# US 2006/0151855 A1 · Semiconductor device and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0151855 A1
- Document ID: US20060151855A1
- Status: Published application
- Kind: A1
- Application number: 11/285,156
- Filed: 2005-11-23
- Published: 2006-07-13
- Earliest claimed: 2004-11-25
- Inventors: Masahiro Kiyotoshi; Atsuko Kawasaki
- Web page: https://patentgrep.com/patent/US20060151855A1

## CPC

- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10W 10/0143: {comprising concurrently refilling multiple trenches having different shapes or dimensions}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device includes a semiconductor substrate including an isolation trench provided on a surface thereof, an isolation film provided in the isolation trench, the isolation film including a coating film and a silicon oxide film provided on the coating film, and an oxide film provided between the isolation trench and the isolation film, the oxide film having a thickness such that a portion on a side surface of the isolation trench corresponding to an interface portion between the coating film and the silicon oxide film is thicker than other portion on the side surface.

## Claims

### Claim 1

A semiconductor device comprising:
a semiconductor substrate including an isolation trench provided on a surface thereof;
an isolation film provided in the isolation trench, the isolation film including a coating film and a silicon oxide film provided on the coating film; and
an oxide film provided between the isolation trench and the isolation film, the oxide film having a thickness such that a portion on a side surface of the isolation trench corresponding to an interface portion between the coating film and the silicon oxide film is thicker than other portion on the side surface.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein the oxide film on the side surface of the isolation trench corresponding to the interface portion includes a bird's beak shape.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein the silicon oxide film is an HDP silicon oxide film.

### Claim 4

A semiconductor device comprising:
a semiconductor substrate including an isolation trench provided on a surface thereof;
an isolation film provided in the isolation trench, the isolation film including a coating film and a silicon oxide film provided on the coating film; and
a liner film provided between the isolation trench and the isolation film, the liner film having a thickness such that a portion on an upper surface of the isolation trench decreases upward.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1, wherein the coating film is a coating film of a perhydro silazane polymer.

### Claim 6

The semiconductor device according to claim ˜4, wherein the liner oxide film is an HDP silicon nitride film or a silicon nitride film.

### Claim 7 (depends on 4)

The semiconductor device according to claim 4, wherein a density of the coating film is not higher than 6.0×1023 cm−3.

### Claim 8

A method of manufacturing a semiconductor device, comprising:
forming an isolation trench on a surface of a semiconductor substrate;
filling the isolation trench with a coating film;
heating the coating film under at least one of condition that shrinkage ratio of the coating film is not higher than a predetermined value and condition that film density of the coating film is not higher than a predetermined value;
removing an upper portion of the coating film in the isolation trench by etch back using wet etching;
forming a silicon oxide film on the semiconductor substrate so as to fill the isolation trench; and
planarizing the silicon oxide film by CMP process.

### Claim 9 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, wherein the coating film is a coating film of a perhydro silazane polymer, and the heating the coating film includes heating the coating film under an atmosphere containing mainly water vapor.

### Claim 10 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, wherein the coating film is a coating film of a perhydro silazane polymer, and the heating the coating film includes heating the coating film under an atmosphere containing mainly water vapor under at least one of condition that shrinkage ration of the coating film is not higher than 10% and condition that film density of the coating film is not higher than 6.0×1023 cm−3.

### Claim 11 (depends on 10)

The method of manufacturing the semiconductor device according to claim 10, wherein the coating film is a coating film of a perhydro silazane polymer, and the heating the coating film under the atmosphere containing mainly the water vapor includes setting the temperature of the atmosphere in a range of 250° C. to 350° C.

### Claim 12 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, wherein the silicon oxide film is formed by high density plasma CVD process.

### Claim 13 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, further comprising: oxidizing the semiconductor substrate of a side surface of the isolation trench, the side surface being a surface exposed by the etch back used for removing the upper portion of the coating film in the isolation trench.

### Claim 14 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, further comprising: covering an inner surface of the isolation trench with a liner film before filling the isolation trench with the coating film.

### Claim 15 (depends on 14)

The method of manufacturing the semiconductor device according to claim 14, wherein the liner film is an HTO film or a silicon nitride film.

### Claim 16 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, wherein the removing the upper portion of the coating film in the isolation trench by the etch back using the wet etching includes setting the wet etching rate ratio of the coating film to a thermal oxide film not smaller than 10.

### Claim 17 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, further comprising:
forming a gate oxide film and a gate electrode on the semiconductor substrate before the forming the isolation trench

### Claim 18 (depends on 17)

The method of manufacturing the semiconductor device according to claim 17, wherein a position of uppermost surface of the coating film filling the isolation trench is lower than a position of lowermost surface of the gate oxide film.

### Claim 19 (depends on 8)

The method of manufacturing the semiconductor device according to claim 8, wherein the isolation trench include a first trench region having a first isolation width and a second trench region having a second isolation width being wider than the first isolation width.

### Claim 20 (depends on 19)

The method of manufacturing the semiconductor device according to claim 19, wherein the filling the isolation trench with the coating film includes filling substantially completely the first trench region with the coating film and filling partway the second trench region with the coating film.