Rigid polyurethane foams, a process for their production and their use
OwnerChristoph Hollmann, Dieter Seidel +1inventors
InventorsChristoph Hollmann, Dieter Seidel, Klaus-Werner Huland
Life of this patent
Estimating the term…
Abstract
Predominantly open-cell, cold-formable, compressed rigid polyurethane foams are produced from an isocyanate component satisfying specified criteria and an isocyanate-reactive component composed of at least 5 polyhydroxyl compounds satisfying specified criteria. These foams are produced by a double conveyor belt process. The foams of the present invention are particularly useful for the manufacture of soft trim for cars, especially inside roof linings, roof stiffening boards and column trim.
Claims5
A continuous process for the production of cold-formable, compressed, open-cell rigid polyurethane foams by a double conveyor belt process comprising:
- I) mixing
- component A) comprising
- a) an organic polyisocyanate component comprising:
- a1) from 70 to 90 wt. %, based on total weight of A), of monomeric diphenylmethane diisocyanate containing from 18 to 32 wt. % of 2,4′-diphenylmethane diisocyanate, and
- a2) from 10 to 30 wt. %, based on total weight of A), of polyphenylpolymethylene polyisocyanate
- with
- component B) comprising
- b) a combination of polyhydroxyl compounds comprising:
- b1) from 20 to 35 wt. %, based on total weight of component B), of at least one polyoxyalkylene polyol having a functionality of from 2 to 3 and a hydroxyl number of from 25 to 40,
- b2) from 20 to 30 wt. %, based on total weight of component B), of at least one polyoxylalkylene polyol having a functionality of from 3 to 4 and a hydroxyl number of from 400 to 650,
- b3) from 5 t 15 wt. %, based on total weight of component B), of at least one polyoxyalkylene polyol having a functionality of 2 and a hydroxyl number of from 150 to 550,
- b4) from 15 to 30 wt. %, based on total weight of component B), of at least one polyester polyol having a functionality of 2 and a hydroxyl number of from 200 to 350, and
- b5) from 4 to 7 wt. %, based on total weight of component B), of glycerol,
- c) from 3.5 to 5.5 wt. %, based on total weight of component B), of water,
- d) from 0.5 to 4 wt. %, based on total weight of component B), of at least one catalyst,
- e) from 0.5 to 2 wt. %, based on total weight of component B), of at least one foam stabilizer,
- f) from 1 to 3.5 wt. %, based on total weight of component B), of a cell opener, and
- g) from 0 to 7 wt. %, based on total weight of component B), of one or more auxiliary substances and/or additives
- in a mixer at a temperature of from 20 to 35° C. and an NCO index of from 95to125,
- II) introducing the mixture from I) between two facings of a double conveyor belt at a temperature of from 40 to 100° C., and
- III) allowing the mixture introduced in II) to form a foam,
- IV) cooling the foam formed in III), and
- V) optionally removing one or both of the facings and, optionally, cutting the cooled foam.
A cold-formable, compressed, open-cell rigid polyurethane foam comprising the reaction product of
- 1) component A) comprising
- a) an organic polyisocyanate component comprising:
- a1) from 70 to 90 wt. %, based on total weight of A), of monomeric diphenylmethane diisocyanate containing from 18 to 32 wt. % of 2,4′-diphenylmethane diisocyanate, and
- a2) from 10 to 30 wt. %, based on total weight of A), of polyphenylpolymethylene polyisocyanate
- with
- 2) component B) comprising
- b) a combination of polyhydroxyl compounds comprising:
- b1) from 20 to 35 wt. %, based on total weight of component B), of at least one polyoxyalkylene polyol having a functionality of from 2 to 3 and a hydroxyl number of from 25 to 40,
- b2) from 20 to 30 wt. %, based on total weight of component B), of at least one polyoxylalkylene polyol having a functionality of from 3 to 4 and a hydroxyl number of from 400 to 650,
- b3) from 5 t 15 wt. %, based on total weight of component B), of at least one polyoxyalkylene polyol having a functionality of 2 and a hydroxyl number of from 150 to 550,
- b4) from 15 to 30 wt. %, based on total weight of component B), of at least one polyester polyol having a functionality of 2 and a hydroxyl number of from 200 to 350, and
- b5) from 4 to 7 wt. %, based on total weight of component B), of glycerol,
- c) from 3.5 to 5.5 wt. %, based on total weight of component B), of water,
- d) from 0.5 to 4 wt. %, based on total weight of component B), of at least one catalyst,
- e) from 0.5 to 2 wt. %, based on total weight of component B), of at least one foam stabilizer,
- f) from 1 to 3.5 wt. %, based on total weight of component B), of a cell opener, and
- g) from 0 to 7 wt. %, based on total weight of component B), of one or more auxiliary substances and/or additives
- at an NCO index of from 95 to 125.
Dependencies are inferred from the claim text.