# US 2006/0150894 A1 · Method for producing a wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0150894 A1
- Document ID: US20060150894A1
- Status: Published application
- Kind: A1
- Application number: 10/567,488
- Filed: 2004-08-04
- Published: 2006-07-13
- Earliest claimed: 2003-08-12
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Inventors: Takeshi Kobayashi
- Web page: https://patentgrep.com/patent/US20060150894A1

## CPC

- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B 29/06: Silicon
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The present invention is a method for producing a wafer comprising, at least, a BMD forming step of subjecting a silicon single crystal in a state of an ingot to heat treatment thereby to form bulk micro defects (BMDs) inside, and a wafer processing step of processing the ingot in which the bulk micro defects (BMDs) was formed into wafers. Thereby, there can be provided a method for producing a wafer, wherein heat treatment for providing IG capability in production of wafer can be shortened and wafers with high IG capability can be produced in large quantity. Also, the present invention can further comprise a wafer heat-treating step of subjecting the processed wafer to heat treatment, or an epitaxial growth step of forming an epitaxial layer on the wafer. Thereby, there is improved productivity of annealed wafers or epitaxial wafers that are excellent in gettering capability.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A method for producing a wafer comprising at least an ingot heat-treating step of subjecting a silicon single crystal in a state of an ingot to heat treatment, and a wafer processing step of processing the heat-treated ingot into wafers.

### Claim 18 (depends on 17)

The method for producing a wafer according to claim 17, wherein in the ingot heat-treating step, bulk micro defects (BMDs) are formed in the silicon single crystal.

### Claim 19 (depends on 17)

The method for producing a wafer according to claim 17, further comprising a wafer heat-treating step of subjecting the wafers to heat treatment after the wafer processing step.

### Claim 20 (depends on 18)

The method for producing a wafer according to claim 18, further comprising a wafer heat-treating step of subjecting the wafers to heat treatment after the wafer processing step.

### Claim 21 (depends on 17)

The method for producing a wafer according to claim 17, wherein in the wafer processing step, the heat-treated ingot is processed into mirror-like wafers.

### Claim 22 (depends on 21)

The method for producing a wafer according to claim 21, further comprising an epitaxial growth step of forming an epitaxial layer on the wafer after the processing into the mirror-like wafers.

### Claim 23 (depends on 17)

The method for producing a wafer according to claim 17, wherein in the ingot heat-treating step, the silicon single crystal in a state of an ingot is subjected to heat treatment at 700° C. or more.

### Claim 24 (depends on 23)

The method for producing a wafer according to claim 23, wherein in the ingot heat-treating step, the heat treatment is performed at a heat treatment temperature of 1100° C. or less for 30 minutes to 8 hours.

### Claim 25 (depends on 24)

The method for producing a wafer according to claim 24, wherein in the ingot heat-treating step, the heat treatment is performed at a heat treatment temperature of 700° C. to 900° C. for 30 minutes to 8 hours.

### Claim 26 (depends on 17)

The method for producing a wafer according to claim 17, wherein in the ingot heat-treating step, the heat treatment is performed at a temperature rising rate of 0.5° C./min to 10° C./min.

### Claim 27 (depends on 19)

The method for producing a wafer according to claim 19, wherein in the wafer heat-treating step, a defect-free region (a DZ (denuded zone) layer) is formed in a surface of the wafer.

### Claim 28 (depends on 20)

The method for producing a wafer according to claim 20, wherein in the wafer heat-treating step, a defect-free region (a DZ (denuded zone) layer) is formed in a surface of the wafer.

### Claim 29 (depends on 19)

The method for producing a wafer according to claim 19, wherein in the wafer heat-treating step, the heat treatment is performed at a heat treatment temperature of 900° C. to 1300° C. for 5 minutes to 16 hours.

### Claim 30 (depends on 20)

The method for producing a wafer according to claim 20, wherein in the wafer heat-treating step, the heat treatment is performed at a heat treatment temperature of 900° C. to 1300° C. for 5 minutes to 16 hours.

### Claim 31 (depends on 19)

The method for producing a wafer according to claim 19, wherein in the wafer heat-treating step, the temperature is raised at a temperature rising rate of 5° C./min or more.

### Claim 32 (depends on 20)

The method for producing a wafer according to claim 20, wherein in the wafer heat-treating step, the temperature is raised at a temperature rising rate of 5° C./min or more.

### Claim 33 (depends on 22)

The method for producing a wafer according to claim 22, wherein the epitaxial growth step is that after a pretreatment is performed at a temperature of 1000° C. or more, the epitaxial growth is performed at a temperature of 1000° C. or more.

### Claim 34 (depends on 17)

The method for producing a wafer according to claim 17, wherein the silicon single crystal is a crystal doped with nitrogen.

### Claim 35 (depends on 17)

The method for producing a wafer according to claim 17, wherein the silicon single crystal is a crystal in a nearly perfect crystal (NPC) region produced by Czochralski method.

### Claim 36 (depends on 17)

The method for producing a wafer according to claim 17, wherein the silicon single crystal in a state of an ingot is an ingot pulled by a single crystal-pulling apparatus according to Czochralski method as it is or an ingot in a state that the pulled ingot is cylindrically ground and cut in a shape of a block.