# US 2006/0138572 A1 · Semiconductor device and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0138572 A1
- Document ID: US20060138572A1
- Status: Published application
- Kind: A1
- Application number: 11/357,072
- Filed: 2006-02-21
- Published: 2006-06-29
- Earliest claimed: 2003-08-29
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Tsunetoshi Arikado; Takaaki Kawahara; Kazuyoshi Torii; Hiroshi Kitajima; Seiichi Miyazaki
- Web page: https://patentgrep.com/patent/US20060138572A1

## CPC

- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A gate insulating film on a silicon substrate of includes a SiO2 film and a high-k film. The high-k film contains a transition metal, aluminum, silicon, and oxygen. The concentration of silicon in the high-k film is higher than the concentrations of the transition metal and aluminum in the vicinity of the interface with the SiO2 film and the vicinity of the interface with the gate electrode. Furthermore, it is preferable that the concentration of silicon is the highest at least in one of the vicinity of the interface with the SiO2 film or the vicinity of the interface with the gate electrode, gradually decreases with distance from these interfaces, and becomes the lowest in a central part of the high-k film.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A method for manufacturing a semiconductor device comprising:
forming a SiO2 film on a silicon substrate,
forming a HfAlSiOx film on said SiO2 film, and
forming a gate electrode of polysilicon on said HfAlSiOx film, wherein
said HfAlSiOx film is formed by ALD (Atomic Layer Deposition) using HfCl4, Al(CH3)3, Si(OC2H5)4, and an oxidizing gas as source materials, and
a concentration of silicon in said HfAlSiOx film is increased over concentrations of hafnium and aluminum in proximity to an interface with said SiO2 film and in proximity to an interface with said gate electrode by changing the time during which each of HfCl4, Al(CH3)3, and Si(OC2H5)4 is supplied.

### Claim 17 (depends on 16)

The method for manufacturing a semiconductor device according to claim 16, wherein said oxidizing gas is H2O.

### Claim 18

A method for manufacturing a semiconductor device comprising:
forming a HfAlSiOx film on a silicon substrate, and
forming a gate electrode of polysilicon on said HfAlSiOx film, wherein
said HfAlSiOx film is formed by ALD using HfCl4, Al(CH3)3, Si(OC2H5)4, and an oxidizing gas as source materials, and
a concentration of silicon in said HfAlSiOx film is increased over concentrations of hafnium and aluminum in proximity to an interface with said silicon substrate and proximity to an interface with said gate electrode by changing the time during which each of HfCl4, Al(CH3)3, and Si(OC2H5)4 is supplied.

### Claim 19 (depends on 18)

The method of manufacturing a semiconductor device according to claim 18, wherein said oxidizing gas is H2O.

### Claim 20 (depends on 16)

The method according to claim 16, wherein the concentration of the silicon:
is made largest in at least one of areas in proximity to the interface with said SiO2 film and in proximity to the interface with said gate electrode;
gradually decreases with distance from these interfaces; and
becomes smallest at a central part of said HfAlSiOx film.

### Claim 21 (depends on 16)

The method according to claim 16, wherein concentrations of hafnium, aluminum, and silicon in said HfAlSiOx film are 25.0% to 35.0%, 32.5% to 37.5%, and 32.5% to 37.5%, respectively.

### Claim 22 (depends on 18)

The method according to claim 18, wherein the concentration of the silicon:
is made largest in at least one of areas in proximity to the interface with said silicon substrate and in proximity to the interface with said gate electrode;
gradually decreases with distance from these interfaces; and
becomes smallest at a central part of said HfAlSiOx film.

### Claim 23 (depends on 18)

The method according to claim 18, wherein concentrations of hafnium, aluminum, and silicon in said HfAlSiOx film are 25.0% to 25.0%, 32.5% to 37.5%, and 32.5% to 37.5%, respectively.