# US 2006/0151106 A1 · Method for producing laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0151106 A1
- Document ID: US20060151106A1
- Status: Published application
- Kind: A1
- Application number: 10/559,130
- Filed: 2004-06-01
- Published: 2006-07-13
- Earliest claimed: 2003-06-02
- Inventors: Katsufumi Hiraishi; Katsumi Takata; Isamu Takarabe
- Web page: https://patentgrep.com/patent/US20060151106A1

## CPC

- B32B 37/0053: {Constructional details of laminating machines comprising rollers; Constructional features of the rollers}
- H05K 3/022: {Processes for manufacturing precursors of printed circuits, i.e. copper-clad substrates}
- B32B 38/004: {by physically contacting the layers, e.g. by the use of heated platens or rollers}
- B32B 2305/55: Liquid crystals
- B32B 2311/00: Metals, their alloys or their compounds
- B32B 2379/08: Polyimides
- H05K 2201/0141: Liquid crystal polymer [LCP]
- H05K 2201/0355: Metal foils
- H05K 2203/0143: Using a roller; Specific shape thereof; Providing locally adhesive portions thereon
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A laminate is produced from a film of a liquid crystal polymer forming an optically anisotropic molten phase and a metal foil by thermocompression bonding of a pile of the two between pressing rolls and the method comprises using a metal roll coated with a resin such as fluororubber and polyimide to a thickness of 0.02-5 mm as at least one of the pressing rolls or piling a heat-resistant film on the surface of a pile of polymer film and metal foil contacting a metal pressing roll and passing the resulting pile between metal pressing rolls. The method is capable of producing a laminate of good heat resistance from a liquid crystal polymer film and a metal foil with sufficient adhesion between the two at high productivity.

## Claims

### Claim 1

A method for producing a laminate by piling a film of a liquid crystal polymer forming an optically anisotropic molten phase on a metal foil and passing the pile between pressing rolls to effect compression bonding of said film and metal foil which comprises using a metal roll provided on its surface with a layer of resin coating having a thickness of 0.02-5 mm as at least one of said pressing rolls.

### Claim 2 (depends on 1)

A method for producing a laminate as described in claim 1 wherein said pressing rolls consist of a pair of rolls either of which is a metal roll provided on its surface with a layer of resin coating having a thickness of 0.02-2 mm.

### Claim 3 (depends on 1)

A method for producing a laminate as described in claim 1 wherein the surface temperature of said rolls during compression bonding is controlled at a point lower than the melting point of the liquid crystal polymer film by 20-60° C.

### Claim 4

A method for producing a laminate by piling a film of a liquid crystal polymer forming an optically anisotropic molten phase on a metal foil and passing the pile between metal pressing rolls to effect compression bonding of said film and metal foil which comprises further piling a heat-resistant film selected from heat-resistant resin films and heat-resistant resin composite films on the surface of said pile of the liquid crystal polymer film and metal foil contacting a metal pressing roll and passing the resulting pile between metal pressing rolls.

### Claim 5 (depends on 4)

A method for producing a laminate as described in claim 4 wherein the thickness of the heat-resistant film is 25-300 μm.

### Claim 6 (depends on 4, 5)

A method for producing a laminate as described in claim 4 or 5 wherein the tensile modulus of the heat-resistant film is 1-30 GPa.

### Claim 7 (depends on 4)

A method for producing a laminate as described in claim 4 wherein the heat-resistant film does not adhere to the metal pressing rolls when the surface temperature of the metal pressing rolls is 250° C. and the pressure applied is 150 kN/m.