# US 2006/0141725 A1 · Method of manufacturing flash memory device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0141725 A1
- Document ID: US20060141725A1
- Status: Published application
- Kind: A1
- Application number: 11/129,776
- Filed: 2005-05-16
- Published: 2006-06-29
- Earliest claimed: 2004-12-28
- Assignees: Hynix Semiconductor Inc.
- Inventors: Seung Lee; Sang Park
- Web page: https://patentgrep.com/patent/US20060141725A1

## CPC

- H10D 30/681: {having only two programming levels (Floating gate IGFETs programmable by two single electrons H10D30/688)}
- H10D 30/0411: {of FETs having floating gates}
- H10D 30/6891: {characterised by the shapes, relative sizes or dispositions of the floating gate electrode}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of manufacturing a flash memory device wherein before an insulating film spacer of a contact region is removed after a gate line and source/drain are formed, a high quality buffer oxide film formed between the gate line and the insulating film spacer is made dense by means of an annealing process. Abnormal oxidization is thus prevented from occurring due to an exposed metal layer in a gate when the insulating film spacer is removed as at least part of the buffer oxide remains after the spacer is removed.

## Claims

### Claim 1

A method of manufacturing a flash memory device, comprising:
forming a gate line on a semiconductor substrate;
sequentially forming a buffer oxide film and a nitride film on the gate line;
etching the nitride film by means of a blanket etch process, thereby forming an insulating film spacer;
forming impurity regions in the semiconductor substrate by using the gate line and the insulating film spacer as an ion implant mask;
performing an annealing process to densify the buffer oxide film;
removing the insulating film spacer; and
performing a self-aligned contact process.

### Claim 2 (depends on 1)

The method as claimed in claim 1, further comprising, before the buffer oxide film is formed, forming low-concentration impurity regions in the semiconductor substrate by means of an ion implant process using the gate line as an ion implant mask.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the insulating film spacer is removed by means of a wet etch process using phosphoric acid.

### Claim 4 (depends on 3)

The method as claimed in claim 3, wherein the wet etch process includes removing the insulating film spacer without removing the buffer oxide film.

### Claim 5 (depends on 3)

The method as claimed in claim 3, wherein the wet etch process is performed for a time period ranging from 5 to 25 minutes.

### Claim 6 (depends on 3)

The method as claimed in claim 3, wherein the buffer oxide film remains at a thickness in a range from 50 to 150 Å after the insulating film spacer is removed.

### Claim 7

A method of manufacturing a flash memory device, comprising:
forming a gate line on a semiconductor substrate;
sequentially forming a buffer oxide film and a nitride film on the gate line;
etching the nitride film by means of a blanket etch process, form an insulating film spacer from a remaining portion of the nitride film;
forming impurity regions in the semiconductor substrate by using the gate line and the insulating film spacer as an ion implant mask;
performing an annealing process to densify the buffer oxide film;
removing the insulating film spacer without removing the buffer oxide film.

### Claim 8 (depends on 7)

The method as claimed in claim 7, further comprising, before the buffer oxide film is formed, forming low-concentration impurity regions in the semiconductor substrate by means of an ion implant process using the gate line as an ion implant mask.

### Claim 9 (depends on 7)

The method as claimed in claim 7, wherein the insulating film spacer is removed by means of a wet etch process using phosphoric acid.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein the wet etch process includes removing the insulating film spacer without removing the buffer oxide film by considering etch rates of the insulating film spacer and buffer oxide films and timing the wet etch process so at least a portion of the buffer oxide film remains.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein the wet etch process is performed for a time period ranging from 5 to 25 minutes.

### Claim 12 (depends on 10)

The method as claimed in claim 10, wherein the buffer oxide film remains at a thickness in a range from 50 to 150 Å after the insulating film spacer is removed.

### Claim 13

A method of manufacturing a flash memory device, comprising:
forming a gate line on a semiconductor substrate;
sequentially forming a buffer oxide film and a nitride film over the gate line;
etching the nitride film by means of a blanket etch process, thereby forming an insulating film spacer on top of the buffer oxide film;
forming impurity regions in the semiconductor substrate by using the gate line and the insulating film spacer as an ion implant mask;
performing an annealing process to densify the buffer oxide film;
removing the insulating film spacer without removing all of the buffer oxide film.

### Claim 14 (depends on 13)

The method as claimed in claim 13, further comprising, before the buffer oxide film is formed, forming low-concentration impurity regions in the semiconductor substrate by means of an ion implant process using the gate line as an ion implant mask.

### Claim 15 (depends on 13)

The method as claimed in claim 13, wherein the insulating film spacer is removed by means of a wet etch process using phosphoric acid.

### Claim 16 (depends on 15)

The method as claimed in claim 15, wherein the wet etch process includes completely removing the insulating film spacer without removing the buffer oxide film by limiting a time period for the wet etch process.

### Claim 17 (depends on 16)

The method as claimed in claim 16, wherein the wet etch process is performed for a time period ranging from 5 to 25 minutes.

### Claim 18 (depends on 17)

The method as claimed in claim 17, wherein the buffer oxide film remains at a thickness in a range from 50 to 150 Å after the insulating film spacer is removed.