1)

The organic electroluminescent device of claim 1, further comprising an electron injection layer stacked on the emitting layer, the electron injection layer (EIL) being one selected from the group consisting of LiF, NaCl, CsF, Li2, BaO, Liq, and a mixture thereof.

### Claim 11

A method for preparing an organic electroluminescent device, comprising:
forming an anode on a substrate;
forming a hole injection layer on the anode;
performing an electron shower treatment on the hole injection layer;
forming an emitting layer on the hole injection layer; and
forming a cathode on the emitting layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the electron shower treatment is carried out by a side electron shower method.

### Claim 13 (depends on 11)

The method of claim 11, wherein the electron shower treatment comprises using an electron gun, and a distance from the electron gun to the hole injection layer ranges from 100 mm to 200 mm.

### Claim 14 (depends on 11)

The method of claim 11, wherein the electron shower treatment is carried out with an electron energy of 10 eV to 100 eV.

### Claim 15 (depends on 11)

The method of claim 11, wherein a processing time of the electron shower treatment is adjusted such that surface resistance of the hole injection layer is increased by not greater than 10% initial surface resistance.

### Claim 16 (depends on 11)

The method of claim 11, wherein the electron shower treatment comprises a blowing treatment carried out in a nitrogen atmosphere.

### Claim 17 (depends on 11)

The method of claim 11, wherein the electron shower treatment comprises heating under vacuum or in a nitrogen atmosphere.

### Claim 18 (depends on 11)

An organic electroluminescent device produced by the method of claim 11.

### Claim 19

A method for preparing an organic electroluminescent device, comprising:
forming an anode on a substrate;
forming a hole injection layer on the anode;
removing impurities or unstable ions from the hole injection layer;
forming an emitting layer on the hole injection layer; and
forming a cathode on the emitting layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the removal of the impurities is performed by side electron shower treatment.