# US 2006/0138590 A1 · Electronic parts and method for manufacture thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0138590 A1
- Document ID: US20060138590A1
- Status: Published application
- Kind: A1
- Application number: 10/544,008
- Filed: 2004-02-03
- Published: 2006-06-29
- Earliest claimed: 2003-02-05
- Assignees: TDK Corporation
- Inventors: Kazutaka Suzuki; Shigeki Sato
- Web page: https://patentgrep.com/patent/US20060138590A1

## CPC

- H01G 4/0085: {Fried electrodes}
- H01G 4/012: Form of non-self-supporting electrodes
- H01G 4/1227: {based on alkaline earth titanates}
- H01G 4/30: Stacked capacitors (H01G4/33 takes precedence)
- H01G 4/306: {made by thin film techniques}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

An electronic device having an element body comprising an internal electrode layer, wherein the internal electrode layer includes an alloy, the alloy contains a nickel (Ni) element and at least one kind of element selected from ruthenium (Ru), rhodium (Rh), rhenium (Re) and platinum (Pt), and a content of each component is Ni: 80 to 100 mol % (note that 100 mol % is excluded) and a total of Ru, Rh, Re and Pt: 0 to 20 mol % (note that 0 mol % is excluded).

## Claims

### Claim 1

An electronic device having an element body comprising an internal electrode layer, wherein
said internal electrode layer contains an alloy;
the alloy contains
nickel (Ni), and
at least one kind of element selected from a group of ruthenium (Ru), rhodium (Rh), rhenium (Re) and platinum (Pt); and
a content of each component is
Ni: 80 to 100 mol % (note that 100 mol % is excluded), and
a total of Ru, Rh, Re and Pt: 0 to 20 mol % (note that 0 mol % is excluded).

### Claim 2 (depends on 1)

The electronic device as set forth in claim 1, wherein a content of each component is
Ni: 87 to 99.9 mol %, and
a total of Ru, Rh, Re and Pt: 0.1 to 13 mol %.

### Claim 3 (depends on 1)

The electronic device as set forth in claim 1, wherein said alloy includes at least one kind of element selected from the group of rhodium (Rh), rhenium (Re) and platinum (Pt).

### Claim 4 (depends on 1)

The electronic device as set forth in claim 1, wherein
said internal electrode layer includes an alloy; and
when assuming that peak strength of a diffraction line on a crystal plane (111) is I(111), peak strength of a diffraction line on a crystal plane (200) is I(200), and peak strength of a diffraction line on a crystal plane (220) is I(220), the alloy has a main plane satisfying relationships of (I(111)/I(200))≧3 and (I(111)/I(220))≧3.

### Claim 5 (depends on 1)

A production method of an electronic device for producing an electronic device as set forth in claim 1, wherein
a green chip having an internal electrode layer film formed to be a predetermined pattern by a thin film method is fired to produce said element body.

### Claim 6 (depends on 5)

The production method of an electronic device as set forth in claim 5, wherein said internal electrode layer film has a crystalline size of 10 to 100 nm.

### Claim 7 (depends on 5)

The production method of an electronic device as set forth in claim 5, wherein said internal electrode film is formed by the sputtering method or the evaporation method.

### Claim 8 (depends on 1)

A production method of an electronic device for producing an electronic device as set forth in claim 1, wherein:
a green chip having an internal electrode layer film formed to be a predetermined pattern by the printing method using a paste including alloy powder having an average particle diameter of 0.001 to 1 μm is fired to produce said element body.

### Claim 9 (depends on 8)

The production method of an electronic device as set forth in claim 8, wherein said alloy powder has a crystalline size of 10 to 100 nm.

### Claim 10 (depends on 8)

The production method of an electronic device as set forth in claim 8, wherein said alloy powder is formed by grinding an alloy film formed by the sputtering method or the evaporation method.

### Claim 11 (depends on 1)

A production method of an electronic device for producing an electronic device as set forth in claim 1, wherein:
a green chip having an internal electrode layer film formed to be a predetermined pattern by the printing method using a paste including conductive particles is fired to produce said element body; wherein
said conductive particle includes
a core portion containing nickel as the main component, and
a cover layer covering at least a part around said core portion; and
said cover layer is composed of a metal or an alloy including as the main component at least one kind of element selected from ruthenium (Ru), rhodium (Rh), rhenium (Re) and platinum (Pt).

### Claim 12 (depends on 11)

The production method of an electronic device as set forth in claim 11, wherein said core portion is powder in a spherical shape, a flake shape, a projection form and/or an amorphous shape, wherein a typical length of the particle is in a range of 0.01 μm to 1.0 μm.

### Claim 13 (depends on 11)

The production method of an electronic device as set forth in claim 11, wherein a thickness of said cover layer is in a range of 0.1 to 15 nm.

### Claim 14 (depends on 1)

A production method of an electronic device for producing an electronic device as set forth in claim 1, comprising the steps of:
forming a sub conductive layer composed of a metal layer or an alloy layer having at least one kind of element selected from ruthenium (Ru), rhodium (Rh), rhenium (Re) and platinum (Pt);
forming a main conductive layer including nickel as the main component by stacking said sub conductive layer; and
firing a green chip including an internal electrode layer film comprising said sub conductive layer and main conductive layer.

### Claim 15 (depends on 14)

The production method of an electronic device as set forth in claim 14, wherein said main conductive layer is sandwiched between a pair of said sub conductive layers, and said internal electrode layer has the configuration that three or more layers are stacked.

### Claim 16 (depends on 14)

The production method of an electronic device as set forth in claim 14, wherein a thickness of said sub conductive layer is more than 0 μm and 0.1 μm or less.

### Claim 17 (depends on 14)

The production method of an electronic device as set forth in claim 14, wherein a thickness of said main conductive layer is 0.1 to 1.0 μm.

### Claim 18 (depends on 14)

The production method of an electronic device as set forth in claim 14, wherein said sub conductive layer is formed by the thin film forming method, and said main conductive layer is formed by the printing method or the thin film forming method.

### Claim 19 (depends on 5)

The production method of an electronic device as set forth in claim 5, wherein said green chip is fired in an atmosphere having an oxygen partial pressure of 10−10 to 10−2 Pa at the temperature of 1000 to 1300° C.

### Claim 20 (depends on 5)

The production method of an electronic device as set forth in claim 5, wherein said element body is annealed in an atmosphere having an oxygen partial pressure of 10−2 to 100 Pa at the temperature of 1200° C. or lower after a step of firing said green chip.

### Claim 21 (depends on 5)

An electronic device formed by any one of the methods described in claim 5.