# US 2006/0150685 A1 · Method for elongating and collapsing a blank made of quartz glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0150685 A1
- Document ID: US20060150685A1
- Status: Published application
- Kind: A1
- Application number: 10/559,481
- Filed: 2004-06-03
- Published: 2006-07-13
- Earliest claimed: 2003-06-04
- Assignees: Heraeus Tenevo GmbH
- Inventors: Heinz Fabian
- Web page: https://patentgrep.com/patent/US20060150685A1

## CPC

- C03B 37/01242: {Controlling or regulating the down-draw process}
- C03B 37/0253: {Controlling or regulating (for glass fibre manufacture in general C03B37/07)}
- C03B 2205/44: Monotoring or regulating the preform feed rate
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

The invention relates to a method for the production of an optical component made of quartz glass by elongating a coaxial array, comprising of a hollow quartz glass cylinder that has an inner bore hole and that has been mechanically machined to the end volume and a core rod arranged inside the inner bore hole, wherein the coaxial array is fed to a heat zone with a predetermined forward feed motion and is softened zonewise therein and the optical component is drawn from the softened area, wherein an annular gap between the core rod and the hollow cylinder is collapsed. The invention aims at providing an economical method by means of which an optical component can be produced and which is characterized by a low break rate when the fibers are drawn. Depending on the outer diameter of the hollow cylinder D [in mm], the forward feed motion V [in mm/min] is maintained within a range complying with the following calculation Vmin=3000×(2/D)2 and Vmax=16000×(2/D)2.

## Claims

### Claim 1

A method for producing an optical component of quartz glass, the method comprising: elongating a coaxial assembly, the coaxial assembly comprising a hollow cylinder of quartz glass having an inner bore and an outer diameter, the hollow cylinder being mechanically treated to a final dimension, and a core rod arranged inside the inner bore, the coaxial assembly being supplied at a predetermined feed rate to a heating zone and being softened therein zonewise, and the optical component being drawn off from the softened region, an annular gap between the core rod and the hollow cylinder being collapsed, wherein the hollow cylinder has an outer diameter D of at least 150 mm, and the predetermined feed rate, V (expressed in units of mm/min), is kept within a range satisfying the following dimensioning rule:
Vmin=3000×(2/D)2,
Vmax=16000×(2/D)2,
and wherein the predetermined feed rate is below 2.5 mm/min.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the predetermined feed rate is is kept below a Vmax determined according to the expression 8000×(2/D)2.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the predetermined feed rate is set to a value below 1.5 mm/min.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the mechanical treatment of the hollow cylinder includes grinding of the inner wall of the inner bore and a subsequent etching treatment, the inner wall of the inner bore having subsurface cracks that remain after grinding, the subsurface cracks having a crack depth ranging from 0.2 mm to 2 mm.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the annular gap between the core rod and the hollow cylinder is on average greater than 2 mm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the annular gap between the core rod and the hollow cylinder is on average smaller than 1 mm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the hollow cylinder has an inner diameter of not more than 70 mm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein a ratio of a radial cross-sectional area CSA(C) of the hollow cylinder to a radial cross-sectional area CSA(R) of the core rod is within the range between 5 and 100.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the hollow cylinder is produced by an OVD method.

### Claim 10 (depends on 2)

The method according to claim 2, wherein the mechanical treatment of the hollow cylinder includes grinding of the inner wall of the inner bore and a subsequent etching treatment, the inner wall of the inner bore having subsurface cracks that remain after grinding, the subsurface cracks having a crack depth ranging from 0.2 mm to 2 mm.

### Claim 11 (depends on 3)

The method according to claim 3, wherein the mechanical treatment of the hollow cylinder includes grinding of the inner wall of the inner bore and a subsequent etching treatment, the inner wall of the inner bore having subsurface cracks that remain after grinding, the subsurface cracks having a crack depth ranging from 0.2 mm to 2 mm.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the annular gap between the core rod and the hollow cylinder averages greater than 5 mm.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the annular gap between the core rod and the hollow cylinder is on average smaller than 0.7 mm.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the hollow cylinder has an inner diameter of not more than 50 mm.

### Claim 15 (depends on 1)

The method according to claim 1, wherein a ratio of a radial cross-sectional area CSA(C) of the hollow cylinder to a radial cross-sectional area CSA(R) of the core rod is within the range between 10 and 80.

### Claim 16 (depends on 2)

The method according to claim 2, wherein the annular gap between the core rod and the hollow cylinder averages greater than 5 mm.

### Claim 17 (depends on 2)

The method according to claim 2, wherein the annular gap between the core rod and the hollow cylinder is on average smaller than 0.7 mm.

### Claim 18 (depends on 2)

The method according to claim 2, wherein the hollow cylinder has an inner diameter of not more than 50 mm.

### Claim 19 (depends on 2)

The method according to claim 2, wherein a ratio of a radial cross-sectional area CSA(C) of the hollow cylinder to a radial cross-sectional area CSA(R) of the core rod is within the range between 10 and 80.

### Claim 20 (depends on 1)

The method according to claim 1, wherein wherein the mechanical treatment of the hollow cylinder includes grinding of the inner wall of the inner bore and a subsequent etching treatment, the inner wall of the inner bore having subsurface cracks that remain after grinding, the subsurface cracks having a crack depth ranging from 0.2 mm to 2 mm, wherein the annular gap between the core rod and the hollow cylinder averages greater than 5 mm, wherein the annular gap between the core rod and the hollow cylinder is on average smaller than 0.7 mm, and wherein the hollow cylinder has an inner diameter of not more than 50 mm.