# US 2006/0151911 A1 · Process and mold for molding and coating a substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0151911 A1
- Document ID: US20060151911A1
- Status: Published application
- Kind: A1
- Application number: 11/312,885
- Filed: 2005-12-20
- Published: 2006-07-13
- Earliest claimed: 2004-12-24
- Assignees: Bayer MaterialScience AG
- Inventors: Olaf Zollner; Thorsten Just; Jorg Tillack; Bernd Hausstatter; Michael Glawe; Klaus Konejung; Steffen Lang
- Web page: https://patentgrep.com/patent/US20060151911A1

## CPC

- B29C 37/0028: {In-mould coating, e.g. by introducing the coating material into the mould after forming the article}
- B29C 45/1615: {The materials being injected at different moulding stations}
- B29C 45/1679: {applying surface layers onto injection-moulded substrates inside the mould cavity, e.g. in-mould coating [IMC] (applying suface layers after ejection B29C45/0053)}
- B29C 67/246: {Moulding high reactive monomers or prepolymers, e.g. by reaction injection moulding [RIM], liquid injection moulding [LIM] (casting monomers B29C39/006, mixing construction B29B7/74)}
- B29C 45/561: {Injection-compression moulding}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A process for in-mold coating and a mold is disclosed. The process entails (i) obtaining a mold having at least two cavities, (ii) molding a thermoplastic substrate in a first cavity, (iii) introducing the substrate into a second cavity, and (iv) coating said substrate with lacquer, the coating being carried out under enhanced pressure.

## Claims

### Claim 1

A process for in-mold coating comprising
(i) obtaining a mold having at least two cavities,
(ii) molding a thermoplastic substrate in a first cavity,
(iii) introducing the substrate into a second cavity,
(iv) coating said substrate with lacquer, the coating being carried out under enhanced pressure and curing the lacquer.

### Claim 2 (depends on 1)

Process according to claim 1, characterized in that the coating with lacquer according to step (iv) is carried out by the reaction injection molding (RIM) process.

### Claim 3 (depends on 1, 2)

Process according to claim 1 or 2, wherein during step (iv) the pressure in the second cavity or in a part of the second cavity is kept constant or is kept above a threshhold pressure of 10 bar (10.000 hPa) by treating the substrate and the lacquer during coating and curing of the lacquer.

### Claim 4 (depends on 1)

The process according to claim 1 wherein the molding is by injection molding, injection compression molding, compression, foaming or reaction injection molding.

### Claim 5 (depends on 1)

The process according to claim 1 wherein the lacquer cures via free radicals, ionically or via polyaddition.

### Claim 6 (depends on 1)

The process according to claim 1 wherein the lacquer contains not more than 10 wt. % solvent, the percent being relative to the weight of the lacquer.

### Claim 7 (depends on 1)

The process according to claim 1 wherein the lacquer contains not more than 2 wt. % solvent, the percent being relative to the weight of the lacquer.

### Claim 8 (depends on 1)

The process according to claim 1 wherein the lacquer contains not more than 1 wt. % solvent, the percent being relative to the weight of the lacquer.

### Claim 9 (depends on 1)

The process according to claim 1 wherein the lacquer is solvent free.

### Claim 10 (depends on 1)

The process according to claim 1 wherein the lacquer is a one-component or two-component lacquer.

### Claim 11 (depends on 1)

The process according to claim 1 wherein the lacquer is a polyurethane system or a polyurea system.

### Claim 12 (depends on 1)

The process according to claim 1 wherein the lacquer is a solvent-free aliphatic polyurethane system.

### Claim 13 (depends on 1)

The process according to claim 1 wherein the lacquer has a pot life of not more than 30 min.

### Claim 14 (depends on 1)

The process according to claim 1 wherein the lacquer has a pot life of not more than 10 min.

### Claim 15 (depends on 1)

The process according to claim 1 wherein the lacquer has a pot life of not more than 2 min.

### Claim 16 (depends on 1)

The process according to claim 1 wherein the pressure during coating according to step (iv) is in the range of from 10 to 90 bar (10.000 to 90.000 hPa).

### Claim 17

A mold for in-mold coating comprising at least two cavities, wherein at least one cavity is connected to an injection molding device and at least one cavity is connected to an RIM lacquer injection device.